Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.06 GPa | 299 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycoloy® MC1300 PC+ABS Cycoloy MC1300 resin is an injection moldable PC/ABS blend with excellent flow and impact performance. It is designed for plating applications mostly used in the automotive industry. |
|||
Flexural Modulus | 2.06 GPa | 299 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics GELOY CR8510 ASA (Asia Pacific) ASA with outstanding UV exposure performance for both exterior and interior applications. F1 Rated. |
|||
Flexural Modulus | 2.06 GPa | 299 ksi | DIN 53452; ASTM D790 |
Kolon SPESIN® KP210 General Purpose PBT Resin
(discontinued **) SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High hea.. |
|||
Flexural Modulus | 2.06 GPa | 299 ksi | DIN 53452; ASTM D790 |
Kolon KOPA® KN173HI2 High Impact Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Flexural Modulus | 2.06 GPa @Thickness 6.40 mm |
299 ksi @Thickness 0.252 in |
5mm/min; ASTM D790 |
LG Chemical Lupox® TE5000SP PBT+PC Description: Injection Molding, PBT+PC, Low Gloss, Good WeatherabilityApplication: Automotive (Roof Rack)CAS No. 137050-02-03, 24968-12-5 and 103598-77-2Information provided by LG Chemical |
|||
Flexural Modulus | 2.06 GPa | 299 ksi | ASTM D790 |
GRECO ISOPAK 625 Polycarbonate/ABS Alloy General purpose polycarbonate/ABS alloy; good impact and dimensional stabilityInformation provided by Greater Eastern Resins Industrial Co., Ltd. |
|||
Flexural Modulus | 2.06 GPa @Temperature 23.0 °C |
299 ksi @Temperature 73.4 °F |
ASTM D790 |
IRPC Polimaxx Porene KU650 Acrylonitrile Butadiene Styrene Applications:injection moldingautomotive parts such as instrument panels, console boxes, switches, automotive louvers, ectelectrical appliances |
|||
Flexural Modulus | 2.06 GPa | 299 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP GL003 PSU LNP* Lubricomp* GL003 is a compound based on Polysulfone resin containing 15% PTFE. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 2.06 GPa | 299 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Lubricomp GL004 PSU (Asia Pacific) LNP* Lubricomp* GL004 is a compound based on Polysulfone resin containing PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Asia Pacifi.. |
|||
Flexural Modulus | 2.06 GPa | 299 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP IL004 PA 6/12 (Asia Pacific) LNP* Lubricomp* IL004 is a compound based on Nylon 6/12 resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 2.06 GPa | 299 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP Noryl_NWR5810 PPE+HIPS (Europe-Africa-Middle East) LNP* Lubricomp* Noryl_NWR5810 compound is a 10% PTFE filled PPE+PS. High flow and good impact. Applications requiring wear resistance/lubricity. Electronics. |
|||
Flexural Modulus | 2.06 GPa | 299 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP RP003 PA 66 (Asia Pacific) LNP* Lubricomp* RP003 is a compound based on Nylon 66 resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 2.06 GPa | 299 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRILOY D20009P PC (Asia Pacific) LNP* Lubriloy* D20009P is a compound based on Polycarbonate resin containing Flame Retardant, Proprietary Lubricant. Added features of this material include: Internally Lubricated, Flame Retardant,.. |
|||
Flexural Modulus | 2.06 GPa | 299 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® V2105U PBT Unreinforced, Wear resistant, UV Stabilized PBT designed for outdoor, agricultural, industrial and automotive applications. This grade has very high impact strength to stiffness ratio. |
|||
Flexural Modulus | 2.06 GPa | 299 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP KZ001L Acetal Copoly LNP* THERMOCOMP* KZ001L is a compound based on Acetal Copolymer resin containing 5% Milled Glass. Added features of this material include: Low Extractible. |
|||
Flexural Modulus | 2.06 GPa | 299 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® HI-1001BP PC/ABS, Metal Plating Grade PC/ABS material for platingInformation provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.06 GPa | 299 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® TX-0510 TRABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.06 GPa | 299 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® HP-1000H PC/ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.06 GPa | 299 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® SD-0150U ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.06 GPa | 299 ksi | ASTM D790 |
Samyang Trirex® 3022L1 Polycarbonate, Lens Grade TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec.. |
|||
Flexural Modulus | 2.06 GPa | 299 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Thermotuf U1000AIS PPA (Asia Pacific) LNP* Thermotuf* U1000AIS is a compound based on Polyphthalamide resin. Added features of this material include: High Impact, Heat Stabilized.This data was supplied by SABIC-IP for the Asia Pacific .. |
|||
Flexural Modulus | 2.06 GPa | 299 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP MB008S PP LNP* THERMOCOMP* MB008S is a compound based on Polypropylene resin containing 40% Glass Bead. Added features of this material include: Heat Stabilized. |
|||
Flexural Modulus | 2.06 GPa | 299 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp MB008S PP (Asia Pacific) LNP* Thermocomp* MB008S is a compound based on Polypropylene resin containing Glass Bead. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Asia Pa.. |
|||
Flexural Modulus | 2.06 GPa | 299 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® HG-0760 ABS, Unreinforced Used in telephones, vacuum cleaners and electric fan standsInformation provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.06 GPa | 299 ksi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® VE-0860EX ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.06 GPa | 299 ksi | ASTM D790 |
PlastxWorld CEVIAN® S3100 PC/ABS alloy Flame retarded PC/ABS Alloy.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Flexural Modulus | 2.06 GPa | 299 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Thermotuf V1000SU PA LNP* Thermotuf* V1000SU is a compound based on Nylon resin. Added features of this material include: Heat Stabilized, UV Stabilized.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 2.06 GPa | 299 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOTUF V1000SU PA (Asia Pacific) LNP* Thermotuf* V1000SU is a compound based on Nylon resin. Added features of this material include: Heat Stabilized, UV Stabilized. |
|||
Flexural Modulus | 2.06 GPa | 299 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP DL004XXC PC LNP* LUBRICOMP* DL004XXC is a compound based on Polycarbonate containing 20% PTFE. Characteristics of this grade are: Interrnally Lubricated. |
|||
Flexural Modulus | 2.06 GPa | 299 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON MFD02 PP (Asia Pacific) LNP* Stat-kon* MFD02 is a compound based on Polypropylene resin containing Glass Fiber, Carbon Powder. Added features of this material include: Electrically Conductive. |