Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 6.20 GPa | 899 ksi | |
Plastcom SLOVALEN PH 69 GF 45 PP, 45% glass fibre FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 45% glass fibre, contains the modifier of mechanical properties.Thermo stable. Increased strength in comparison wit.. |
|||
Flexural Modulus | 6.20 GPa @Temperature 23.0 °C |
899 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB SCANBLEND P AP2060 F20 PBT/ASA, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Flexural Modulus | 6.20 GPa | 899 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1520A PC LNP* Lubricomp* Lexan_LF1520A compound is a 20% glass reinforced, 15% PTFE filled PC. Flame retardant and wear resistant. Tight tolerances. |
|||
Flexural Modulus | 6.20 GPa | 899 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON Cycoloy_JK800 PC+ABS LNP* Stat-kon* Cycoloy_JK800 compound is an 8% carbon fiber reinforcedPC+ABS, electrostatic dissipative ECO conforming FR. Good hydrolytic stability. |
|||
Flexural Modulus | 6.20 GPa | 899 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® 4022 PBT (Europe-Africa-Middle East) VALOX 4022 is a 20% high strength glass fibre reinforced PBT injection moulding resin, with improved mechanical properties. Applications : Spotlights, appliance housings and handles. |
|||
Flexural Modulus | 6.20 GPa | 899 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP GF004 PSU LNP* Thermocomp* GF004 is a compound based on Polysulfone resin containing 20% Glass Fiber. |
|||
Flexural Modulus | 6.20 GPa | 899 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp HX05073 PA 11 LNP THERMOCOMP* HX05073 is a compound based on Nylon 11 resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 6.20 GPa | 899 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp KF003 Acetal Copoly (Asia Pacific) LNP* Thermocomp* KF003 is a compound based on Acetal Copolymer resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 6.20 GPa | 899 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP MF006A PP (Europe-Africa-Middle East) LNP* THERMOCOMP* MF006A is a compound based on Polypropylene resin containing Glass Fiber. |
|||
Flexural Modulus | 6.20 GPa | 899 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP MF006S PP LNP* THERMOCOMP* MF006S is a compound based on Polypropylene resin containing 30% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Flexural Modulus | 6.20 GPa | 899 ksi | ISO 178 |
Solvay TECHNYL® A 216 V33 PA66, 33% glass fiber, Conditioned Description: TECHNYL® A 216 V33 is a polyamide 66, reinforced with 33% of glass fiber, for injection molding. This product is available in natural color.Benefits: The product offers an excellent .. |
|||
Flexural Modulus | 6.20 GPa | 899 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp MF006S PP (Asia Pacific) LNP* Thermocomp* MF006S is a compound based on Polypropylene resin containing Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Asia P.. |
|||
Flexural Modulus | 6.20 GPa | 899 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP NF004 PC+ABS LNP* THERMOCOMP* NF004 is a compound based on PC+ABS resin containing 20% Glass Fiber. |
|||
Flexural Modulus | 6.20 GPa | 899 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP NF004 PC+ABS (Asia Pacific) LNP* Thermocomp* NF004 is a compound based on PC+ABS Blend resin containing Glass Fiber. |
|||
Flexural Modulus | 6.20 GPa @Thickness 4.00 mm |
899 ksi @Thickness 0.157 in |
2mm/min, injection molded, unannealed; ISO 178 |
Styron EMERGEâ„¢ 5302 Acrylonitrile Butadiene Styrene (ABS) EMERGEâ„¢ ABS 5302 is a black, 20% glass-filled ABS which is suitable for use in a wide variety of internal structural component applications in the information technology market. Applications: .. |
|||
Flexural Modulus | 6.20 GPa | 899 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp OF002A PPS LNP* Thermocomp* OF002A is a compound based on Polyphenylene Sulfide resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 6.20 GPa | 899 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP WF0049XP PBT (Europe-Africa-Middle East) LNP* Thermocomp* WF0049XP is a compound based on Polybutylene Terephalate resin containing Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant. |
|||
Flexural Modulus | 6.20 GPa @Temperature -40.0 °C |
899 ksi @Temperature -40.0 °F |
ASTM D790 |
Toyobo NB-5620S Nylon/Olefin Alloy, 15% Mineral Reinforced (DAM) Features: 15% Mineral Reinforced, Light WeightInformation provided by Toyobo. |
|||
Flexural Modulus | 6.20 GPa | 899 ksi | ASTM D790 |
Adell BR-14 Nylon 6, 20% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Flexural Modulus | 6.20 GPa | 899 ksi | ASTM D790 |
Chem Polymer Chemlon 125 G Nylon 66, 25% Glass Sphere Reinforced A 25% glass sphere reinforced nylon 66 offering a balance of rigidity, dimensional stability and surface appearance.Data provided by the manufacturer, Chem Polymer. |
|||
Flexural Modulus | 6.20 GPa | 899 ksi | ASTM D790 |
A. Schulman ComAlloy Aqualoy® 135 Polypropylene, Glass Reinforced, Chemically Coupled NSF, UL Data provided by the manufacturer, ComAlloy International Company.35% Glass Reinforced. In Aqualoy® materials, carefully selected base resins and proprietary additives meld hydrolytic stability an.. |
|||
Flexural Modulus | 6.20 GPa | 899 ksi | ASTM D790 |
A. Schulman ComAlloy Comtuf® 105 Polypropylene, Glass Reinforced, Chemically Coupled, Impact Modified Data provided by the manufacturer, ComAlloy International Company.40% Glass Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been int.. |
|||
Flexural Modulus | 6.20 GPa | 899 ksi | ASTM D790 |
A. Schulman ComAlloy Voloy® 681 Nylon 6/6, Glass Fiber/Bead Reinforced, Nylon 6/6 Alloy, Flame Retardant, UL Data provided by the manufacturer, ComAlloy International Company.45% Glass Fiber/Bead Reinforced. Halogen- and phosphorous-freeThe ComAlloy product line has been integrated into the A Schulman prod.. |
|||
Flexural Modulus | 6.20 GPa | 899 ksi | ASTM Data |
BASF Capron® 8334G Impact Modified, 40% Glass-Filled Nylon 6 (Conditioned)
(discontinued **) Capron 8334G is a heat stabilized, 40% glass fiber reinforced polyamide 6 molding compound developed for applications requiring a high level of stiffness combined with excellent impact performance. .. |
|||
Flexural Modulus | 6.20 GPa | 899 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP DFP34 PC (Asia Pacific) LNP* Lubricomp* DFP34 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE, Silicone. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 6.20 GPa | 899 ksi | ASTM D790 |
Plenco 7321 Phenolic, Nodular, Injection Molded PLENCO 07321 is an organic fiber reinforced phenolic molding compound, offering improved mechanical strength and excellent dimensional stability. Type ASTM 5948 CFI-5, and UL recognized under compon.. |
|||
Flexural Modulus | 6.20 GPa | 899 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP DFP34 PC LNP* Lubricomp* DFP34 is a compound based on Polycarbonate resin containing 20% Glass Fiber, 15% PTFE/Silicone. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 6.20 GPa | 899 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP DX06410 PC LNP* THERMOCOMP* DX06410 is a compound based on Polycarbonate resin containing 20% Glass Fiber. Added features of this material include: Easy Molding, Mold Release. |
|||
Flexural Modulus | 6.20 GPa | 899 ksi | ASTM-D790 |
Polyram RamOfin PPH308G8 Polypropylene, 40% Glass Fiber 40% glass fiber reinforced, heat stabilized, impact modified polypropylene for injection molding applicationsInformation provided by Polyram Ram On Ind. |