Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 5.20 GPa | 754 ksi | ASTM D790 |
Nylene® PA6 Glass Filled 5213 HS Nylon 6 13% Glass Filled; Property data for dry as molded samples.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation. |
|||
Flexural Modulus | 5.20 GPa @Temperature 23.0 °C |
754 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYabs T00 GF20 ABS, Glass Fibre-Reinforced Information provided by Polykemi AB |
|||
Flexural Modulus | 5.20 GPa @Temperature -40.0 °C |
754 ksi @Temperature -40.0 °F |
ASTM D790 |
Penn Fibre Pennite® 4512 Nylon 6, 12% Glass Fiber Reinforced (PA6) PENNITE® 4512 is a 12% glass fiber reinforced, black pigmented, thermally modified, type 6 nylon, available in sheets and rolls for high performance thermoforming and fabrication applications. PENN.. |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP DFP36 PC (Europe-Africa-Middle East) LNP* Lubricomp* DFP36 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE, Silicone. |
|||
Flexural Modulus | 5.20 GPa @Temperature 23.0 °C |
754 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYshine PBT D211 GF10 PBT, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP DX00714H PC LNP LUBRICOMP* DX00714H is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Wear Resistant, Healthcare. |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | ISO 178 |
Solvay TECHNYL® A 21T2 V25 PA66, 25% glass fiber, Conditioned Description: Flame retardant polyamide 66, reinforced with 25% of glass fiber, heat stabilized, for injection molding.Available in: Asia Pacific, Europe, Latin America and North AmericaProduct Appl.. |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | ISO 178 |
Solvay TECHNYL® C 246 V 30 PA6, 30% glass fiber, Conditioned Description: Polyamide PA6, reinforced with 30 % of glass fiber, high impact strength, for injection molding.Available in: Asia Pacific and North AmericaProduct Applications: Having good mechanical .. |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® DR48 - CS1049 PBT (Europe-Africa-Middle East) VALOX DR48 is a 15 % glass reinforced, flame retardant injection moulding PBT resin. Applications: lamp sockets, connectors, switches, electrical housings and bases, bobbins, trimmers and electromot.. |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Thermocomp PK0049 PA 6 (Europe-Africa-Middle East) LNP* THERMOCOMP* PK0049 is a compound based on PA 6 resin containing Glass Bead, Flame Retardant. Added features include; Flame Retardant.This data was supplied by SABIC-IP for the Europe-Africa-Mid.. |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL GTX GTX820 PPE+PA (Europe-Africa-Middle East) NORYL GTX820 is a 20% glass reinforced grade with excellent chemical resistance in combination with high stiffness and heat resistance. |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP 2F005 ETFE LNP* Thermocomp* 2F005 is a fluoropolymer compound based on ETFE containing 25% Glass Fiber. |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | 2 mm/min; ISO 178 |
Sax Polymers SAXALEN PPH305G30 Polypropylene Homopolymer, 30% Glass Filled SAXALEN PPH305G30 is a 30% glass filled Polypropylene - Homopolymer injection molding grade with high stiffness, low creep under load and good flow properties.Information provided by SAX Polymers |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | ISO 178 |
Polyram RamLloy PN300G4 PPE/PS Alloy, 20% Glass Fiber PPE/PS alloy, 20% glass fiber reinforced for injection molding applications.Information provided by Polyram. |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | ISO 178 |
Polyram RamShine PW311G4 SAN, 20% Glass Fiber 20% Glass fiber reinforced SAN for injection molding applications.Information provided by Polyram. |
|||
Flexural Modulus | 5.20 GPa @Temperature 160 °C |
754 ksi @Temperature 320 °F |
ISO 178 |
DSM Stanyl® TE200F8 PA46-GF40 40% Glass Reinforced, Heat Stabilized, for E&E applications |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | DIN 52457 |
CP-Polymer-Technik Wellamid® 6000/52 GV 15 HWUVCP 15% Glass Fiber Nylon 6, Low Temperature Impact Modified, UV Stabilized, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | ISO 178 |
DuPont Performance Polymers Crastin® SK602 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) 15% Glass Reinforced Polybutylene Terephthalate Crastin SK602 NC010 is a 15% glass fiber reinforced lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont P.. |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | 2 mm/min; ISO 178 |
Eurostar Starflam PK0049 PA6, Mineral Fiber Filled, Flame Retardant, Injection Molded Starflam PK0049 is a Free Flame Retardant Mineral Filled Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | ISO 178 |
Ascend Performance Materials Vydyne® R513H Black Nylon 66, 13% Glass Reinforced, DAM Vydyne® R513H Black is general-purpose, 13% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is an injection-molding grade that is lubricated for machine feed, flow, and m.. |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | ASTM D790 |
Chem Polymer Chemlon 115 G Nylon 66, 15% Glass Fiber Reinforced A 15% glass fiber reinforced nylon 66 offering improved creep resistance, stiffness, tensile strength and dimensional stability over unmodified nylon 66 materials. This product offers slight improv.. |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | ASTM D790 |
A. Schulman ComAlloy Comtuf® 635 Nylon 6/6, Glass/Mineral Reinforced, Impact Modified, Flow Enhanced Data provided by the manufacturer, ComAlloy International Company.40% Glass/Mineral Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has .. |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | ASTM D790 |
A. Schulman ComAlloy Comtuf® 639 Nylon 6/6, Mineral Reinforced, Impact Modified, Flow Enhanced Data provided by the manufacturer, ComAlloy International Company.40% Mineral reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been i.. |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | ISO 178 |
BASF Ultramid® B35EG3 BK 00564 15% Glass Filled PA6 (Dry) Description: 15% glass-fiber reinforced injection-molding grade for gIT applications such as, for example, steering column switches, vehicle mirror housings and the wheels of mountain bikes.Informat.. |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 621 Nylon 6/6, Glass Reinforced Data provided by the manufacturer, ComAlloy International Company.15% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 5.20 - 10.7 GPa | 754 - 1550 ksi | Average value: 9.47 GPa Grade Count:7 |
Overview of materials for Polyethylene Terephthalate (PET), Recycled, Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Recycled, Glass Reinforced". Each property range of values reported is.. |
|||
Flexural Modulus | 5.20 GPa | 754 ksi | Tangent, 0.05 in/min; ASTM D790 |
LyondellBasell Hostacom™ PF062-3 Polypropylene Homopolymer Description: Hostacom™ PF062-3 high melt flow, 5,200 MPa flexural modulus, chemically coupled, 30% glass fiber-reinforced polypropylene homopolymer has good impact strength, high stiffness and very.. |