Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer IRPC Polimaxx
Trade Name Polene
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF IRPC Polimaxx Polene N700P Polypropylene Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
APPLICATION: BASE COMPONENT FOR COLORING RESIN
Physical Properties Metric English Comments
Particle Size 700 µm
700 µm
S1010-2802-T20
Melt Flow 11 g/10 min

@Load 2.16 kg,
Temperature 230 °C
11 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 107
107
ASTM D785
Tensile Strength, Yield 36.0 MPa
5220 psi
ASTM D638
Elongation at Yield 26 %
26 %
ASTM D638
Flexural Modulus 1.50 GPa
218 ksi
1% Secant; ASTM D790
Charpy Impact, Notched 0.290 J/cm²

@Temperature 23.0 °C
1.38 ft-lb/in²

@Temperature 73.4 °F
DIN 53453
Thermal Properties Metric English Comments
Heat Distortion Temperature 110 °C
230 °F
ASTM D648