Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Overview of materials for Polyethylene Terephthalate (PET), Recycled, Glass Reinforced

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), Recycled, Glass Reinforced
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Polyethylene Terephthalate (PET), Recycled, Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Recycled, Glass Reinforced". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.43 - 1.80 g/cc
0.0517 - 0.0650 lb/in³
Average value: 1.71 g/cc Grade Count:7
Water Absorption 0.0200 - 0.100 %
0.0200 - 0.100 %
Average value: 0.0557 % Grade Count:7
Linear Mold Shrinkage 0.000600 - 0.00250 cm/cm
0.000600 - 0.00250 in/in
Average value: 0.00138 cm/cm Grade Count:5
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 106 - 133 MPa
15400 - 19300 psi
Average value: 116 MPa Grade Count:7
Elongation at Break 1.18 - 3.00 %
1.18 - 3.00 %
Average value: 1.68 % Grade Count:7
Modulus of Elasticity 9.29 - 13.2 GPa
1350 - 1910 ksi
Average value: 11.3 GPa Grade Count:6
Flexural Yield Strength 165 - 200 MPa
23900 - 29000 psi
Average value: 178 MPa Grade Count:7
Flexural Modulus 5.20 - 10.7 GPa
754 - 1550 ksi
Average value: 9.47 GPa Grade Count:7
Compressive Yield Strength 144 - 169 MPa
20800 - 24500 psi
Average value: 160 MPa Grade Count:6
Izod Impact, Notched 0.490 - 0.740 J/cm
0.918 - 1.39 ft-lb/in
Average value: 0.644 J/cm Grade Count:7
Thermal Properties Metric English Comments
CTE, linear 15.12 - 15.12 µm/m-°C

@Temperature 100 - 100 °C
8.400 - 8.400 µin/in-°F

@Temperature 212 - 212 °F
Average value: 15.1 µm/m-°C Grade Count:1
CTE, linear, Transverse to Flow 46.8 - 46.8 µm/m-°C

@Temperature 100 - 100 °C
26.0 - 26.0 µin/in-°F

@Temperature 212 - 212 °F
Average value: 46.8 µm/m-°C Grade Count:1
Deflection Temperature at 1.8 MPa (264 psi) 203 - 221 °C
397 - 430 °F
Average value: 216 °C Grade Count:7
Flammability, UL94 HB - V-0
HB - V-0
Grade Count:7
Electrical Properties Metric English Comments
Electrical Resistivity 7.95e+15 - 2.50e+16 ohm-cm
7.95e+15 - 2.50e+16 ohm-cm
Average value: 1.44e+16 ohm-cm Grade Count:6
Dielectric Constant 3.10 - 3.80
3.10 - 3.80
Average value: 3.53 Grade Count:7
Dielectric Strength 14.0 - 21.0 kV/mm
356 - 533 kV/in
Average value: 16.5 kV/mm Grade Count:7
Dissipation Factor 0.0100 - 0.0460
0.0100 - 0.0460
Average value: 0.0170 Grade Count:7
Arc Resistance 20.0 - 119 sec
20.0 - 119 sec
Average value: 48.4 sec Grade Count:7
Comparative Tracking Index 200 - 225 V
200 - 225 V
Average value: 217 V Grade Count:6