Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 10.4 GPa @Temperature 23.0 °C |
1510 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB SCANAMID 66 A53^ F43 Nylon 66, Glass Fiber Reinforced, Modified Information provided by Polykemi AB |
|||
Flexural Modulus | 10.4 GPa @Temperature 23.0 °C |
1510 ksi @Temperature 73.4 °F |
ISO 178 |
Solvay Specialty Polymers Amodel® A-1133 DW Polyphthalamide (PPA)
(discontinued **) Amodel A-1133 DW is a 33% glass-fiber reinforced polyphthalamide (PPA) grade approved for use with potable water in the United States, the United Kingdom and France. - Natural: A-1133 NT DW - Black:.. |
|||
Flexural Modulus | 10.4 GPa | 1510 ksi | ASTM D790 |
Plenco 51240 PET, Pellet, Injection Molded, Green
(discontinued **) PLENCO 51240 is an engineering grade glass reinforced flame retarded recycled polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed.Information supplied by P.. |
|||
Flexural Modulus | 10.4 GPa | 1510 ksi | ASTM D790 |
Solvay Specialty Polymers AvaSpire® AV-742 SL30 Polyaryletherketone (PAEK)
(Unverified Data**) AV-742 SL30 is a wear resistant grade of AvaSpire polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to outstanding wear re.. |
|||
Flexural Modulus | 10.4 GPa | 1510 ksi | ASTM D790 |
Solvay Specialty Polymers KetaSpire® KT-820 GF30 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-820 GF30 is a medium flow, 30% glass fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaSpire.. |
|||
Flexural Modulus | 10.4 GPa | 1510 ksi | ASTM D790 |
Mitsui AURUM® JGN6230 Thermoplastic Polyimide Resin, Crystalline
(discontinued **) AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i.. |
|||
Flexural Modulus | 10.4 GPa | 1510 ksi | ASTM D790 |
Plenco 506 Black Heat Resistant Mineral Filled Phenolic Molding Compound
(discontinued **) Plaslok 506 is a two-stage, mineral-filled phenolic molding compound. It is formulated for automotive ashtrays and for appliance applications such as utensil handles receiving repeated exposure to .. |
|||
Flexural Modulus | 10.4 GPa | 1510 ksi | ASTM D790 |
Plaslok 506 Black Heat Resistant Mineral Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 506 is a two-stage, mineral-filled ph.. |
|||
Flexural Modulus | 10.4 GPa @Temperature 23.0 °C |
1510 ksi @Temperature 73.4 °F |
ISO 178 |
Solvay Specialty Polymers Amodel® AS-4133 HS Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® AS-4133 HS is a 33% glass reinforced, lubricated, heat stabilized grade of polyphthalamide (PPA) that offers fast cycle times and moldability in hot water molds. Testing conducted on samp.. |
|||
Flexural Modulus | 10.4 GPa | 1510 ksi | ISO 178 |
Solvay Specialty Polymers Amodel® HFZ A-1133 L Polyphthalamide (PPA), 33% Glass Fiber Amodel® HFZ A-1133 L is a high-flow, 33% glass fiber reinforced polyphthalamide (PPA) grade.Features: Good Chemical Resistance; Good Creep Resistance; Good Dimensional Stability; Good Stiffness; .. |
|||
Flexural Modulus | 10.4 GPa | 1510 ksi | ASTM D790 |
Solvay Specialty Polymers AvaSpire® AV-742 SL30 Polyaryletherketone (PAEK) AV-742 SL30 is a wear resistant grade of AvaSpire® polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to outstanding wea.. |
|||
Flexural Modulus | 10.4 GPa | 1510 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP RF008 PA 66 (Asia Pacific) LNP Thermocomp RF008 is a compound based on PA66 resin containing glass fiber. It is used in many applications requiring high strength over weight performance. Also known as Thermocomp RF-1008 |
|||
Flexural Modulus | 10.41 GPa | 1510 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP RF008XXZ PA 66 LNP THERMOCOMP* RF008XXZ is a compound based on Nylon 66 resin containing 40% Glass Fiber. |
|||
Flexural Modulus | 10.4 GPa | 1510 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP LF008 PEEK (Asia Pacific) LNP* Thermocomp* LF008 is a compound based on Polyetheretherketone resin containing Glass Fiber. |
|||
Flexural Modulus | 10.4 GPa | 1510 ksi | ASTM D790 |
A. Schulman SCHULAMID® 66 GF33HS 33% Glass Fiber Reinforced, Heat Stabilized Nylon 66 Information provided by A. Schulman. |
|||
Flexural Modulus | 10.4 GPa | 1510 ksi | ISO 178 |
Polyplastics FR-PET® B3030FA Glass Fiber Reinforced Polyethylene Terephthalate (GF-PET), Slow burning, General purpose Information provided by PolyPlastics. |
|||
Flexural Modulus | 10.4 GPa | 1510 ksi | ISO 178 |
Polyplastics FR-PET® C3030FA Glass Fiber Reinforced Polyethylene Terephthalate (GF-PET), Slow burning, General purpose Information provided by PolyPlastics. |
|||
Flexural Modulus | 10.4 GPa | 1510 ksi | ASTM D790 |
A. Schulman SCHULAMID® 66 GF33HS 33% Glass Fiber Reinforced, Heat Stabilized Nylon 66 Information provided by A. Schulman. |
|||
Flexural Modulus | 10.4 GPa | 1510 ksi | ASTM D790 |
A. Schulman SCHULAMID® 66 GF33HS 33% Glass Fiber Reinforced, Heat Stabilized Nylon 66 Information provided by A. Schulman. |
|||
Flexural Modulus | 10.4 GPa | 1510 ksi | ASTM D790 |
A. Schulman SCHULAMID® 66 GF33HS 33% Glass Fiber Reinforced, Heat Stabilized Nylon 66 Information provided by A. Schulman. |
|||
Flexural Modulus | 10.4 GPa | 1510 ksi | ASTM D790 |
A. Schulman SCHULAMID® 66 GF33HS 33% Glass Fiber Reinforced, Heat Stabilized Nylon 66 Information provided by A. Schulman. |
|||
Flexural Modulus | 10.4 GPa | 1510 ksi | dry; ISO 178 |
DSM Novamid® 3010GN30 NAT PA66-GF30 FR(17) 30% Glass Reinforced, Flame Retardant |
|||
Flexural Modulus | 10.4 GPa | 1510 ksi | 2 mm/min; ISO 178 |
Eurostar Starflam RF0077E PA66, 35% Glass Filled, Injection Molded Starflam RF0077E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 66 Injection Molding Resin (also known as RF1007Z270)Information provided by Polymer T.. |
|||
Flexural Modulus | 10.4 GPa | 1510 ksi | ASTM D790 |
Ashley Polymers Ashlene® 528L-43G Nylon 66, 43% Glass Reinforced A general purpose 43% glass reinforced nylon resin.Data provided by the manufacturer |
|||
Flexural Modulus | 10.4 GPa | 1510 ksi | ASTM D790 |
A. Schulman ComAlloy Voloy® 688 Nylon 6/6, Glass Fiber/Bead Reinforced, Nylon 6/6 Alloy, Flame Retardant, UL Data provided by the manufacturer, ComAlloy International Company.45% Glass Fiber/Bead Reinforced. Halogen- and phosphorous-freeThe ComAlloy product line has been integrated into the A Schulman prod.. |
|||
Flexural Modulus | 10.4 GPa | 1510 ksi | Dry; ASTM D790 |
Asahi Kasei Leona® 14G33 33% Glass Filled Nylon 66 Enhanced strength and stiffness; with 33% GF. Superior heat aging resistance, fatigue resistance, and creep resistance.Applications:Mechanical and electrical parts, engine mounts and other under-the.. |
|||
Flexural Modulus | 10.4 GPa @Temperature 23.0 °C |
1510 ksi @Temperature 73.4 °F |
ISO 178 |
Solvay Specialty Polymers Amodel® AS-4133 HN Polyphthalamide (PPA), Dry, 33% Glass Fiber Reinforcement, Heat Stabilizer Amodel AS-4133 HN polyphthalamide (PPA) is a non-lubricated, heat stabilized grade that offers fast cycle times and is hot-water moldable. Typical applications include electrical and electronic comp.. |
|||
Flexural Modulus | 10.4 GPa @Temperature 23.0 °C |
1510 ksi @Temperature 73.4 °F |
ISO 178 |
Solvay Specialty Polymers Amodel® A-4133 L Polyphthalamide (PPA), Dry
(discontinued **) Amodel A-4133L polyphthalamide (PPA) is a 33% glass reinforced resin designed to offer high crystallinity when molded in water-cooled molds. Key properties include high heat resistance, reduced outg.. |