Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plenco 4548 Phenolic, Granular, Injection Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Novolac, Mineral Filled
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Plenco 4548 Phenolic, Granular, Injection Molded.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
PLENCO 04548 is a heat resistant mineral filled phenolic molding compound, offering fast cure rates and hot rigidity. Type ASTM 5948 CFG, and UL recognized under component file E40654. 04548 is available in black and brown.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.660 g/cc
0.0238 lb/in³
ASTM D1895
Density 1.48 g/cc
0.0535 lb/in³
ASTM D792
Water Absorption 0.236 %
0.236 %
ASTM D570
Linear Mold Shrinkage 0.0086 cm/cm
0.0086 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 79
79
ASTM D785
Tensile Strength, Ultimate 54.0 MPa
7830 psi
ASTM D638
Elongation at Break 0.74 %
0.74 %
ASTM D638
Tensile Modulus 8.20 GPa
1190 ksi
ASTM D638
Flexural Strength 90.0 MPa
13100 psi
ASTM D790
Flexural Modulus 7.80 GPa
1130 ksi
ASTM D790
Compressive Strength 183 MPa
26500 psi
ASTM D695
Poissons Ratio 0.35
0.35
ASTM D638
Shear Modulus 3.04 GPa
441 ksi
Calculated
Izod Impact, Notched 0.166 J/cm
0.311 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.183 J/cm²
0.871 ft-lb/in²
ASTM D256
Impact 90
90
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
CTE, linear 56.0 µm/m-°C

@Temperature 40.0 - 130 °C
31.1 µin/in-°F

@Temperature 104 - 266 °F
TMA; ASTM E831
Maximum Service Temperature, Air 202 °C
396 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 157 °C
315 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
Oxygen Index 26.5 %
26.5 %
ASTM D2863
Shrinkage 0.34 %
0.34 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 2.40e+11 ohm-cm
2.40e+11 ohm-cm
ASTM D247
Dielectric Constant 5.0
5.0
ASTM D150
Dielectric Strength 11.0 kV/mm
279 kV/in
Short Time; ASTM D149
Dissipation Factor 0.054
0.054
ASTM D150
Arc Resistance 158 sec
158 sec
ASTM D495
Comparative Tracking Index 175 V
175 V
ASTM D3638
Users viewing this material also viewed the following: