Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 11.5 GPa | 1670 ksi | ISO 178 |
PolyOne OnForce™ LFT NN-40LGF/000 HS Natural Polyamide 66 (Nylon 66) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Flexural Modulus | 11.5 GPa | 1670 ksi | ISO 178 |
Victrex® PEEK 150GL30 30% Glass Fiber Reinforced Product Description: High performance thermoplastic material, 30% glass fibre reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact c.. |
|||
Flexural Modulus | 11.5 GPa | 1670 ksi | ISO 178 |
Victrex® PEEK 450FC30 General Purpose Product Description: High performance thermoplastic material, 30% reinforced with carbon fibre / graphite / PTFE PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and ext.. |
|||
Flexural Modulus | 11.5 GPa | 1670 ksi | ISO 178 |
Victrex® PEEK 90GL30 BLACK EU 30% Glass Fiber Filled, PolyEtherEtherKetone High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, very easy flow, FDA and EU food contact compliant, .. |
|||
Flexural Modulus | 11.5 GPa | 1670 ksi | ISO 178 |
Solvay Specialty Polymers Ixef® 1002 Polyarylamide (PARA)
(Unverified Data**) Ixef 1002 is a 30% glass-fiber reinforced, general purpose polyarylamide compound which exhibits high strength and rigidity, outstanding surface finish, and excellent creep resistance. - Black: Ixef.. |
|||
Flexural Modulus | 11.5 GPa | 1670 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP RCL34 PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RCL34 is a compound based on Nylon 66 resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Flexural Modulus | 11.5 GPa | 1670 ksi | ISO 178 |
Solvay Specialty Polymers Amodel® AS-1935 HS Polyphthalamide (PPA), 35% Glass Fiber Amodel® AS-1935 HS is a 35% glass reinforced grade of polyphthalamide (PPA) resin developed specifically for improved performance in a 50/50 ethylene glycol and water environment. This material e.. |
|||
Flexural Modulus | 11.5 GPa | 1670 ksi | ISO 178 |
Solvay Specialty Polymers Ixef® 1002 Polyarylamide (PARA), 30% Glass Fiber Ixef® 1002 is a 30% glass-fiber reinforced, general purpose polyarylamide compound which exhibits high strength and rigidity, outstanding surface finish, and excellent creep resistance.Features: .. |
|||
Flexural Modulus | 11.5 GPa | 1670 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON KE004 Acetal Copoly LNP* STAT-KON* KE004 is a compound based on Acetal Copolymer resin containing 20% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Flexural Modulus | 11.5 GPa | 1670 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON KE004 Acetal Copoly (Asia Pacific) LNP* Stat-kon* KE004 is a compound based on Acetal Copolymer resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Flexural Modulus | 11.5 GPa | 1670 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics LNP Stat-kon WEF42 PET/PBT LNP Stat-Kon WCF-1006 is a compound based on PET/PBT resin containing carbon and glass fiber reinforcements.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 11.5 GPa | 1670 ksi | ASTM D790 |
Techmer ES Luriblend® PA6 CF30 TS15 BK 30% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAdditive: PTFE Lubricant (15%) and Silicone LubricantFeatures: LubricatedAppearance: Natural ColorPro.. |
|||
Flexural Modulus | 11.5 GPa | 1670 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp PH0600A PA 6 LNP THERMOCOMP* PH0600A is a compound based on Nylon 6 resin. Added features of this material include: High Specific Gravity.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 11.5 GPa | 1670 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp PH0600A PA 6 (Asia Pacific) LNP* THERMOCOMP* PH0600A is a compound based on Nylon 6 resin. Added features of this material include: High Specific Gravity.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 11.5 GPa | 1670 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP RX09411H PA 66 LNP* Thermocomp* RX09411H is a compound based on Nylon 66 containing Proprietary Fillers. Characteristics are: Radiopacity and Healthcare. |
|||
Flexural Modulus | 11.5 GPa | 1670 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP WCP36 PBT (Europe-Africa-Middle East) LNP* LUBRICOMP* WCP36 is a compound based on Polybutylene Terephalate resin containing Carbon Fiber, PTFE, Silicone. Added features include; Internally Lubricated, Electrically Conductive. |
|||
Flexural Modulus | 11.5 GPa | 1670 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON EX07311P PEI (Asia Pacific) LNP Stat-kon* EX07311P is an easy flowing ESD-safe compound based on Polyetherimide resin. This compound is developed for good dimensional stability for use in ESD Tray for Backend Semicon and HDD t.. |
|||
Flexural Modulus | 11.5 GPa | 1670 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON REF42I PA 66 LNP* STAT-KON* REF42I is a compound based on Nylon 6/6 containing Proprietary Fillers. Added feature of this grade is: Electrically Conductive. |
|||
Flexural Modulus | 11.5 GPa | 1670 ksi | ASTM D790 |
Plenco 6310 Phenolic, Granular, Compression Molded PLENCO 06310 is a glass and mineral filled phenolic molding compound offering excellent heat resistance and dimensional stability. 06310 is available in black.Information supplied by Plenco. |
|||
Flexural Modulus | 11.5 GPa | 1670 ksi | dry; ISO 178 |
DSM Novamid® 1010GN2-30 NAT/BK37 PA6-GF30 FR(17) 30% Glass Reinforced, Flame Retardant |
|||
Flexural Modulus | 11.5 GPa | 1670 ksi | dry; ISO 178 |
DSM Stanyl® TE200F8 PA46-GF40 40% Glass Reinforced, Heat Stabilized, for E&E applications |
|||
Flexural Modulus | 11.5 GPa | 1670 ksi | dry; ISO 178 |
DSM Stanyl® TW271F8 (PA46+PTFE)-GF40 40% Glass Reinforced, Heat Stabilized, Wear and Friction Modified |
|||
Flexural Modulus | 11.5 GPa | 1670 ksi | ASTM D790 |
E-Polymers TEKAMID® TB120G45 , 45% Glass Fiber Reinforced PA6, DAM 45% Glass Fiber Reinforced, High Strength.Information provided by E-Polymers Co. Ltd. |
|||
Flexural Modulus | 11.5 GPa | 1670 ksi | DIN 52457 |
CP-Polymer-Technik Wellamid® 6000 CF 18 HWCP 18% Carbon Fiber Nylon 6, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Flexural Modulus | 11.5 GPa | 1670 ksi | SAE J949 |
Azdel SuperLite® SL550800-100 PP Resin Matrix / 55% Glass Fiber (3 mm Molded Thickness) AZDEL SuperLite® SL550800-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Flexural Modulus | 11.5 GPa | 1670 ksi | ASTM D790 |
A. Schulman ComAlloy Comtuf® 615 Nylon 6, Glass Reinforced, Impact Modified Data provided by the manufacturer, ComAlloy International Company.45% Glass Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been int.. |
|||
Flexural Modulus | 11.5 GPa | 1670 ksi | 2mm/min; ISO 178 |
Teijin Panlite® BN-8120R Improved Mold Release, Carbon Fiber Reinforced, Flame Resistant Polycarbonate Resin CF 20% reinforced grade, meeting UL 94 V-2. It has excellent strength, stiffness, heat resistance and electric conductivity. Other features are flame retardance, low molding shrinkage and dimensiona.. |
|||
Flexural Modulus | 11.5 GPa | 1670 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP RF0069XZ PA 66 LNP THERMOCOMP* RF0069XZ is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of this material include: Flame Retardant. |
|||
Flexural Modulus | 11.5 GPa | 1670 ksi | ASTM D790 |
LNP Thermocomp® UF-1006 A HS Polyphthalamide, Glass Fiber Reinforcement
(discontinued **) Features: Heat StabilizedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are sti.. |
|||
Flexural Modulus | 11.5 GPa @Temperature 23.0 °C |
1670 ksi @Temperature 73.4 °F |
ISO 178 |
Victrex® PEEK 150GL30 Black Polyetheretherketone, 30% Glass Fiber Reinforced Product Description:High performance thermoplastic material, 30% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact co.. |