Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Techmer ES HiFill® SPS GF40 BK 40% Glass Filled

Category Polymer , Thermoplastic , Polystyrene (PS) , Syndiotactic Polystyrene (SPS) , Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber
Manufacturer Techmer ES
Trade Name HiFill®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES HiFill® SPS GF40 BK 40% Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightFeatures: SyndiotacticAppearance: BlackInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.36 g/cc
0.0491 lb/in³
ASTM D792
Water Absorption 0.0090 %

@Time 86400 sec
0.0090 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0030 cm/cm

@Thickness 3.17 mm
0.0030 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
ASTM D785
Tensile Strength, Yield 121 MPa
17500 psi
ASTM D638
Elongation at Break 1.1 %
1.1 %
ASTM D638
Flexural Yield Strength 224 MPa
32500 psi
ASTM D790
Flexural Modulus 11.9 GPa
1720 ksi
ASTM D790
Izod Impact, Notched 1.12 J/cm

@Thickness 3.17 mm
2.10 ft-lb/in

@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched 13.3 J/cm

@Thickness 3.17 mm
25.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 16.2 µm/m-°C
9.00 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 243 °C
470 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 263 °C
505 °F
Unannealed; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
ASTM D257
Dielectric Strength 23.6 kV/mm
600 kV/in
Method A (Short-Time); ASTM D149
Users viewing this material also viewed the following: