M. Holland Company PP510 Polypropylene Homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer M. Holland Company
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF M. Holland Company PP510 Polypropylene Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
AntistaticGood flowHomopolymerNucleatedGood stiffnessApplications: CapsClosuresDisposable hospital goodsHousehold goods
Physical Properties Metric English Comments
Density 0.905 g/cc
0.0327 lb/in³
ASTM D1505
Melt Flow 20 g/10 min

@Load 2.16 kg,
Temperature 230 °C
20 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 108
108
ASTM D785
Tensile Strength, Yield 38.6 MPa
5600 psi
ASTM D638
Flexural Modulus 1.79 GPa
260 ksi
ASTM D790
Izod Impact, Notched 0.320 J/cm
0.600 ft-lb/in
73°F; ASTM D256
Descriptive Properties Value Comments
Characteristics Antistatic, Nucleating agent
Forms Pellets
Processing Methods Injection molding