Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 16.0 GPa | 2320 ksi | ISO 178 |
PolyOne OnForce™ LFT NN-60LGF/000 HS UV Black Polyamide 66 (Nylon 66) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Flexural Modulus | 16.0 - 18.0 GPa | 2320 - 2610 ksi | Injection; ISO 178 |
Raschig Group 2568 AMC Glass fiber-reinforced polyester molding compound. Very good mechanical strength, very good electrical properties and dimensional stability, heat resistant up to 500°C for short time - usable for s.. |
|||
Flexural Modulus | 16.0 - 20.0 GPa | 2320 - 2900 ksi | Compression; ISO 178 |
Raschig Group RALUPOL® 4566 UP Polyester Glass-fiber reinforced polyester molding compound. Low mold shrinkage and post-shrinkage, good electrical values, excellent heat resistance, outstanding pourability. This product meets the allowed u.. |
|||
Flexural Modulus | 16.0 GPa | 2320 ksi | |
Cookson Group Plaskon® 3300SH Mineral Filled Epoxy Molding Compound
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.Exhibits exceptional reliability, excellent moldability, good release characteristics and low flash. This compound is especially.. |
|||
Flexural Modulus | 16.0 GPa | 2320 ksi | |
Lehmann & Voss LUVOCOM® 1301/CF/20 PPS, linear, with carbon fiber Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w.. |
|||
Flexural Modulus | 16.0 GPa | 2320 ksi | |
Lehmann & Voss LUVOCOM® 19-8373 Polyamide 46, with carbon fiber, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Antistatic.Improved fri.. |
|||
Flexural Modulus | 16.0 GPa | 2320 ksi | |
Lehmann & Voss LUVOCOM® 1100-8134 Polyether sulfone, with carbon fiber Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta.. |
|||
Flexural Modulus | 16.0 GPa | 2320 ksi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP ECL36 PEI LNP* Lubricomp* ECL36 is a compound based on Polyetherimide resin containing 30% Carbon Fiber, 15% PTFE. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 16.0 GPa | 2320 ksi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP ECL36 PEI (Europe-Africa-Middle East) LNP* Lubricomp* ECL36 is a compound based on Polyetherimide resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 16.0 GPa | 2320 ksi | ASTM D790 |
Solvay TECHNYLSTARâ„¢ AFX 218S V50 PA6, 50% glass filled, DRY Description: High stiffness materials TECHNYLSTAR Polyamide 66, reinforced with 50% of glass fiber, heat stabilized for injection molding. Characterized by a high fluidity of the melt. Available in:.. |
|||
Flexural Modulus | 16.0 GPa | 2320 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics LNP Stat-kon EX08308C PEI (Asia Pacific) Stat-Kon* EX08308C is a high cleanliness Polyetherimide Compound reinforced with Carbon Fiber for use in applications requiring the highest level of cleanliness. This compound is compounded using LN.. |
|||
Flexural Modulus | 16.0 GPa | 2320 ksi | ISO 178 |
Sumitomo Bakelite North America RX® 611 Fiberglass Reinforced Phenolic RX 611 is a fiberglass reinforced phenolic molding compound, with good dimensional stability and good strength at elevated temperatures. Meets ASTM D-5948 Type MFH.Information supplied by Sumitomo.. |
|||
Flexural Modulus | 16.0 GPa | 2320 ksi | ISO 178 |
Vyncolit TX10916/15 Graphite Filled Novolac Phenolic Novolac resin based, graphite filled compound used for low friction applications where dimensional stability is requiredInformation provided by Sumitomo Bak North America, Inc. |
|||
Flexural Modulus | 16.0 GPa | 2320 ksi | ASTM D790 |
Toyobo Vylopet® EMC145 Glass Reinforced Polyester, Standard Grade Key Feature: Flame retardant V-0 UL-94 classApplications: Ultra-precise componentsGeneral features of Vylopet® include heat resistance, good mechanical properties, high dielectric strength and trac.. |
|||
Flexural Modulus | 16.0 GPa | 2320 ksi | ISO 178 |
Vyncolit G865 Novolac Phenolic Glass fiber filled phenolic molding compound with high mechanical, good thermal and electrical properties. USES: Asbestos-free replacement for die-cast automotive metal parts, e.g. reactors for aut.. |
|||
Flexural Modulus | 16.0 GPa | 2320 ksi | tangent; chs 0.05 in/min; ASTM D790 |
Diamond Polymers Centrex® 833 Sheet Extrusion Grade Centrex 833 resin is a high-gloss, high-impact grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. It has good melt strength for extrusion and thermoforming, and it .. |
|||
Flexural Modulus | 16.0 GPa | 2320 ksi | ISO 178 |
Eurostar Star L PA66 30Y D51 PA66, Carbon Fiber Filled, Injection Molded Star L PA66 30Y D51 is a PTFE Lubricated, Carbon Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Modulus | 16.0 GPa | 2320 ksi | ISO 178 |
Ascend Performance Materials Vydyne® R550H Nylon 66, 50% Glass Reinforced, DAM Vydyne® R550H is general-purpose, heat-stabilized, hydrolysis-resistant, 50% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physic.. |
|||
Flexural Modulus | 16.0 GPa | 2320 ksi | ASTM D790 |
A. Schulman ComAlloy E-16674B PPS, Electrically Conductive - Carbon Fiber Filled Data provided by the manufacturer, ComAlloy International Company.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 16.0 GPa | 2320 ksi | ASTM D790 |
LATI LARPEEK 50 G/50 50% Glass Reinforced Polyetheretherketone (PEEK)
(discontinued **) Larpeek polyetheretherketone (PEEK) is a high performance thermoplastic offering cost effective performance in difficult environments across all industries. PEEK is temperature resistant (up to 250°.. |
|||
Flexural Modulus | 16.0 GPa | 2320 ksi | ASTM D790 |
Resinoid 1329 Phenolic Molding, Glass Reinforced Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance |
|||
Flexural Modulus | 16.0 GPa | 2320 ksi | ASTM D790 |
Sumitomo Bakelite North America Epiall® 1961B-1 Mineral and Glass Filled Electrical Encapsulation Grade Epoxy Epiall 1961B-1 is a short glass fiber and mineral filled epoxy molding compound with excellent dimensional stability, good strength properties, and good electrical insulation properties.Information .. |
|||
Flexural Modulus | 16.0 GPa | 2320 ksi | ISO 178 |
Sumitomo Bakelite North America RX® 790 Fiberglass Reinforced Phenolic Novolac RX 790 is a fiberglass reinforced phenolic novolac compound, featuring a good balance of strength and toughness. Information supplied by Sumitomo Bak North America. |