Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 44.1 MPa
6400 psi
ASTM D638
Multibase Nylex™ 2185 HFX Natural Polyamide + PP
Forms: PelletsProcessing Methods:Injection moldingFeatures:Tensile Strength, HighInformation provided by Multibase
Tensile Strength, Ultimate 44.1 MPa
6400 psi
ASTM Data
Americas Styrenics Styron® 615APR Polystyrene  (discontinued **)
STYRON® 615 APR is a general purpose easy flow resin typically used for medical, pharmaceutical and thin-walled parts. It is an excellent resin for blending with K-Resin (K-Resin is a trademark of ..
Tensile Strength, Ultimate 44.1 MPa
6400 psi
50 mm/min; ASTM D638
Techno Polymer Techno ABS LM100 Transparent
Excellent shock resistance, rigidity, and processability.Applications: Appliance parts, office and computer equipment, machine parts, and tool handles.
Tensile Strength, Ultimate 44.1 - 80.0 MPa
6400 - 11600 psi
Average value: 67.0 MPa Grade Count:14
Overview of materials for Acrylic, Heat Resistant, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Heat Resistant, Molded". Each property range of values reported is minimum and maximum values o..
Tensile Strength, Ultimate 44.1 MPa
6400 psi
ASTM D638
Kolon DIAMAT® EG
Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl..
Tensile Strength, Ultimate 44.1 MPa
6400 psi
ASTM D638
Kolon DIAMAT® IG
Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl..
Tensile Strength, Ultimate 44.1 MPa

@Temperature 23.0 °C
6400 psi

@Temperature 73.4 °F
ASTM D638
IRPC Polimaxx Porene KU650 Acrylonitrile Butadiene Styrene
Applications:injection moldingautomotive parts such as instrument panels, console boxes, switches, automotive louvers, ectelectrical appliances
Tensile Strength, Ultimate 44.1 MPa

@Temperature 23.0 °C
6400 psi

@Temperature 73.4 °F
ASTM D638
IRPC Polimaxx Porene SP100 Acrylonitrile Butadiene Styrene
Applications:injection moldinghelmetsautomotive
Tensile Strength, Ultimate 44.1 MPa
6400 psi
Indium Corp. Indalloy® 255 Bi-Pb Fusible Alloy
General purpose fusible alloy. Poor solderability.Information provided by the manufacturer, Indium Corporation.
Tensile Strength, Ultimate 44.1 MPa
6400 psi
50 mm/min; ASTM D638
Techno Polymer Techno ABS LM100 Transparent
Excellent shock resistance, rigidity, and processability.Applications: Appliance parts, office and computer equipment, machine parts, and tool handles.
Tensile Strength, Ultimate 44.1 MPa
6400 psi
ASTM D412
SK Chemicals SKYTHANE® S368D Polyester Based Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Tensile Strength, Ultimate 44.1 MPa
6400 psi
ASTM D412
SK Chemicals SKYTHANE® S392A Polyester Based Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Tensile Strength, Ultimate 44.1 MPa
6400 psi
ASTM D638
SK Chemicals SKYTHANE® U101 Magnetic Binder
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Tensile Strength, Ultimate 44.1 MPa
6400 psi
ASTM D412
Lubrizol Estane® S160D Thermoplastic Polyurethane
Type: Estane® S160D is a Shore 63D, polyester based thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Availability: Americas, Europe, Middle East, ..
Tensile Strength, Ultimate 44.1 MPa
6400 psi
ASTM D412
Lubrizol Estane® S168D Thermoplastic Polyurethane
Type: Estane® S168D is a Shore 68D, polyester grade thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Availability: AsiaInformation Provided by The..
Tensile Strength, Ultimate 44.1 MPa
6400 psi
ASTM D412
Lubrizol Estane® S368D Thermoplastic Polyurethane
Type: Estane® S368D is a Shore 68D, polyester based thermoplastic polyurethane (TPU) with excellent transparency. FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Availability: Asi..
Tensile Strength, Ultimate 44.1 MPa
6400 psi
ASTM D412
Lubrizol Estane® S385AH Thermoplastic Polyurethane
Type: Estane® S385AH is a Shore 87A, polyester based thermoplastic polyurethane (TPU) with excellent transparency and Hydrolytic Stabilizer. FDA approved (21 CFR 177.2600, 177.1680).Uses: Injectio..
Tensile Strength, Ultimate 44.1 MPa
6400 psi
ASTM D412
Lubrizol Estane® S392A Thermoplastic Polyurethane
Type: Estane® S392A is a Shore 93A, polyester based thermoplastic polyurethane (TPU) with excellent transparency. FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding, Extrusion, Blow ..
Tensile Strength, Ultimate 44.1 MPa
6400 psi
ASTM D412
Lubrizol Estane® X-590A-31 Thermoplastic Polyurethane
Type: Estane® X-590A-31 is a Shore 91A, polyester grade without lubricant thermoplastic polyurethane (TPU). USP Class VI Certified.Uses: Extrusion, Film Blowing.Information Provided by The Lubrizo..
Tensile Strength, Ultimate 44.1 MPa
6400 psi
ASTM D412
Lubrizol Estane® 2102-65D Thermoplastic Polyurethane Elastomer
Formerly PellethaneAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009.
Tensile Strength, Ultimate 44.1 MPa
6400 psi
ASTM D412
Lubrizol Estane® 2103-55D Thermoplastic Polyurethane Elastomer
Formerly PellethaneFeature: Load bearing capacityAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in ..
Tensile Strength, Ultimate 44.1 MPa
6400 psi
ASTM D638
Buckeye Polymers BP ABS 5425 ABS
General PurposeABS is a copolymer of acrylonitrile and styrene, modified with butadiene rubber. ABS is primarily used for their combination of toughness, rigidity, chemical resistance, ease of proc..
Tensile Strength, Ultimate 44.1 MPa
6400 psi
ASTM D638
Buckeye Polymers BP ABS 7336 ABS
High Gloss & FlowABS is a copolymer of acrylonitrile and styrene, modified with butadiene rubber. ABS is primarily used for their combination of toughness, rigidity, chemical resistance, ease of pr..
Tensile Strength, Ultimate 44.1 MPa
6400 psi
ASTM D638-95
Multibase Multi-ABS 3246 High Flow Grade
Data provided by Multibase.
Tensile Strength, Ultimate 44.1 MPa
6400 psi
ASTM D412
Lubrizol Estane® S375D Thermoplastic Polyurethane
Type: Estane® S375D is a Shore 78D, polyester based thermoplastic polyurethane (TPU) with excellent transparency. FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Availability: Asi..
Tensile Strength, Ultimate 44.1 MPa
6400 psi
ASTM D412
SK Chemicals SKYTHANE® 392A S series Polyurethane
SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr..
Tensile Strength, Ultimate 44.1 MPa
6400 psi
ASTM D412
SK Chemicals SKYTHANE® 368D S series Polyurethane
SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr..