Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 8.10 GPa | 1170 ksi | |
Plastcom SLOVAMID 66 Y 35 FRY 7 PA66, 35% mineral filling FeaturesPA 66 for injection moulding, chemically reinforced with 35 % mineral filler and non-halogen flame retardant, with heat resistance and nonflammability, achieves V 0 /3.2 mm/ in accordance wi.. |
|||
Flexural Modulus | 8.10 GPa | 1170 ksi | ISO 178 |
Nilit FRIANYL B63 W-GV35 Nylon 6 for injection molding, 35% glass fiber reinforced Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Modulus | 8.10 GPa @Temperature 23.0 °C |
1170 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB SCANAMID 66 A12^ F30 TF15 Nylon 66, Glass Fiber Reinforced, Modified Information provided by Polykemi AB |
|||
Flexural Modulus | 8.10 GPa | 1170 ksi | ASTM D790 |
Parker Chomerics PREMIER™ A230-ST EMI Shielding Plastic Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer .. |
|||
Flexural Modulus | 8.10 GPa | 1170 ksi | ISO 178 |
Radici Radilon® ARV300 (dry) Nylon 66 30% Glass-fiber reinforcedInformation provided by Radici group. |
|||
Flexural Modulus | 8.10 GPa | 1170 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP DFL36E PC (Europe-Africa-Middle East) LNP* LUBRICOMP* DFL36E is a compound based on Polycarbonate resin containing Glass Fiber, PTFE. Added features include; Internally Lubricated, Easy Molding. |
|||
Flexural Modulus | 8.10 GPa | 1170 ksi | ASTM D790 |
Solvay Specialty Polymers Amodel® A-4122 LS WH678 Polyphthalamide (PPA)
(Unverified Data**) Amodel A-4122 LS is a 22% glass fiber reinforced, light-stabilized, high-reflectivity white grade of Amodel polyphthalamide (PPA). It is designed to provide high crystallinity when molded in water-c.. |
|||
Flexural Modulus | 8.10 GPa | 1170 ksi | ASTM D790 |
LATI LAESTRA E01 G/30 30% Glass Fiber Reinforced, Elastomer Modified Syndiotactic Polystyrene (SPS)
(disconti Description: Laestra compounds are syndiotactic polystyrene (SPS) products. SPS is a polymer offering a combination of properties unavailable with other materials. It exhibits a melting point of 270.. |
|||
Flexural Modulus | 8.10 GPa | 1170 ksi | ISO 178 |
Nilit FRIANYL B63 GV35 Nylon 6 for injection molding, 35% glass fiber reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Modulus | 8.10 GPa | 1170 ksi | ASTM D790 |
Albis Plastics Polyamide 6/66 PA 152 GF30/02 BK8-1114 Black 30% Glass Fiber
(discontinued **) Semi-crystalline Nylon 6/66 (PA6/66)Characteristics: Industrial GradeApplications: Office Furniture, Gear, Housings and ConnectorsProcessing: Injection Molding (Melt Temperature: 465 -555°F, Mold .. |
|||
Flexural Modulus | 8.10 GPa | 1170 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Lubricomp JX91055 PES (Europe-Africa-Middle East) LNP* LUBRICOMP* JX91055 is a compound based on Polyethersulfone resin containing Carbon Fiber and Proprietary Lubricant . Added features include Internally Lubricated and Electrically Conductive.Thi.. |
|||
Flexural Modulus | 8.10 GPa | 1170 ksi | ASTM D790 |
Solvay Specialty Polymers Amodel® A-4122 LS WH678 Polyphthalamide (PPA), 22% Glass Fiber Amodel® A-4122 LS is a 22% glass fiber reinforced, light-stabilized, high-reflectivity white grade of Amodel polyphthalamide (PPA). It is designed to provide high crystallinity when molded in wat.. |
|||
Flexural Modulus | 8.10 GPa | 1170 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Stat-kon DCL33 PC (Europe-Africa-Middle East) LNP* Stat-kon* DCL4033 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP .. |
|||
Flexural Modulus | 8.10 GPa | 1170 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Stat-kon ZEL34XXC PPE+PS (Europe-Africa-Middle East) LNP* Stat-kon* ZEL34XXC is a compound based on PPE+PS Blend resin containing Carbon Fiber, PTFE. Added features include : Electrically Conductive , Internally Lubricated.This data was supplied by S.. |
|||
Flexural Modulus | 8.10 GPa | 1170 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP RF007H PA 66 LNP* Thermocomp* RF007H is a compound based on Nylon 66 containing glass fiber. Added feature includes: Healthcare. |
|||
Flexural Modulus | 8.10 GPa | 1170 ksi | 2 mm/min; ISO 178 |
Sax Polymers SAXAMID 126F6T3 Nylon 6, 30% Glass Fiber and PTFE SAXAMID 126F6T3 is a polyamide 6 injection-molding-grade reinforced with 30% glass fibers and 15% PTFE. Because of its high strength and stiffness this grade is often used for stressed parts requiri.. |
|||
Flexural Modulus | 8.10 GPa | 1170 ksi | ASTM D790 |
Plenco 00732 Melamine-Phenolic, Granular, Transfer Molded PLENCO 00732 is a melamine-phenolic copolymer molding compound, exhibiting excellent electrical and flame resistant properties. Type ASTM 5948 CMG, and UL recognized under component file E40654. 007.. |
|||
Flexural Modulus | 8.10 GPa | 1170 ksi | ASTM D790 |
Plenco 2369 Phenolic, Granular, Compression Molded PLENCO 02369 is a general purpose, organic filled phenolic molding compound, formulated to minimize the generation of free ammonia for applications that are sensitive to such formation. PLENCO 02369.. |
|||
Flexural Modulus | 8.10 GPa | 1170 ksi | ASTM D790 |
Plenco 2482 Phenolic, Granular, Transfer Molded PLENCO 02482 is a general purpose, organic filled phenolic molding compound offering excellent mechanical strength while maintaining dielectric properties at elevated humidity levels. UL recognized .. |
|||
Flexural Modulus | 8.10 GPa | 1170 ksi | ISO 178 |
Polyram PlusTek RA303G33 Nylon 66 for Injection Molding, 33% Glass Fiber Reinforced, Heat Stabilized, Hydrolysis Resistant 33% Glass fiber reinforced, heat stabilized and hydrolysis resistant Nylon 66 for injection molding applications.Information provided by Polyram. |
|||
Flexural Modulus | 8.10 GPa | 1170 ksi | cond; ISO 178 |
DSM EcoPaXX® Q-X07209 PA410-I-GF40 % Glass Reinforced, Impact Modified |
|||
Flexural Modulus | 8.10 GPa | 1170 ksi | cond; ISO 178 |
DSM Novamid® 3010GN30 NAT PA66-GF30 FR(17) 30% Glass Reinforced, Flame Retardant |
|||
Flexural Modulus | 8.10 GPa | 1170 ksi | 2 mm/min; ISO 178 |
Eurostar Starflam RF0057P PA66/6, 25% Glass Filled, Injection Molded Starflam RF0057P is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 66/6 Injection Molding Resin (also known as RF1005Z270EM)Information provided by Polym.. |
|||
Flexural Modulus | 8.10 GPa | 1170 ksi | 2 mm/min; ISO 178 |
Eurostar Starflam RFK517E PA66, Glass/Mineral Fiber Reinforced, Flame Retardant, Injection Molding Starflam RFK517E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Mineral Filled, Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Modulus | 8.10 GPa | 1170 ksi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 413 Polyester - PBT, Glass Reinforced Data provided by the manufacturer, ComAlloy International Company.33% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 8.10 GPa | 1170 ksi | ASTM D790 |
Adell DR-16 30% Glass Reinforced Polycarbonate |
|||
Flexural Modulus | 8.10 GPa | 1170 ksi | Dry; ASTM D790 |
Asahi Kasei Leona® 13G25 25% Glass Filled Nylon 66 Enhanced strength, stiffness and durability; with 25% GF.Applications:Automotive parts Information provided by Asahi Kasei |