Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.79 GPa | 260 ksi | Tangent; ASTM D790 |
RheTech Products CC30P100-01 30% Calcium Carbonate Reinforced Polypropylene, Black Applications: Consumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 1.79 GPa | 260 ksi | ASTM D790 |
PolyOne Trilliant™ HC HC3620-0040 RS Natural Polycarbonate + PBT (PC+PBT) The Trilliant® specialty compounds offer a complete system of specialty engineered materials, certified processes, services and technical support that enable healthcare OEM's to get to market ahead.. |
|||
Flexural Modulus | 1.79 GPa | 260 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics GELOY CR7020 ASA ASA copolymer. Profile/sheet coextrusion over ABS. Excellent weatherability, good flow/aesthetics and high impact. |
|||
Flexural Modulus | 1.79 GPa | 260 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics GELOY CR7020 ASA (Asia Pacific) ASA copolymer. Profile/sheet coextrusion over ABS. Excellent weatherability, good flow/aesthetics and high impact. |
|||
Flexural Modulus | 1.79 GPa | 260 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics GELOY FXW710SK ASA General purpose injection molding ASA with Visual Fx sparkle effect. |
|||
Flexural Modulus | 1.79 GPa | 260 ksi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N1000STHL Nylon 6/6 (DAM) Information provided by Ravago |
|||
Flexural Modulus | 1.79 GPa | 260 ksi | ASTM D790 |
Albis Plastics Cellulose Acetate Butyrate B9304 (Odor Mask Added), 4% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Flexural Modulus | 1.79 GPa | 260 ksi | ASTM D790 |
M. Holland Company PP510 Polypropylene Homopolymer AntistaticGood flowHomopolymerNucleatedGood stiffnessApplications: CapsClosuresDisposable hospital goodsHousehold goods |
|||
Flexural Modulus | 1.79 GPa | 260 ksi | Tangent; ASTM D790 |
M. Holland Company PP700 Polypropylene Homopolymer Features: Antistatic, NucleatedUses: Closure Caps, Thin-walled PartsApprovals: FDA 21 CFR 177.1520Processing Method: Injection MoldingInformation provided by M. Holland. |
|||
Flexural Modulus | 1.79 GPa | 260 ksi | |
Ineos Styrenics Avantra® 597N Polystyrene (NAFTA) High-impact grade of polystyrene with improved impact strength and heat resistance, developed for injection molding and extrusion/thermoforming applications.Information provided by BASF.Ineos Styren.. |
|||
Flexural Modulus | 1.79 GPa | 260 ksi | ASTM D790 |
LTL Color Compounds ColorRxâ„¢ PE3-0200RX Biocompatible LDPE A biocompatible Low Density Polyethylene for healthcare applicationsAll information provided by LTL Color Compounders, Inc. |
|||
Flexural Modulus | 1.79 GPa | 260 ksi | ASTM D790 |
LTL Color Compounds ColorRxâ„¢ PE3-0202ARX Biocompatible, Antimicrobial LDPE A biocompatible Low Density Polyethylene for healthcare applications containing antimicrobial protection.All information provided by LTL Color Compounders, Inc. |
|||
Flexural Modulus | 1.79 GPa | 260 ksi | ASTM D790 |
Techmer ES Elastoblend® PA6/6 IM L N Nylon 66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubricant and Impact ModifiedUL File Number: E157318Processing Method: Inj.. |
|||
Flexural Modulus | 1.79 GPa | 260 ksi | ASTM D790 |
Spartech Royalite R84 Weather Resistant Sheet Description: Weather Resistant SheetInformation provided by Spartech. |
|||
Flexural Modulus | 1.79 GPa | 260 ksi | Tangent; ASTM D790 |
Plastics Group Polifil® RMC-20V 20% Calcium Carbonate-Reinforced Polypropylene, High Impact, UV Stabilized Polifil® RMC-V series compounds are high impact, UV stabilized polypropylenes reinforced with fine particle size calcium carbonate. In addition to the highest impact possible, these compounds retar.. |
|||
Flexural Modulus | 1.79 GPa | 260 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 3716 Talc Filled Copolymer Polypropylene DescriptionPolyfort® FPP 3716 is a 12% talc filled copolymer polypropylene product. Information provided by A. Schulman. |
|||
Flexural Modulus | 1.79 GPa | 260 ksi | 1% Secant; ASTM D790 |
Washington Penn Medium Impact Copolymer 40% Calcium Carbonate Filled Calcium carbonate-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug pa.. |
|||
Flexural Modulus | 1.79 GPa | 260 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 3716 Talc Filled Copolymer Polypropylene DescriptionPolyfort® FPP 3716 is a 12% talc filled copolymer polypropylene product. Information provided by A. Schulman. |
|||
Flexural Modulus | 1.79 GPa | 260 ksi | 1.3mm per min, 1% secant; ASTM D790 |
Formosa Plastics Formolene® 4142T Injection Molding Polypropylene Homopolymer with Nucleating, Antistat AdditivesApplications: Appliance, closure and thin wall applications.Formolene 4142T is a low viscosity, highly isotactic polypropylene homopolymer designed pri.. |
|||
Flexural Modulus | 1.79 GPa | 260 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 3716 Talc Filled Copolymer Polypropylene DescriptionPolyfort® FPP 3716 is a 12% talc filled copolymer polypropylene product. Information provided by A. Schulman. |
|||
Flexural Modulus | 1.79 GPa | 260 ksi | Tangent, chs 0.05 in/min; ASTM D790 |
Diamond Polymers ABS/PC 8901 Description: Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Flexural Modulus | 1.79 GPa | 260 ksi | ASTM D790 |
CIP Composites 100 Series Laminated Polymer Bearing Material The 100 series consists of polyester fabric and one of several solid lubricants (optional) in a resin matrix. Non-metallic, high load, high impact and self lubricating laminated material. Laminated.. |
|||
Flexural Modulus | 1.79 GPa | 260 ksi | ASTM D790 |
BASF Ultramid® BU50I BK 106 PA6 (Dry) Description: Ultramid Ultratough Nylon BU50I BK-106 is an unreinforced PA6, impact modified, pigmented black, injection molding product that maintains its impact strength and ductility to -40 deg F .. |
|||
Flexural Modulus | 1.79 GPa | 260 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics GELOY CR7520 ASA (Asia Pacific) ASA copolymer. Automotive grilles and exteriors. Excellent weatherability, good flow/aesthetics and high impact. Rated f2 by UL. |
|||
Flexural Modulus | 1.79 GPa | 260 ksi | ISO 178 |
Polyram RamLloy A001 Nylon 66/Polyethylene Alloy for Injection Molding, Impact Modified Nylon 66/PE Alloy, reduction of water absorption, impact modified, for injection molding applications.Information provided by Polyram. |
|||
Flexural Modulus | 1.79 GPa | 260 ksi | ASTM D790 |
Polymer Resources PC/TP-GP3 PC Polyester, High Impact, Superior Chemical Resistance
(Unverified Data**)&l Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Flexural Modulus | 1.79 GPa | 260 ksi | ASTM D790 |
LTL Color Compounds ColorRx™ PE3-0201A Antimicrobial LDPE Low Density Polyethylene containing antimicrobial protection. Ingredients are not approved for biocompatibility or food contact applications.All information provided by LTL Color Compounders, Inc. |
|||
Flexural Modulus | 1.79 GPa | 260 ksi | 0.1 in/min; ASTM D790 |
Ineos Nova Zyntar® 7041 High Performance Flame Retardant Polystyrene
(discontinued **) Non-Decabromodiphenyl Oxide, High flow, Ease of processingApplications: Electronics, TelevisionsThis is an impact grade of polystyrene containing chemicals to increase resistance to ignition in labo.. |
|||
Flexural Modulus | 1.79 GPa | 260 ksi | ASTM D790 |
PlastxWorld CEVIAN®-V T150 ABS Medium impact transparent ABS.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |