Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.900 - 1.30 GPa | 131 - 189 ksi | |
Reliance Industries Polypropylene Random Copolymer Typical properties of Reliance - Repol Polypropylene gradesInformation provided by Reliance Industries |
|||
Flexural Modulus | 0.900 GPa | 131 ksi | 3 pt. secant. ASTM D790 |
Chevron Phillips HiD® 9326 HDPE Natural Pipe Resin
(discontinued **) Resin Type: Linear Copolymer; PE3408 Pipe Resin; ASTM D 3350 Classification: 335440A; ASTM D 4976 Classification: PE 235, A 56606Applications:Base Resin for use in Oil Patch and Industrial Pipe Appl.. |
|||
Flexural Modulus | 0.900 GPa | 131 ksi | 3 pt. secant. ASTM D790 |
Chevron Phillips HiD® 9502/HiD® 9503 with Antistat HDPE Blow Molding Resin
(discontinued **) Resin Type: Linear Copolymer; Blow Molding ResinCharacteristics: Medium Molecular Weight Distribution, Wide Range of Processing Conditions, Excellent ESCR, High Melt Strength, Good Impact Resistance.. |
|||
Flexural Modulus | 0.900 GPa | 131 ksi | 3 pt. secant. ASTM D790 |
Chevron Phillips HiD® 9646T HDPE High Molecular Weight Sheeting Resin
(discontinued **) Resin Type: Linear Copolymer; ASTM D 4976 Classification: PE 235, A 56606Applications:Sheeting, Thermoforming, Profile ExtrusionData provided by Chevron Chemical. |
|||
Flexural Modulus | 0.900 GPa | 131 ksi | 1% Secant; ASTM D 790 |
Chevron Phillips HiD® 9502H - 9503H High Performance Series HDPE Blow Molding Resin
(discontinued **) Resin Type: linear copolymerCharacteristics: outstanding ESCR, excellent impact resistance, medium molecular weight distribution, wide range of processing conditions, high melt strength, good pariso.. |
|||
Flexural Modulus | >= 0.900 GPa | >= 131 ksi | ASTM D790 |
Forever Plast Namtene® 1002 Recycled Pipe Grade HDPE Namtene® 1002 is used for pipes. It features a lower polypropylene content than standard Namtene®. |
|||
Flexural Modulus | 0.900 GPa | 131 ksi | ISO 178 |
Iran Petrochemical (PCC) EP2C 37 F Polypropylene EP2S 37 F offers good process ability, excellent clarity and gloss and exhibits very good heat weld ability.Applications: packaging of stationery, packaging of food stuffs, lamination.Information pr.. |
|||
Flexural Modulus | 0.900 GPa | 131 ksi | ASTM D790 |
Kaneka PHBH Semi-Rigid Bio-based Polymer A copolymer produced of 3-hydroxybutyrate and 3-hydroxyhexanoate produced by fermentation of plant oils. It has excellent biodegradability (under anaerobic, aerobic, aquatic, and compost conditions.. |
|||
Flexural Modulus | 0.900 GPa | 131 ksi | DIN 53457 |
Schwartz Technical Plastics LAMIGAMID® 710 High Density Polyethylene Application: chain-guides, cutting plates, linersInformation provided by Schwartz Technical Plastics GmbH |
|||
Flexural Modulus | 0.900 GPa | 131 ksi | ISO Data |
Styrolution Styrolux 3G55 SBC Styrolux 3G55 is a thermoplastic styrene-butadiene block copolymer which is suitable for film and sheet extrusion, and thermoforming. It offers and outstanding combination of crystal clarity and ex.. |
|||
Flexural Modulus | 0.900 GPa | 131 ksi | ASTM D790 |
SCG Chemicals EL-Leneâ„¢ H1000PYL High Density Polyethylene Pipe Resin Key Characteristics: Good processing, high thermal stability, good resistance to weatheringRecommended Applications: Stripe lines for PE100 pipe, non pressure pipesCertification: Certified by LNE.. |
|||
Flexural Modulus | 0.900 GPa | 131 ksi | 50% humidity; ISO 178 |
Borealis Bormed™ RE806CF Polypropylene Random Copolymer Bormed™ RE806CF is a random copolymer. The material is specially formulated for medical applications. Applications: Bormed™ RE806CF is recommended for medical packaging. Bormed™ RE806CF contai.. |
|||
Flexural Modulus | 0.900 GPa | 131 ksi | 2mm/min; ISO 178 |
Borealis EE002AE Polypropylene Elastomer Modified EE002AE is a reactor elastomer modified polypropylene compound intended for injection molding. The product is available in natural color. This material has excellent balanced mechanical properties.. |
|||
Flexural Modulus | 0.900 GPa | 131 ksi | ISO 178 |
Unipetrol PE HD LITEN® LS 87 HDPE Made for special applicationsInformation provided by Unipetrol RPA |
|||
Flexural Modulus | 0.900 GPa | 131 ksi | ISO 178 |
Unipetrol PE HD LITEN® MB/ML 62 HDPE Made for injection molding applications.Information provided by Unipetrol RPA |
|||
Flexural Modulus | 0.900 GPa | 131 ksi | ISO 178 |
Unipetrol PE HD LITEN® MB/ML 87 HDPE Made for injection molding applications.Information provided by Unipetrol RPA |
|||
Flexural Modulus | 0.900 GPa | 131 ksi | ASTM D790 |
A. Schulman POLYFORT™ PP 7001 Information provided by A. Schulman. |
|||
Flexural Modulus | 0.900 GPa | 131 ksi | 1.3 mm/min at 70°C |
A. Schulman POLYPUR™ FPU 1380 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Flexural Modulus | 0.900 GPa | 131 ksi | ASTM D790 |
A. Schulman POLYFORT™ PP 7001 Information provided by A. Schulman. |
|||
Flexural Modulus | 0.900 GPa | 131 ksi | at 70°C, tangent |
A. Schulman POLYPUR™ FPU 1376 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Flexural Modulus | 0.900 GPa | 131 ksi | 1.3 mm/min at 70°C |
A. Schulman POLYPUR™ FPU 1380 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Flexural Modulus | 0.900 GPa | 131 ksi | ISO 178 |
Unitika A1030SR PA6, Conditioned Information provided by Unitika Ltd. |
|||
Flexural Modulus | 0.900 GPa | 131 ksi | 1.3 mm/min at 70°C |
A. Schulman POLYPUR™ FPU 1380 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Flexural Modulus | 0.900 GPa | 131 ksi | ISO 178 |
Total PPR 3261 Random Copolymer Polypropylene, Extrusion Grade Polypropylene PPR 3261 is a high melt strength random copolymer polypropylene with a melt flow index of 1.8 g/10 min suitable for extrusion applications.Information provided by Total Petrochemicals... |
|||
Flexural Modulus | 0.900 GPa | 131 ksi | 3 pt. secant. ASTM D790 |
Chevron Phillips Marlex® 9346 HDPE Natural Pipe Resin Resin Type: Linear Copolymer; PE3408 Pipe Resin; ASTM D 3350 Classification:345464C when used with an approved color concentrate; ASTM D 4976 Classification: PE 235, A 56607Applications:Pressure Pip.. |
|||
Flexural Modulus | 0.900 GPa | 131 ksi | ISO 178 |
Ascend Performance Materials Vydyne® 66R Nylon 66, General Purpose, high viscosity, Conditioned Vydyne® 66R is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66R resin offers high strength, .. |
|||
Flexural Modulus | >= 0.900 GPa | >= 131 ksi | ASTM D790 |
Centro Plastica CiPiTENE® Recycled High Density Polyethylene Granules Bottle Grade. Source: Italian post-consumer plastic bottles coming from collection of municipal waste and selected by PE/PP matrix. |
|||
Flexural Modulus | 0.900 GPa | 131 ksi | STN EN ISO 178 |
Plastcom SLOVALEN PQ 51 N Polypropylene Homopolymer, Modified with Elastomer, Impacted FeaturesHomopolymer PP modified with elastomer. The addition of thermoplastic elastomer causes increased toughness, possible alternative to PP copolymers. General application in all industry branc.. |
|||
Flexural Modulus | 0.900 GPa | 131 ksi | 1.3 mm/min at 70°C |
A. Schulman POLYPUR™ FPU 1380 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Flexural Modulus | 0.900 GPa | 131 ksi | 80x10x4 mm specimen, 2 mm/min; ISO 178 |
Solvay Engineered Polymers DEXFLEX® 980HF TPO
(discontinued **) Description: DEXFLEX® 980HF is a thermoplastic olefinic elastomer (TPO) designed for large automotive exterior applications that require high flow for excellent processability, ductile impact prope.. |