Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.20 GPa | 319 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycolac® MG47F ABS (Europe-Africa-Middle East) Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. FDA compliant. |
|||
Flexural Modulus | 2.20 GPa | 319 ksi | ISO 178 |
Premix Thermoplastics PREBOARD E1026 Standard Epoxy Circuit Boards PREBOARD is a thermoplastic based PCB laminate. Low dissipation factor leads to high gain in the antennas. As a non filled laminate PREBOARD is fully homogenous so that consistant properties are ac.. |
|||
Flexural Modulus | 2.20 - 3.20 GPa | 319 - 464 ksi | ASTM D790 |
Prodways PLASTCure Cast 200 3D Printing Polymer Good reactivity and low viscosity. Outstanding burnout properties with nearly zero ash content.Highly suitable for direct investment casting or dental applications.Information provided by Genistar. |
|||
Flexural Modulus | 2.20 - 3.20 GPa | 319 - 464 ksi | ASTM D790-04 |
Proto3000 Objet Digital Materials™ DM_8310 Rigid Opaque Prototyping Polymer Primary material: VeroWhitePlusSecondary material: VeroBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide.. |
|||
Flexural Modulus | 2.20 GPa | 319 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® CY200FC PC+ABS High flow PC+ABS material designed for local Pacific Automotive applications |
|||
Flexural Modulus | 2.20 GPa | 319 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® HPS7R PC (Europe-Africa-Middle East) Low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma sterilizable. .. |
|||
Flexural Modulus | 2.20 GPa | 319 ksi | 2mm/min; ASTM D790 |
Kingfa MAC-601 PC/ABS Alloy Features:Excellent balance propertiesHigh impact strengthGood electro-plating propertiesGood processing propertiesApplications:Injection moldingAutomobile instrument panelElectrical and electronic p.. |
|||
Flexural Modulus | 2.20 GPa | 319 ksi | 2 mm/min; ISO 178 |
LG Chemical NT-520 ABS, High Flow, Non Toxic Information Provided by LG Chem |
|||
Flexural Modulus | 2.20 - 2.40 GPa | 319 - 348 ksi | ASTM D790 |
Loxim 600 00HB Polycarbonate/Polybutylene Terephthalate Information provided by Loxim Industries |
|||
Flexural Modulus | 2.20 GPa | 319 ksi | 15 mm/min; ASTM D790 |
LG Chemical 501S-S HIPS Self lubricant, Balanced mechanical properties, Good surface appearance with high gloss, Conforming to FDA CFR 177.1640, Excellent processability, Applications include refrigerator food holders, par.. |
|||
Flexural Modulus | 2.20 GPa | 319 ksi | ISO 178 |
SABIC Innovative Plastics LNP LUBRILOY R2000A PA 66 LNP LUBRILOY* R2000A is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant. |
|||
Flexural Modulus | 2.20 GPa | 319 ksi | |
SPS Guang Zhou FILLMAâ„¢ 5002F30B Mineral Filled Polypropylene Characteristic: 30%wt of Sulfate Barium filled, high gloss, high heat resistanceApplications: Household appliance partsInformation Provided by SPS (Guang Zhou) Ltd. |
|||
Flexural Modulus | 2.20 GPa | 319 ksi | 2mm/min; ISO 178 |
Teijin Panlite® LN-1250G Flame Resistant, Translucent Polycarbonate Resin Flame retardant and mold release grade with normal fluidity, which is suitable for injection molding applications.Applications:Electric, electronic and business machine components that need flame re.. |
|||
Flexural Modulus | 2.20 GPa | 319 ksi | 1.3 mm/min; ASTM D790 |
A. Schulman POLYFORT™ FPP 1512E Talc Filled, High Impact Copolymer Polypropylene DescriptionPolyfort® FPP 1512E is a 10% talc-filled, high impact copolymer polypropylene. ApplicationPolyfort® FPP 1512E is suitable for extrusion or blow molding applications. Information provid.. |
|||
Flexural Modulus | 2.20 GPa | 319 ksi | ASTM D790 |
A. Schulman POLYFORT™ FXP 2779U UV Stabilized Copolymer Polypropylene DescriptionPolyfort® FXP 2779U is a 20% talc-filled, UV stabilized copolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 2.20 GPa | 319 ksi | 1.3 mm/min; ASTM D790 |
A. Schulman POLYFORT™ FPP 1512E Talc Filled, High Impact Copolymer Polypropylene DescriptionPolyfort® FPP 1512E is a 10% talc-filled, high impact copolymer polypropylene. ApplicationPolyfort® FPP 1512E is suitable for extrusion or blow molding applications. Information provid.. |
|||
Flexural Modulus | 2.20 GPa | 319 ksi | ASTM D790 |
A. Schulman POLYFORT™ FXP 2779U UV Stabilized Copolymer Polypropylene DescriptionPolyfort® FXP 2779U is a 20% talc-filled, UV stabilized copolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 2.20 GPa | 319 ksi | ISO 178 |
Polyram PlusTek PB841 Nylon 6 for Injection Molding, Impact Modified Impact modified Nylon 6 for injection molding applications.Information provided by Polyram. |
|||
Flexural Modulus | 2.20 GPa | 319 ksi | 2 mm/min; ISO 178 |
Chi Mei Polylac® PA-757 ABS High gloss, medium impact |
|||
Flexural Modulus | 2.20 GPa | 319 ksi | ASTM D790 |
Ashley Polymers Ashlene® 520BU Nylon 66 A general purpose Nylon 66 resin, black, utility grade.Data provided by the manufacturer |
|||
Flexural Modulus | 2.20 GPa | 319 ksi | ASTM D790 |
Beijing Chemical Industry KAIFA® GL3200 ABS Flame-Retardant Grade Good flammabilityInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Flexural Modulus | 2.20 GPa | 319 ksi | ASTM D790 |
Ashley Polymers Ashlene® C1176 Polycarbonate These are also available with UV, designated by -3. For release, add R. These are all flame retardant grades developed for various applications such as electrical, electronic, lighting, computer, .. |
|||
Flexural Modulus | 2.20 GPa | 319 ksi | 2 mm/min; ASTM D790 |
Solvay Specialty Polymers Solef® 1008 PVDF Homopolymer
(discontinued **) Key features of this grade: Low Viscosity, All Purpose, Injection, Virgin. Recommended processing is injection. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF .. |
|||
Flexural Modulus | 2.20 GPa @Temperature 23.0 °C |
319 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYfill PP 150ENH Polypropylene, Flame Retardant, Halogen Free Information provided by Polykemi AB |
|||
Flexural Modulus | 2.20 GPa | 319 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Noryl FXN119LG PPE+HIPS (Asia Pacific) Noryl FXN119LG is a low gloss PPE/HIPS grade. It provides a balance of mechanical properties and heat performance with intrinsic low gloss appreance. FXN119LG is available in mutliple colors.This da.. |
|||
Flexural Modulus | 2.20 GPa | 319 ksi | 2 mm/min; ISO 178-A |
Lanxess Pocan® C 1206 000000 PET + PC PET + PC, non-reinforced, injection molding, improved impact strengthInformation provided by LANXESS. |
|||
Flexural Modulus | 2.20 GPa | 319 ksi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP DL002ER PC (Asia Pacific) LNP* Lubricomp* DL002ER is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Internally Lubricated, Easy Molding, Mold Release. |