SABIC Innovative Plastics Cycoloy® MC5400 PC+ABS (Asia Pacific)

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Cycoloy®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics Cycoloy® MC5400 PC+ABS (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.19 g/cc
1.19 g/cc
ASTM D792
Water Absorption 0.20 %

@Time 86400 sec
0.20 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cm

@Thickness 3.20 mm
0.0040 - 0.0060 in/in

@Thickness 0.126 in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 58.0 MPa
8410 psi
SABIC - Japan Method
Elongation at Break 150 %
150 %
SABIC - Japan Method
Flexural Strength 92.0 MPa
13300 psi
ASTM D790
Flexural Modulus 2.45 GPa
355 ksi
ASTM D790
Izod Impact, Notched 5.88 J/cm
11.0 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 60.0 - 80.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
33.3 - 44.4 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C

@Thickness 3.20 mm
194 °F

@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C

@Thickness 6.40 mm
194 °F

@Thickness 0.252 in
unannealed; ASTM D648
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
UL 94
5VB

@Thickness 2.30 mm
5VB

@Thickness 0.0906 in
UL 94