Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LTL Color Compounds ColorRx™ PE3-0201A Antimicrobial LDPE

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE
Manufacturer LTL Color Compounds
Trade Name ColorRx™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LTL Color Compounds ColorRx™ PE3-0201A Antimicrobial LDPE.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Low Density Polyethylene containing antimicrobial protection. Ingredients are not approved for biocompatibility or food contact applications.All information provided by LTL Color Compounders, Inc.
Physical Properties Metric English Comments
Specific Gravity 0.920 g/cc
0.920 g/cc
ASTM D792
Melt Flow 1.9 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.9 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 14.5 MPa
2100 psi
ASTM D638
Elongation at Break >= 500 %
>= 500 %
ASTM D638
Flexural Modulus 1.79 GPa
260 ksi
ASTM D790
Thermal Properties Metric English Comments
Vicat Softening Point 95.6 °C
204 °F
ASTM D648