Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics Cycoloy® MC1300 PC+ABS

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Cycoloy®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics Cycoloy® MC1300 PC+ABS.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Cycoloy MC1300 resin is an injection moldable PC/ABS blend with excellent flow and impact performance. It is designed for plating applications mostly used in the automotive industry.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
ASTM D792
Water Absorption 0.10 %

@Time 86400 sec
0.10 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0050 - 0.0080 cm/cm

@Thickness 3.20 mm
0.0050 - 0.0080 in/in

@Thickness 0.126 in
SABIC Method
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm

@Thickness 3.20 mm
0.0050 - 0.0070 in/in

@Thickness 0.126 in
SABIC Method
Melt Flow 14 g/10 min

@Load 5.00 kg,
Temperature 260 °C
14 g/10 min

@Load 11.0 lb,
Temperature 500 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 44.0 MPa
6380 psi
Type I, 50 mm/min; ASTM D638
Tensile Strength, Yield 50.0 MPa
7250 psi
Type I, 50 mm/min; ASTM D638
Elongation at Break 150 %
150 %
Type I, 50 mm/min; ASTM D638
Elongation at Yield 8.6 %
8.6 %
Type I, 50 mm/min; ASTM D638
Tensile Modulus 2.13 GPa
309 ksi
50 mm/min; ASTM D638
Flexural Yield Strength 72.0 MPa
10400 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.06 GPa
299 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 5.34 J/cm
10.0 ft-lb/in
ASTM D256
4.27 J/cm

@Temperature -30.0 °C
8.00 ft-lb/in

@Temperature -22.0 °F
ASTM D256
Dart Drop, Total Energy 33.0 J

@Temperature -30.0 °C
24.3 ft-lb

@Temperature -22.0 °F
ASTM D3763
40.0 J

@Temperature 23.0 °C
29.5 ft-lb

@Temperature 73.4 °F
ASTM D3763
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 72.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
40.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
CTE, linear, Transverse to Flow 90.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
50.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
Thermal Conductivity 0.200 W/m-K
1.39 BTU-in/hr-ft²-°F
ASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 115 °C

@Thickness 3.20 mm
239 °F

@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 98.0 °C

@Thickness 3.20 mm
208 °F

@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 111 °C
232 °F
Rate B/50; ASTM D1525