Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 11.0 GPa | 1600 ksi | ISO 178 |
PolyOne OnForce™ LFT LF9200-5001 RS Natural Polyphenylene Sulfide (PPS) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Flexural Modulus | 11.0 GPa | 1600 ksi | |
Plastcom SLOVASTER® E GF 30 PBT, 30% glass fibre FeaturesPET for injection moulding, chemically reinforced with 30% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending.. |
|||
Flexural Modulus | 11.0 GPa | 1600 ksi | ASTM D790 |
Oxford Polymers 40GF 40% Glass Fiber Filled Polyetherimide for Extrusion and Injection Molding 40% Glass Fiber Filled Polyetherimide for Extrusion and Injection MoldingInformation provided by Oxford Polymers. |
|||
Flexural Modulus | 11.0 GPa | 1600 ksi | ASTM D790 |
Niche Polymer PA66GF43N Nylon 66, 43% Glass Fiber Filled Information provided by Niche Polymer |
|||
Flexural Modulus | 11.0 - 14.0 GPa | 1600 - 2030 ksi | Compression; ISO 178 |
Raschig Group DECAL® 572R Phenolic Glass-fiber reinforced phenolic molding compound. Exceptional heat resistance with regard to maintaining surface finish and mechanical properties, outstanding mechanical properties, excellent rotati.. |
|||
Flexural Modulus | 11.0 GPa | 1600 ksi | ASTM D790 |
PolyOne Nymax™ GF 1200 A 40 IM Black 13A Polyamide 66 (Nylon 66) The Nymax® GF 1200 Series of glass fiber-reinforced nylon 6/6 compounds have been specifically formulated for applications requiring high stiffness, tensile properties, heat resistance, and durabil.. |
|||
Flexural Modulus | 11.0 GPa | 1600 ksi | ASTM D790 |
Polymer Resources PEI-G40 Polyetherimide, 40% Glass Reinforced
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Flexural Modulus | 11.0 GPa | 1600 ksi | ASTM D790 |
PolyOne Edgetek® LCP-15GF/000 Liquid Crystal Polymer - 15% Fiber Glass
(discontinued **) Data provided by PolyOne. |
|||
Flexural Modulus | 11.0 GPa | 1600 ksi | |
Lehmann & Voss LUVOCOM® 65-8285 PP-copolymer, with carbon fiber Applications: Office communication.High-stiff parts with low creep.Electrically conductive, suitable for continuous discharging of statically generated electricity.Low warpage.Information provided b.. |
|||
Flexural Modulus | 11.0 GPa | 1600 ksi | ASTM D790 |
Kuraray Genestarâ„¢ GN2332 Nylon, 33% Glass Filled High Flow V-0 Grade. Improves flow-ability in thin-walled parts. Used for components requiring high-flowability, such as 0.3 mm pitch connectors. |
|||
Flexural Modulus | 11.0 GPa | 1600 ksi | |
MTI ThermoStran® PA66-40G Long Glass Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |
|||
Flexural Modulus | 11.0 GPa | 1600 ksi | ISO 178 |
Solvay TECHNYL® A 218 V43 Black 21 N PA66, 43% glass fiber, DRY Description: Polyamide PA66, reinforced with 43% of glass fiber, heat stabilized, for injection molding.Available in: North AmericaProduct Applications: TECHNYL® A 218 V43 is used in all sectors .. |
|||
Flexural Modulus | 11.03 GPa | 1600 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP OFL36A PPS - Branched LNP* LUBRICOMP* OFL36A is a compound based on PPS - Branched resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant. |
|||
Flexural Modulus | 11.0 GPa | 1600 ksi | ASTM D790 |
Solvay Specialty Polymers Amodel® AS-4133 HS Polyphthalamide (PPA), 33% Glass Fiber (Conditioned) Amodel® AS-4133 HS is a 33% glass reinforced, lubricated, heat stabilized grade of polyphthalamide (PPA) that offers fast cycle times and moldability in hot water molds. Testing conducted on samp.. |
|||
Flexural Modulus | 11.0 GPa | 1600 ksi | ASTM D790 |
Techmer ES Electrablend® PA6/6 03003 CF Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber ReinforcementAdditive: Lubricant, Impact Modifier and Heat StabilizerFeatures: Lubricated, Electrically Conductive, Impact.. |
|||
Flexural Modulus | 11.0 GPa | 1600 ksi | ASTM D790 |
Techmer ES HiFill® PA4/6 GF40 HS 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedTPCI# 9627150Information provided by T.. |
|||
Flexural Modulus | 11.03 GPa | 1600 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP DC0049XF PC (Asia Pacific) LNP* Thermocomp* DC0049XF is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Fiber. Added features of this material include: Electrically Conductive, , Flame Retardant. |
|||
Flexural Modulus | 11.0 GPa | 1600 ksi | GB/T 9341-2008 |
Sichuan Deyang Haton® hXGR41 Polyphenylene Sulfide Injection molding, high strengthInformation provided by Sichuan Deyang Chemical Co., LTD |
|||
Flexural Modulus | 11.0 GPa | 1600 ksi | 2 mm/min; ISO 178 |
Eurostar Staramide RF008U PA66/6, 40% Glass Filled, Injection Molded Staramide RF008U is a 40% Glass Fiber Reinforced Polyamide 66/Polyamide 6 Injection Molding Resin (also known as Staramide 66 C 40V S4)Information provided by Eurostar. |
|||
Flexural Modulus | 11.0 GPa | 1600 ksi | transverse; ISO 178 |
Bond Laminates TEPEX® dynalite 102-RGUD600(x)/47% Roving Glass – PA 6 Consolidated Composite Laminate Within the TEPEX® composite laminate, Polyamide 6 is a resin known for its toughness, stiffness, abrasion resistance, heat and chemical resistances. Roving E-Glass fibers have an excellent impact .. |
|||
Flexural Modulus | 11.0 GPa | 1600 ksi | ASTM D790 |
A. Schulman ComAlloy Voloy® 430 Glass Reinforced, PBT Alloy, Flame Retardant, UL Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 11.0 - 13.0 GPa | 1600 - 1890 ksi | Compression; ISO 178 |
Raschig Group DECAL® 152CL Phenolic Glass-fiber and mineral reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and mechanical properties. This product meet.. |
|||
Flexural Modulus | 11.0 GPa | 1600 ksi | ASTM-D790 |
Polyram Polytron P50B01 Homopolymer Polypropylene, Chemically Coupled 50% LGF A chemically coupled 50% LGF reinforced black PP, heat stabilized for high temperature applications such as under the hood automotive parts.Information provided by Polyram Ram On Ind. |