Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.45 GPa | 355 ksi | ASTM D790 |
SABIC Innovative Plastics Cycoloy® MC5400 PC+ABS (Asia Pacific) |
|||
Flexural Modulus | 2.45 GPa | 355 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® CFR7431 PC COPOLYMER (Asia Pacific) Lexan* CFR7431 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm an.. |
|||
Flexural Modulus | 2.45 GPa | 355 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® DMX1435 PC Copolymer Lexan* DMX1435 is a UV stabilized standard flow polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 2.45 GPa | 355 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® FXD911A PC (Europe-Africa-Middle East) Lexan FXD911A is a flame retardant, medium viscosity grade with release for the special effect appearance Diffusion in various colors. Color package may affect performance.This data was supplied by .. |
|||
Flexural Modulus | 2.45 GPa | 355 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® FXD9945A PC UV stabilzed Visualfx FR PC with non-brominated and non-chlorinated flame retardant systems. It is available Only in white diffused effect(WH8B111X) meeting UL-94 V0 at 2mm for thin wall application.. |
|||
Flexural Modulus | 2.45 GPa | 355 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® FXD9945A PC (Asia Pacific) UV stabilzed Visualfx FR PC with non-brominated and non-chlorinated flame retardant systems. It is available Only in white diffused effect(WH8B111X) meeting UL-94 V0 at 2mm for thin wall application.. |
|||
Flexural Modulus | 2.45 GPa | 355 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® LUX7432C PC COPOLYMER (Asia Pacific) Lexan* LUX7432C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a.. |
|||
Flexural Modulus | 2.45 GPa | 355 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® LUX7432C PC COPOLYMER (Europe-Africa-Middle East) Lexan* LUX7432C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a.. |
|||
Flexural Modulus | 2.45 GPa | 355 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® LUX7436C PC COPOLYMER Lexan* LUX7436C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a.. |
|||
Flexural Modulus | 2.45 GPa | 355 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® SLX2431T PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Europe-Afri.. |
|||
Flexural Modulus | 2.45 GPa | 355 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® SLX1231T PC Copolymer (Asia Pacific) Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colors |
|||
Flexural Modulus | 2.45 GPa @Thickness 3.20 mm |
356 ksi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical MP220 ABS, High Adhesion, Heat Resistance Feature: Injection Molding, High Adhesion, Metal PlatingApplication: Automobiles Radiator Grill, MoldingCAS No. 9003-56-9 and 9003-54-7Information provided by LG Chemical |
|||
Flexural Modulus | 2.45 GPa @Thickness 3.20 mm |
356 ksi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical RS656H ABS, Chemical Resistance to Cyclopentane Feature: Extrusion Molding, General Purpose, Chemical Resistance to CyclopentaneApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical |
|||
Flexural Modulus | 2.45 GPa | 355 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Noryl V0150BT PPE+HIPS Noryl* V0150BT is an unfilled, injection moldable modified polyphenylene ether resin.. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 1.5 mm .. |
|||
Flexural Modulus | 2.45 GPa | 356 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® NE-1030 PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.45 GPa | 356 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® BF-0677HF MABS, Unreinforced Scratch Resistant Scratch resistant material that is used in TV housing and the exterior material for cleaner and air purifierInformation provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.45 GPa | 356 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® ASF-9810F PBT/PET, Mineral Filled General Purpose Material for automobile lamp with high flowInformation provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.45 GPa | 356 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® HI-1001B PC/ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.45 GPa | 356 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® NH-1001T PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.45 GPa | 356 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® HG-0760LT ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.45 GPa | 356 ksi | |
Zylog Hipolyene® 5131 SX-5 Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Flexural Modulus | 2.45 GPa | 355 ksi | 2mm/min; ISO 178 |
Denka MALECCA K-100 ABS A heat-resistant ABS resin based on "DENKA IP" – a Styrene-N-Phenylmaleimide copolymer. It has been designed as an easy-to-use resin by improving conventional heat-resistant ABS resins which had de.. |
|||
Flexural Modulus | 2.45 GPa | 355 ksi | 2mm/min; ISO 178 |
Denka MALECCA K-300 ABS A heat-resistant ABS resin based on "DENKA IP" – a Styrene-N-Phenylmaleimide copolymer. It has been designed as an easy-to-use resin by improving conventional heat-resistant ABS resins which had de.. |
|||
Flexural Modulus | 2.45 GPa @Thickness 3.17 mm |
355 ksi @Thickness 0.125 in |
ASTM D790 |
Calsak CS-72L General Purpose ABS Resin Product Characteristics:High Impact, High GlossInjection molding grade |
|||
Flexural Modulus | 2.45 GPa @Thickness 6.40 mm |
356 ksi @Thickness 0.252 in |
5 mm/min; ASTM D790 |
Bhansali Engineering Abstron IPM3000 PMMA- ABS Alloy Super High Gloss, High scratch resistanceInformation provided by Bhansali |
|||
Flexural Modulus | 2.45 GPa @Thickness 6.40 mm |
356 ksi @Thickness 0.252 in |
5 mm/min; ASTM D790 |
Bhansali Engineering Abstron IM14GM ABS Injection Molding Grade High Rigidity, Medium Impact, Good paintabilityInformation provided by Bhansali |
|||
Flexural Modulus | 2.45 GPa | 355 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® ML6230 PC Copolymer Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colors.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 2.45 GPa | 355 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® ML6230 PC Copolymer (Asia Pacific) Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colors.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 2.45 GPa | 355 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® ML6240 PC Copolymer (Europe-Africa-Middle East) Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Europe-Africa-Middle Eas.. |
|||
Flexural Modulus | 2.45 GPa | 356 ksi | ASTM D790 |
Shinkong Synthetic Fibers Shinite® D201 PBT Information from Shinkong Synthetic Fibers Corp. |