Mechanical Properties Metric English Comments
Flexural Modulus 7.76 GPa
1130 ksi
ASTM D790
PolyOne Nymax™ GMF 600 A 40 HS Natural Polyamide 6 (Nylon 6)
The Nymax® GMF 600 Series of compounds are based upon nylon 6 resins and select combinations of glass fiber and mineral reinforcements offering a unique balance of physical property and part perfor..
Flexural Modulus 7.80 GPa
1130 ksi
1.3 mm/min; ASTM D790
Ovation Polymers RIGITRON 20433 GF PBT, 33% Glass Reinforced
PBT - Glass reinforced (33 %), high tensile strength, stiffness and HDT. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All samples are prepared acco..
Flexural Modulus 7.80 GPa
1130 ksi
ISO 178, ASTM D790
Nilit Nilitop BT G4 FR C3 is a 20% Glass Fiber Reinforced, Flame Retardant PBT
Description: Nilitop BT G4 FR C3 is a 20% glass fiber reinforced, flame retardant PBT with halogens. The flame retardant does not contain PBB and PBDE, so it is compliant with the WEEE directive. It..
Flexural Modulus 7.80 GPa
1130 ksi
ISO 178
Nilit RECONYL B GV30 Recycled nylon 6 for injection molding, 30% glass fiber reinforced
Recycled nylon 6 for injection molding (available only in black).Information provided by Frisetta Polymer, which merged into Nilit Plastics
Flexural Modulus 7.80 GPa

@Temperature 23.0 °C
1130 ksi

@Temperature 73.4 °F
ISO 178
Polykemi AB SCANMID 6 B23^ E F30 Nylon 6, Glass Fiber Reinforced, Modified
Information provided by Polykemi AB
Flexural Modulus 7.76 GPa
1130 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Lexan® HFD4413 PC (Asia Pacific)
Lexan* HFD4413 is a 30% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release.
Flexural Modulus 7.79 GPa
1130 ksi
ISO 178
Solvay Specialty Polymers Amodel® A-4122 HR WH 117 Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-4122 HR resin is a 22% glass reinforced polyphthalamide (PPA), designed to provide high crystallinity when molded in water-cooled molds. This material exhibits high heat resistance, high st..
Flexural Modulus 7.79 GPa
1130 ksi
ISO 178
Solvay Specialty Polymers Amodel® AT-1125 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AT-1125 HS polyphthalamide (PPA) is a toughened, heat stabilized 25% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional stabi..
Flexural Modulus 7.79 GPa
1130 ksi
ASTM D790
PolyOne Edgetek® AS-40GF/000 Acrylonitrile Butadiene Styrene (ABS), Glass Filled  (discontinued **)
Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Flexural Modulus 7.80 GPa
1130 ksi
ASTM D790
Plenco Valite 4224 Novolac Phenolic, Granular, Transfer Molded  (discontinued **)
This Valite product has been replaced by Plenco 4224. Data provided by Plenco.VALITE 4224 is a brown, two stage, general purpose phenolic molding compound. It has good electrical and moldability ch..
Flexural Modulus 7.80 GPa
1130 ksi
Idemitsu Kosan Xarec® D132 SPS, 25% Glass Filled
Flexural Modulus 7.80 GPa
1130 ksi
conditioned, 2 mm/min; ISO 178-A
Lanxess Durethan® AKV 35 LT H3.0 000000 Nylon 66, 35% Glass Fiber
PA 66, 35% glass fiberInformation provided by LANXESS.
Flexural Modulus 7.80 GPa
1130 ksi
2mm/min; ASTM D790
Kingfa PA6-G30 N101 30% Glass Fiber Reinforced PA6 (general purpose)
Features:Good size stabilityLow tendency to wrapHigh mechanical propertiesGood low temperature resistanceGood surfaceExcellent balance propertiesApplications:Injection moldingAutomobile partsPower t..
Flexural Modulus 7.80 GPa
1130 ksi
2 mm/min; ISO 178-A
Lanxess Pocan® KU 2-7241 000000 PBT, 25% Glass Fiber
PBT, 25% glass fibers, injection molding, flame retardant, improved impact strengthInformation provided by LANXESS.
Flexural Modulus 7.80 GPa
1130 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP LUBRICOMP RFL36 PA 66 (Europe-Africa-Middle East)
LNP* Lubricomp* RFL36 is a compound based on Nylon 66 resin containing Glass Fiber, PTFE.
Flexural Modulus 7.79 GPa
1130 ksi
ASTM D790
SABIC Innovative Plastics LNP STAT-KON DE003ER PC
LNP STAT-KON* DE003ER is a compound based on Polycarbonate resin containing 15% Carbon Fiber. Added features of this material include: Easy Molding. Mold Release, Statically Conductive.
Flexural Modulus 7.79 GPa
1130 ksi
6.4 mm; ASTM D790
SABIC Innovative Plastics LNP STAT-KON Noryl_FMC3008A PPE+HIPS (Europe-Africa-Middle East)
LNP* Stat-kon* Noryl_FMC3008A compound is a 30% carbon fiber/glass/mineral filled, static dissipative, foamable resin. UL94 V1 rated. Property values at 20% weight reduction, 0.250"" wall.
Flexural Modulus 7.76 GPa
1130 ksi
ISO 178
SABIC Innovative Plastics LNP STAT-KON WE002 PBT
LNP STAT-KON* WE002 is a compound based on PBT resin containing 10% Carbon Fiber. Added features of this material include: Electrically Conductive.
Flexural Modulus 7.79 GPa
1130 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP IF006L PA6.12
LNP* THERMOCOMP* IF006L is a compound based on Nylon 6/12 resin containing 30% Glass Fiber. Added features of this material include: Low Extractible.
Flexural Modulus 7.80 GPa
1130 ksi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP PH0460A PA 6
LNP* THERMOCOMP* PH0460A is a compound based on Nylon 6. Added feature of this material is: High Specific Gravity.
Flexural Modulus 7.80 GPa
1130 ksi
ASTM D790
SABIC Innovative Plastics LNP VERTON MV008S PP (Europe-Africa-Middle East)
LNP VERTON* MV008S is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled, Heat Stabilized.
Flexural Modulus 7.80 GPa
1130 ksi
ISO 178
Polyram PlusTek RA331G6 Nylon 66 for Injection Molding, 30% Glass-Fiber Reinforced
30% Glass-fiber reinforced Nylon 66 for injection molding applications.Information provided by Polyram.
Flexural Modulus 7.80 GPa
1130 ksi
ISO 178-93
Wellman EcoLon® MRGF1878-BKJA6A Nylon 6, 30% Mineral/Glass Reinforced
Ford JA6A color matchedAll information provided by Wellman Engineered Resins.
Flexural Modulus 7.79 GPa
1130 ksi
ASTM D790
Westlake Plastics Norylux™ Modified Polyphenylene Oxide 30% glass filled
Norylux modified PPO is a strong, engineering plastic with outstanding mechanical, thermal, and electric properties. Low moisture absorption and low thermal expansion make Norylux one of the most d..
Flexural Modulus 7.80 GPa
1130 ksi
ASTM D790
Plenco 4548 Phenolic, Granular, Injection Molded
PLENCO 04548 is a heat resistant mineral filled phenolic molding compound, offering fast cure rates and hot rigidity. Type ASTM 5948 CFG, and UL recognized under component file E40654. 04548 is avai..
Flexural Modulus 7.80 GPa
1130 ksi
2 mm/min; ISO 178
Eurostar Staramide BG5 PA6, 25% Glass Filled, Injection Molded
BG5 is a 25% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
Flexural Modulus 7.80 GPa
1130 ksi
ASTM D790
A. Schulman ComAlloy Hiloy® 104 Polypropylene, Glass Reinforced
Data provided by the manufacturer, ComAlloy International Company.40% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Flexural Modulus 7.80 GPa
1130 ksi
ASTM D790
Ashley Polymers Ashlene® 79MGS Nylon 6, 40% Glass Mineral reinforced
A 40% glass mineral reinforced Nylon 6 with good dimensional stability, stiffness, sink and warp resistance. Modified for improved surface appearance.Data provided by the manufacturer
Flexural Modulus 7.76 GPa
1130 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics NORYL FE1630PW PPE+PS (Europe-Africa-Middle East)
Noryl* FE1630PW Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability; this grade has been developed for fluid en..