Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 11.9 GPa | 1730 ksi | X, Y direction; Condition A; ASTM D790 |
Rogers Corporation TMM® TMM3 Ceramic Thermoset Polymer Composite TMM® Thermoset microwave materials are ceramic thermoset polymer composites designed for high plate-thru-hole reliability stripline and microstrip applications. The electrical and mechanical prope.. |
|||
Flexural Modulus | 11.9 GPa | 1730 ksi | ISO 178 |
Nilit FRIANYL A63 GV40 Nylon 6.6 for injection molding, 40% glass fiber reinforced Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Modulus | 11.9 GPa | 1730 ksi | ASTM D790 |
Parker Chomerics PREMIER™ A240-ST EMI Shielding Plastic Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer .. |
|||
Flexural Modulus | 11.9 GPa | 1730 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP DCL33E PC (Europe-Africa-Middle East) LNP* LUBRICOMP* DCL33E is a compound based on Polycarbonate resin containing Carbon Fiber, PTFE. Added features include; Internally Lubricated, Electrically Conductive, Easy Molding. |
|||
Flexural Modulus | 11.9 GPa | 1730 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Lubricomp DEL34 PC (Europe-Africa-Middle East) LNP* Lubricomp* DEL34 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP f.. |
|||
Flexural Modulus | 11.9 GPa | 1730 ksi | 13 mm/min; ASTM D790 |
PolyOne Nymax™ NM 6600-44GF0001 White Polyamide 66 (Nylon 66) The Nymax® GMF 1200 Series of compounds are based upon nylon 6/6 resins and select combinations of glass fiber and mineral reinforcements offering a unique balance of physical property and part per.. |
|||
Flexural Modulus | 11.9 GPa | 1730 ksi | ASTM D790 |
PolyOne Stat-Tech™ NN-20CF/000 Black HS Polyamide 66 (Nylon 66) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Flexural Modulus | 11.9 GPa | 1730 ksi | ASTM D790 |
PolyOne Stat-Tech™ NN-20CF/000 Black Polyamide 66 (Nylon 66) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Flexural Modulus | 11.9 GPa @Temperature 23.0 °C |
1730 ksi @Temperature 73.4 °F |
ISO 178 |
Solvay Specialty Polymers Amodel® AE-8133 Polyphthalamide (PPA)
(discontinued **) Amodel AE-8133 is a 33% glass reinforced polyphthalamide (PPA) designed to work in the modern automotive electrical environment. This grade features a high heat deflection temperature, high flexural.. |
|||
Flexural Modulus | 11.9 GPa | 1730 ksi | ASTM D790 |
Techmer ES Electrablend® ABS CF20 BK 20% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 20% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 11.9 GPa | 1730 ksi | ASTM D790 |
Solvay Specialty Polymers Amodel® A-1133 L WH 015 Polyphthalamide (PPA), 33% Glass Fiber Formerly referred to as Amodel® PXM-13015. Amodel® A-1133 L resin is a 33% glass reinforced polyphthalamide (PPA) which is distinguished by its high-reflectivity white color. This grade featu.. |
|||
Flexural Modulus | 11.9 GPa | 1730 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP DC004E PC (Europe-Africa-Middle East) LNP* Thermocomp* DC004E is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Easy Molding. |
|||
Flexural Modulus | 11.9 GPa | 1730 ksi | GB/T 9341-2008 |
Sichuan Deyang Haton® hGR30 Polyphenylene Sulfide, Glass Fiber Reinforced Injection moldingInformation provided by Sichuan Deyang Chemical Co., LTD |
|||
Flexural Modulus | 11.9 GPa | 1730 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP DX10313 PC (Asia Pacific) DX10313 is high modulus polycarbonate, 50% glass filled, with balanced flow and impact strength |
|||
Flexural Modulus | 11.9 GPa | 1730 ksi | ISO 178 |
SABIC Innovative Plastics LNP Thermocomp JF008 PES LNP* Thermocomp* JF008 is a compound based on Polyethersulfone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 11.9 GPa | 1730 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp OX92080 PPS - LINEAR LNP* Thermocomp* OX92080 is a compound based on Linear PPS containing Proprietary Fillers.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 11.9 GPa | 1730 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-KON OE003A PPS - BRANCHED (Europe-Africa-Middle East) LNP* STATKON* OE003A is a compound based on PPS ( branched ) resin containing Carbon Fiber. Added features include: Electrically Conductive. |
|||
Flexural Modulus | 11.9 GPa | 1730 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP VERTON RX00327 PA 66 LNP* VERTON* RX00327 is a compound based on Nylon 66 resin containing proprietary fillers. Added feature of this material is: Structural. |
|||
Flexural Modulus | 11.9 GPa | 1720 ksi | ASTM D790 |
Techmer ES HiFill® SPS GF40 BK 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightFeatures: SyndiotacticAppearance: BlackInformation provided by TP Composites, Inc. |