Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Teknor Apex Sinelec CCB2765 General Purpose Polystyrene

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Molded, Unreinforced
Manufacturer Teknor Apex Company
Trade Name Sinelec
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex Sinelec CCB2765 General Purpose Polystyrene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Availability: Africa & Middle East; Latin America; Asia Pacific; South America Features: Electrically Conductive Uses: Sheets Forms: Pellets Processing Method: Injection Method; Sheet Extrusion; Vacuum FormingInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
ASTM D792
Linear Mold Shrinkage 0.0040 cm/cm
0.0040 in/in
ASTM D955
Melt Flow 5.00 g/10 min

@Load 10.0 kg,
Temperature 200 °C
5.00 g/10 min

@Load 22.0 lb,
Temperature 392 °F
ASTM D1238
100 g/10 min

@Load 21.6 kg,
Temperature 200 °C
100 g/10 min

@Load 47.6 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 20.0 MPa
2900 psi
ASTM D638
Elongation at Break 10 %
10 %
ASTM D638
Flexural Strength 28.0 MPa
4060 psi
ASTM D790
Flexural Modulus 1.50 GPa
218 ksi
ASTM D790
Izod Impact, Notched 1.12 J/cm

@Temperature 22.8 °C
2.10 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 75.0 °C
167 °F
Unannealed; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 1e+05
1e+05
ASTM D257
Surface Resistance 1e+05
1e+05
ASTM D257