Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.50 GPa | 218 ksi | |
Plastcom SLOVALEN PC 59 GB 10 PP, 10% glass beads FeaturesCompouded homopolymer PP, with the content of 10% chemically bound glass beads and modifier of mechanical properties. Increased strength in comparison with unfilled PP. Use in all industry s.. |
|||
Flexural Modulus | 1.50 GPa | 218 ksi | ISO 178 |
Premix Thermoplastics PRE-ELEC® PA 1412 Conductive Thermoplastic Compound PRE-ELEC® PA 1412 is a conductive thermoplastic compound based on polyamide 6. Conductivity is achieved by using conductive carbon black. In addition to a low electrical resistivity PRE-ELEC® PA 1.. |
|||
Flexural Modulus | 1.50 GPa | 218 ksi | ISO 178 |
Premix Thermoplastics PRE-ELEC® PP 1392 Carbon Black Filled Conductive Thermoplastic Compound PRE-ELEC® PP 1392 is a carbon black filled conductive thermoplastic compound based on polypropylene. In addition to a low electrical resistivity PRE-ELEC® PP 1392 has an excellent balance of mecha.. |
|||
Flexural Modulus | 1.50 GPa @Temperature 23.0 °C |
218 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYfill PP CIQ15020 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Modulus | 1.50 GPa @Temperature 90.0 °C |
218 ksi @Temperature 194 °F |
ISO 178, ASTM D790 |
Nilit Nilamon A3 H K8 40% Mineral Reinforced PA66 Description: Nilamon A3 H K8 combines good stiffness with low warpage. It is used for applications which need a degree of rigidity, particularly at higher temperatures, but which need to stay flat a.. |
|||
Flexural Modulus | >= 1.50 GPa | >= 218 ksi | ASTM D790 |
NIZHNEKAMSKNEFTEKHIM PE 2062T (62107) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Flexural Modulus | >= 1.50 GPa | >= 218 ksi | ASTM D790 |
NIZHNEKAMSKNEFTEKHIM PP 2641J (T31SE) Propylene Homopolymer Product obtained by polymerization of propylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation resistance when P.. |
|||
Flexural Modulus | 1.50 GPa | 218 ksi | ISO 178 |
SABIC Innovative Plastics LNP FARADEX MS003 PP LNP* FARADEX* MS003 is a compound based on Polypropylene resin containing 15% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Flexural Modulus | 1.50 GPa @Temperature 23.0 °C |
218 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYfill PPC K5040 E30 Polypropylene Copolymer, Mineral Reinforced, Elastomer Modified Information provided by Polykemi AB |
|||
Flexural Modulus | 1.50 GPa | 218 ksi | ISO 178 |
Iran Petrochemical (PCC) EP-N31MA Polypropylene EP-N31MA is a high ultra fluidity heterophasic copolymer for thin walled injection molding the products offers a good stiffness impact balance. Applications: packaging, house ware and garden furnitu.. |
|||
Flexural Modulus | 1.50 GPa | 218 ksi | ISO 178 |
Iran Petrochemical (PCC) X 30 S Polypropylene Film Polypropylene film with good optical propertiesApplications: film, packing food stuffs, stationary and textiles.Information provided by Iran Petrochemical Commercial Co. |
|||
Flexural Modulus | 1.50 GPa | 218 ksi | 1% Secant; ASTM D790 |
IRPC Polimaxx Polene N700P Polypropylene Homopolymer APPLICATION: BASE COMPONENT FOR COLORING RESIN |
|||
Flexural Modulus | 1.50 GPa | 218 ksi | ISO 178 |
Iran Petrochemical (PCC) EPV 31 RA Polypropylene A high fluidity heterophasic copolymer for thin wall injection molding exhibits high stiffness, relatively good impact residence.Applications: flower pots, containers, filters, house wares.Informati.. |
|||
Flexural Modulus | 1.50 GPa | 218 ksi | 1% secant at 0.05 in/min; ASTM D790A |
LyondellBasell Astryn BA905-74 Polypropylene Copolymer, Flame Retardant Key Features: medium high melt flow, medium high modulus, flame retardant, low specific gravity, good impact strengthApplications: battery jars, electrical componentsDescription: Astryn BA905-74 med.. |
|||
Flexural Modulus | 1.50 GPa | 218 ksi | ASTM D790A |
LyondellBasell Astryn BB725GC Polypropylene Copolymer, Mineral Filled Key Features: medium melt flow, medium high modulus, UV-stabilized, mineral-filled polypropylene copolymer, excellent impact and stiffness balance, good processability, good weatherability,Applicati.. |
|||
Flexural Modulus | 1.50 GPa | 218 ksi | ISO 178 |
LyondellBasell Hifaxâ„¢ HSBMR246 Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ HSBMR246 medium high melt flow, 1,500 MPa flexural modulus, paintable, mineral-filled thermoplastic elastomeric olefin (TEO) resin has an outstanding balance of physical pro.. |
|||
Flexural Modulus | 1.50 GPa | 218 ksi | |
SPS Guang Zhou SAMATâ„¢ 5000C Flame-retarded Polypropylene Characteristic: Good flame retardance, non-halogen, high flow properties, high impact, high heat resistance, meets the requirements of RoHs and PaHsApplications: E/E applianceInformation Provided by.. |
|||
Flexural Modulus | 1.50 GPa | 218 ksi | |
SPS Guang Zhou SAMATâ„¢ 5003 Flame-retarded Polypropylene Characteristic: Good chemical resistance, good mechanical properties, excellent long-term thermal stabilityApplications: E/E applianceInformation Provided by SPS (Guang Zhou) Ltd. |
|||
Flexural Modulus | 1.50 GPa | 218 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Thermocomp MX05038 PP (Europe-Africa-Middle East) Polypropylene compound, containing miniral. Added features include High ImpactThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Modulus | 1.50 GPa | 218 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-LOY K3000SZ Acetal Copoly (Asia Pacific) LNP* Stat-loy* K3000SZ is a compound based on Acetal Copolymer resin containing Anti-Static. Added features of this material include: Antistat. |
|||
Flexural Modulus | 1.50 GPa | 218 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics XYLEX FXY330DF PC+POLYESTER Polyester+PC alloy. Diffusion Effect. Color package may affect performance. |
|||
Flexural Modulus | 1.50 GPa | 218 ksi | ASTM D790 |
Teknor Apex Sinelec CCB2765 General Purpose Polystyrene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Features: Electrically Conductive Uses: Sheets Forms: Pellets Processing Method: Injection Method; Sheet Extrusion; Vac.. |
|||
Flexural Modulus | 1.50 GPa | 218 ksi | ISO 178 |
Borealis HD822CF Polypropylene HD822CF is a polypropylene homopolymer. This grade is suitable for the manufacturing of unoriented films on cast and tubular quench film lines. Applications: food packaging, lamination films, statio.. |
|||
Flexural Modulus | 1.50 GPa | 218 ksi | ASTM D790 |
Unitika M1030B PA6, Conditioned Nano composite nylonInformation provided by Unitika Ltd. |
|||
Flexural Modulus | 1.50 GPa | 218 ksi | ISO 178 |
Total PPC 10641 Polypropylene, Heterophasic Copolymer, Injection Molding Polypropylene PPC 10641 is a nucleated antistatic heterophasic copolymer with high Melt Flow index of 44 g/10 min.Polypropylene PPC 10641 is characterized by high fluidity with good mechanical prope.. |
|||
Flexural Modulus | 1.50 GPa | 218 ksi | ISO 178 |
DuPont Performance Polymers Crastin® ST820 BK503 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced Polybutylene Terephthalate with Excellent Impact Resistance Crastin ST820 BK503 is an unreinforced Super Tough black polybutylene terephthalate resin for injection molding.Information p.. |
|||
Flexural Modulus | 1.50 GPa | 218 ksi | 1% secant; ASTM D790 |
Braskem H 201 Injection Molding Polypropylene Description: H 201 is a high melt flow rate additivated homopolymer suitable for injection molding and fiber extrusion applications. This product exhibits excellent processability with good melt sta.. |
|||
Flexural Modulus | 1.50 GPa | 218 ksi | XY direction; ASTM D790 |
ALM PA 650 Nylon 12 SLS Prototyping Polymer Combines strength, durability (high impact) and chemical resistance and produces strong, durable, end use prototype parts. SL parts are less porous, more precise and have less noticeable build lines.. |
|||
Flexural Modulus | 1.50 GPa | 218 ksi | At 2 mm/min; ISO 178 |
Borealis Daplen™ EE103AE TPO Compound Daplen EE103AE is a 10% mineral and elastomer modified polypropylene compound intended for injection molding. Daplen EE103AE is a material with excellent impact /stiffness ratio. Thanks to its low .. |
|||
Flexural Modulus | 1.50 GPa | 218 ksi | ISO 178 |
Unipetrol PP MONSTEN® GB 218 Polypropylene Homopolymer Applications include injection molding and fibers. Anti Gasfading stabilization. Homopolymer.Information provided by Unipetrol RPA |