Material Notes:
LNP* FARADEX* MS003 is a compound based on Polypropylene resin containing 15% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.
Physical Properties Metric English Comments
Density 1.01 g/cc
0.0365 lb/in³
ASTM D792
1.01 g/cc
0.0365 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.012 cm/cm

@Time 86400 sec
0.012 in/in

@Time 24.0 hour
ISO 294
Linear Mold Shrinkage, Transverse 0.013 cm/cm

@Time 86400 sec
0.013 in/in

@Time 24.0 hour
ISO 294
Mechanical Properties Metric English Comments
Tensile Strength at Break 15.0 MPa
2180 psi
ASTM D638
15.0 MPa
2180 psi
ISO 527
Tensile Strength, Yield 19.0 MPa
2760 psi
ASTM D638
21.0 MPa
3050 psi
ISO 527
Elongation at Break 72 %
72 %
ISO 527
88.4 %
88.4 %
ASTM D638
Elongation at Yield 5.2 %
5.2 %
ISO 527
6.2 %
6.2 %
ASTM D638
Tensile Modulus 1.19 GPa
173 ksi
50 mm/min; ASTM D638
1.30 GPa
189 ksi
1 mm/min; ISO 527
Flexural Strength 27.0 MPa
3920 psi
ASTM D790
32.0 MPa
4640 psi
ISO 178
Flexural Modulus 1.19 GPa
173 ksi
ASTM D790
1.50 GPa
218 ksi
ISO 178
Izod Impact, Notched 2.67 J/cm
5.00 ft-lb/in
ASTM D256
Izod Impact, Unnotched 12.26 J/cm
22.97 ft-lb/in
ASTM D4812
Izod Impact, Notched (ISO) 25.0 kJ/m²
11.9 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 80.0 kJ/m²
38.1 ft-lb/in²
80*10*4; ISO 180/1U
Impact Test 22.0 J
16.2 ft-lb
Multiaxial Impact; ISO 6603
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 104 µm/m-°C

@Temperature -40.0 - 40.0 °C
57.8 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
143 µm/m-°C

@Temperature -40.0 - 40.0 °C
79.4 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow 97.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
54.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
170 µm/m-°C

@Temperature -40.0 - 40.0 °C
94.4 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °C
203 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
92.0 °C

@Thickness 3.20 mm
198 °F

@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 56.0 °C
133 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
53.0 °C

@Thickness 3.20 mm
127 °F

@Thickness 0.126 in
unannealed; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 10000 ohm-cm
10000 ohm-cm
ASTM D257
Surface Resistance 1000 ohm
1000 ohm
ASTM D257
Shielding Effectiveness 50 - 65 dB

@Thickness 3.00 mm
50 - 65 dB

@Thickness 0.118 in