Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, H358/30 | 100 MPa | 14500 psi | ISO 2039-1 |
SABIC Innovative Plastics Cycolac® MG8000SR ABS This data was supplied by SABIC-IP for the Americas region. |
|||
Hardness, H358/30 | 100 MPa | 14500 psi | ISO 2039-1 |
SABIC Innovative Plastics Cycolac® MG8000SR ABS (Europe-Africa-Middle East) This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Hardness, H358/30 | 100 MPa | 14500 psi | ISO 2039-1 |
SABIC Innovative Plastics Cycolac® S157 ABS (Europe-Africa-Middle East) CYCOLAC S157 is a high flow flame retardant ABS with good processability developed for applications requiring UL94 V0 at reduced wall thickness.This data was supplied by SABIC-IP for the Europe-Afri.. |
|||
Hardness, H358/30 | 100 MPa | 14500 psi | ISO 2039-1 |
SABIC Innovative Plastics Cycoloy® CH6410 PC+ABS (Asia Pacific) CH6410 is a high heat, impact modified PC resin, with nonbrominated, nonchlorinated flame retardant system. Limited colors only. |
|||
Hardness, H358/30 | 100 MPa | 14500 psi | ISO 2039-1 |
SABIC Innovative Plastics Lexan® 2034 PC (Europe-Africa-Middle East) LEXAN 2034 is a medium viscosity flame retardant grade. The material is UV-stabilized. Glow wire at 960C also satisfies EDF spec HN 60-S-02. |
|||
Hardness, H358/30 | 100 MPa | 14500 psi | ISO 2039-1 |
SABIC Innovative Plastics Lexan® OQ1023 PC (Asia Pacific) Lexan OQ1023 resin is an optical high purity PC resin optimized for demanding recordable and rewritable formats (CD-R, DVD-R, DVD-RW). It is also suitable for short cycletime CD and DVD production |
|||
Hardness, H358/30 | 100 MPa | 14500 psi | ISO 2039-1 |
SABIC Innovative Plastics NORYL SE1GFN1 PPE+HIPS (Europe-Africa-Middle East) Noryl* SE1GFN1 is a 10% glass reinforced, injection moldable modified polyphenylene ether resin. Designed for improved dimensional stability and good flow , this resin also uses non-chlorinated, non.. |
|||
Hardness, H358/30 | 100 MPa | 14500 psi | ISO 2039-1 |
SABIC Innovative Plastics Noryl V0150BT PPE+HIPS (Asia Pacific) Noryl* V0150BT is an unfilled, injection moldable modified polyphenylene ether resin.. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 1.5 mm .. |
|||
Hardness, H358/30 | 100 MPa | 14500 psi | ISO 2039-1 |
SABIC Innovative Plastics Noryl V0150BT PPE+HIPS (Europe-Africa-Middle East) Noryl* V0150BT is an unfilled, injection moldable modified polyphenylene ether resin.. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 1.5 mm .. |
|||
Hardness, H358/30 | 100 MPa | 14500 psi | ISO 2039-1 |
SABIC Innovative Plastics Noryl V080 PPE+HIPS (Europe-Africa-Middle East) NORYL V080 is an unfilled, flame retardant, high flow material and is halogen free according to VDE/DIN 472 part 815.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Hardness, H358/30 | 100 MPa | 14500 psi | ISO 2039-1 |
SABIC Innovative Plastics NORYL V090 PPE+HIPS (Europe-Africa-Middle East) NORYL V090 is an unfilled, flame retardant material with a Vicat B/120 of 95 °C according ISO 306. NORYL V090 is V0 at 2.0 mm and V1 at 1.6 mm according UL94 and halogen free according VDE/DIN 47.. |
|||
Hardness, H358/30 | 100 MPa | 14500 psi | ISO 2039-1 |
SABIC Innovative Plastics Valox® DR51 PBT (Europe-Africa-Middle East) VALOX DR51 is a 15% glass fiber reinforced PBT injection moulding resin with excellent mechanical, thermal and electrical performance. Applications: spotlights, appliance housings, handles. |
|||
Hardness, H358/30 | 100 MPa | 14500 psi | ISO 2039-1 |
SABIC Innovative Plastics Valox® VX3101N PBT (Europe-Africa-Middle East) VALOX VX3101N is an unreinforced PBT injection moulding resin, with excellent flow properties, good hydrolitical stability and chemical resistance. |
|||
Hardness, H358/30 | 100 MPa | 14500 psi | ISO 2039-1 |
SABIC Innovative Plastics Xenoy® 6370 PBT+PC (Europe-Africa-Middle East) XENOY 6370 is an impact modified semi-crystalline thermoplastic. blend with 30% glass fibre reinforcement offering toughness and ductility. |
|||
Hardness, H358/30 | 100 MPa | 14500 psi | ISO 2039-1 |
SABIC Innovative Plastics NORYL GFN1720 PPE+HIPS (Europe-Africa-Middle East) Noryl* GFN1720 is a 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Noryl .. |
|||
Hardness, H358/30 | 100 MPa | 14500 psi | ISO 2039-1 |
SABIC Innovative Plastics NORYL GFN1V PPE+HIPS (Europe-Africa-Middle East) NORYL GFN1V is a 10 % glass fibre reinforced material with a HDT/A of 110C according ISO 75. NORYL GFN1V cust spec 1977 has been approved for potable water applications up to 85C by the UK WFBS acco.. |
|||
Hardness, H358/30 | 100 MPa | 14500 psi | ISO 2039-1 |
SABIC Innovative Plastics NORYL GFN2 PPE+HIPS (Europe-Africa-Middle East) NORYL GFN2 is a standard 20 % glass fibre reinforced material with a HDT/A of 130C according ISO 75. NORYL GFN2 can be used for all applications where a higher modulus is required. NORYL GFN2 is ava.. |
|||
Hardness, H358/30 | 100 MPa | 14500 psi | ISO 2039-1 |
SABIC Innovative Plastics NORYL GFN2V PPE+HIPS (Europe-Africa-Middle East) NORYL GFN2V is a 20 % glass fibre reinforced material with a HDT/A of 130C according ISO 75. NORYL GFN2V cust spec 1977 has been approved for potable water applications up to 85C by the UK WFBS acco.. |
|||
Hardness, H358/30 | 100 MPa | 14500 psi | ISO 2039-1 |
SABIC Innovative Plastics NORYL GTX GTX820 PPE+PA (Europe-Africa-Middle East) NORYL GTX820 is a 20% glass reinforced grade with excellent chemical resistance in combination with high stiffness and heat resistance. |
|||
Hardness, H358/30 | 100 MPa | 14500 psi | ISO 2039-1 |
SABIC Innovative Plastics NORYL HF185 PPE+HIPS (Europe-Africa-Middle East) NORYL HF185 is an unfilled, halogen free (according VDE/DIN 472 part 815), flame retardant and easy flow NORYL grade. |
|||
Hardness, H358/30 | 100 MPa | 14500 psi | ISO 2039-1 |
SABIC Innovative Plastics NORYL PPX PPX640 PPE+PP (Europe-Africa-Middle East) PPX640 is a 40% glass filled alloy of PP and PPO providing design freedom for applications requiring a wide range of stiffness, toughness and temperature. NSF Standard 61 Compliant (color limited)... |
|||
Hardness, H358/30 | 100 MPa | 14500 psi | ISO 2039-1 |
SABIC Innovative Plastics Valox® VX4910 ASA+PBT (Europe-Africa-Middle East) 10% Glass reinforced nucleated PBT/ASA with excellent mechanical properties high dimensional stability, and low density. |
|||
Hardness, H358/30 | 100 MPa | 14500 psi | ISO 2039-1 |
SABIC Innovative Plastics Xenoy® XL1562 PBT+PC (Europe-Africa-Middle East) XENOY XL1562 is an impact modified PBT+PC blend with outstanding chemical resistance, good UV stability and flow properties.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio.. |
|||
Hardness, H358/30 | 100 MPa | 14500 psi | ISO 2039-1 |
SABIC Innovative Plastics NORYL 731 PPE+HIPS (Europe-Africa-Middle East) NORYL 731 is an unfilled material, with a Vicat B/120 of 140C according ISO 306. NORYL 731 is a general purpose material with good balance of Strength, Impact and Flow. NORYL 731 is available in all.. |
|||
Hardness, H358/30 | 100 MPa | 14500 psi | ISO 2039-1 |
SABIC Innovative Plastics NORYL GFN1 PPE+HIPS (Europe-Africa-Middle East) NORYL GFN1 is a standard 10 % glass fibre reinforced material with a HDT/A of 110C according ISO 75. NORYL GFN1 can be used for all applications where a higher modulus is required. NORYL GFN1 is ava.. |
|||
Hardness, H358/30 | 100 MPa | 14500 psi | ISO 2039-1 |
SABIC Innovative Plastics NORYL GFN1720 PPE+HIPS Noryl* GFN1720 is a 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Noryl .. |
|||
Hardness, H358/30 | 100 MPa | 14500 psi | ISO 2039-1 |
SABIC Innovative Plastics NORYL GFN1720 PPE+HIPS (Asia Pacific) Noryl* GFN1720 is a 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Noryl .. |
|||
Hardness, H358/30 | 100 MPa | 14500 psi | ISO 2039-1 |
SABIC Innovative Plastics Cycoloy® CH6410 PC+ABS (Europe-Africa-Middle East) CH6410 is a high heat, impact modified PC resin, with nonbrominated, nonchlorinated flame retardant system. Limited colors only.This data was supplied by SABIC-IP for the Europe-Africa-Middle East r.. |
|||
Hardness, H358/30 | 100 MPa | 14500 psi | ISO 2039-1 |
SABIC Innovative Plastics Noryl EN130 PPE+HIPS (Europe-Africa-Middle East) NORYL EN130 is an extrusion material with a Vicat B/120 of 140 deg C according ISO 306. NORYL EN130 is a standard extrusion grade for applications where higher temperature resistance is required. NO.. |
|||
Hardness, H358/30 | 100 MPa | 14500 psi | ISO 2039-1 |
SABIC Innovative Plastics Cycoloy® CH6410 PC+ABS CH6410 is a high heat, impact modified PC resin, with nonbrominated, nonchlorinated flame retardant system. Limited colors only. |