Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 11.6 GPa @Temperature 23.0 °C |
1680 ksi @Temperature 73.4 °F |
ISO 178 |
Solvay Specialty Polymers Amodel® A-1133 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resistance.. |
|||
Flexural Modulus | 11.6 GPa | 1680 ksi | 5 mm/min; ISO 178 |
Gromax CFG45-PN11N1 Nylon 6 46% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Flexural Modulus | 11.6 GPa | 1680 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP OFL36 PPS - Linear LNP* LUBRICOMP* OFL36 is a compound based on PPS - Linear resin containing 30% Glass Fiber, 15% PTFE. Added features of this grade include: Wear Resistant. |
|||
Flexural Modulus | 11.6 GPa | 1680 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP OFL36XXC PPS - Linear LNP* LUBRICOMP* OFL36XXC is a compound based on PPS - Linear resin containing 30% Glass Fiber, 15% PTFE. Added features of this grade are: Wear Resistant. |
|||
Flexural Modulus | 11.6 GPa | 1680 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP RFP38 PA6.6 LNP* LUBRICOMP* RFP38 is a compound based on Nylon 66 containing 40% Glass Fiber, 15% PTFE/Silicone. Added feature of this grade is: Wear Resistant. |
|||
Flexural Modulus | 11.6 GPa @Temperature 23.0 °C |
1680 ksi @Temperature 73.4 °F |
ISO 178 |
Solvay Specialty Polymers Amodel® AE-1133 Polyphthalamide (PPA), 33% Glass Fiber Amodel® AE-1133 is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) designed to work in the modern automotive electrical environment. It has a high heat deflection temperature, high .. |
|||
Flexural Modulus | 11.6 GPa | 1680 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON EX03319C PEI (Asia Pacific) LNP* Stat-Kon* EX03319C is a polyetherimide compound reinforced with carbon fiber for good stiffness, dimension stability and has extremely high level of cleanliness for the most demanding applicati.. |
|||
Flexural Modulus | 11.6 GPa | 1680 ksi | ASTM D790 |
Techmer ES Luriblend® PA6 CF30 TL15 BK 30% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAdditive: PTFE Lubricant (15%)Features: Low Friction, Good Wear Resistance and LubricatedAppearance: .. |
|||
Flexural Modulus | 11.58 GPa | 1680 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp RF0069RS PA 66 LNP THERMOCOMP* RF0069RS is a compound based on Nylon 66 resin containing Glass Fiber, Mold Release, Flame Retardant. Added features of this material include: Easy Release.This data was supplied by.. |
|||
Flexural Modulus | 11.6 GPa @Temperature 23.0 °C |
1680 ksi @Temperature 73.4 °F |
ISO 178 |
Solvay Specialty Polymers Amodel® A-1133 HS Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® A-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resist.. |
|||
Flexural Modulus | 11.6 GPa | 1680 ksi | ASTM D790 |
Plenco 08133 Polyester BMC, Compression Molded PLENCO 08133 is a renumber of PlasGlas 10313. PLENCO 08133 is a general purpose polyester bulk molding compound that is characterized by adding utility to a number of applications. Because of its co.. |
|||
Flexural Modulus | 11.6 GPa | 1680 ksi | ISO 178 |
Polyram PlusTek PA313G43 Nylon 66 for Injection Molding, 43% Glass Fiber Reinforced, Heat Stabilized Heat stabilized, 43% Glass fiber reinforced Nylon 6.6 for injection molding applications.Information provided by Polyram. |
|||
Flexural Modulus | 11.6 GPa | 1680 ksi | ISO 178-93 |
Wellman Wellamid® GF1662-GY1 43% Glass Fiber Reinforced, Engineering Grade Nylon 66/6 Description: Glass Fiber Reinforced, Engineering Grade Nylon 66/6Information provided by Wellman. |
|||
Flexural Modulus | 11.6 GPa | 1680 ksi | ISO 178 |
Wellman Wellamid® GF43-66/6 XE-N 43% Glass Fiber Reinforced Nylon 66/6, Lubricated & Heat Stabilized Typical Applications: Machinery gear trains and linkage, conveyor belt links, fasteners, auto under hood and door parts, automotive door handles, appliance parts, sporting goods, lawn and garden equ.. |
|||
Flexural Modulus | 11.6 GPa | 1680 ksi | ASTM D790 |
Toyobo VYLOPET® EMC132-02 Injection Molding Polyester Resin, Flame Resistant Applications: Relay partsFeatures: Excellent arc resistanceFlame resistanceInformation provided by Toyobo. |