Reliance Industries Polypropylene Random Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Reliance Industries
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Reliance Industries Polypropylene Random Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Typical properties of Reliance - Repol Polypropylene gradesInformation provided by Reliance Industries
Mechanical Properties Metric English Comments
Tensile Strength, Yield 25.0 - 28.0 MPa
3630 - 4060 psi
Elongation at Yield 10 - 12 %
10 - 12 %
Flexural Modulus 0.900 - 1.30 GPa
131 - 189 ksi
Izod Impact, Notched 0.600 J/cm
1.12 ft-lb/in
fiber
0.800 J/cm
1.50 ft-lb/in
blow molding
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 90.0 - 95.0 °C
194 - 203 °F