Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 100 MPa | 14500 psi | ASTM D638 |
PTS Trimid® N66-G13 13% Glass Fiber Reinforced Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength, Ultimate | 100 - 145 MPa @Temperature 130 - 180 °C |
14500 - 21000 psi @Temperature 266 - 356 °F |
Average value: 84.7 MPa Grade Count:13 |
Overview of materials for Polyphthalamide (PPA) This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide". Each property range of values reported is minimum and maximum values of appropriate Ma.. |
|||
Tensile Strength, Ultimate | 100 MPa | 14500 psi | ASTM D638 |
Plenco 50015 PET, Pellet, Injection Molded Natural Color
(discontinued **) PLENCO 50015 is an engineering grade glass reinforced polyethylene terephthalate resin designed for increased flexibility and good physical strength. It is UL recognized and available in white, natu.. |
|||
Tensile Strength, Ultimate | 100 MPa | 14500 psi | ISO 527 |
LATI LAPEX A G/10 10% Glass Fiber Reinforced Polyethersulfone (PES) (UL94 V-0)
(Unverified Data**) Description: Lapex A compounds are polyethersulfone (PES) products. They are high temperature compounds offering an interesting combination of properties. Lapex A provides outstanding thermal resist.. |
|||
Tensile Strength, Ultimate | 100 - 200 MPa | 14500 - 29000 psi | Average value: 162 MPa Grade Count:12 |
Overview of materials for Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled". Specific grades with glass content between 15% an.. |
|||
Tensile Strength, Ultimate | 100 - 115 MPa @Temperature 130 - 175 °C |
14500 - 16700 psi @Temperature 266 - 347 °F |
Average value: 101 MPa Grade Count:5 |
Overview of materials for Nylon 66, 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. .. |
|||
Tensile Strength, Ultimate | 100 MPa @Temperature 1095 °C |
14500 psi @Temperature 2003 °F |
|
Haynes 556® alloy, cold rolled, solution annealed sheet, 0.8-2.8 mm thick Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |
|||
Tensile Strength, Ultimate | 100 MPa | 14500 psi | ASTM D638 |
Styron EMERGEâ„¢ 8702 Polycarbonate EMERGEâ„¢ PC 8702 advanced resin is an ignition-resistant, 20% glass reinforced, polycarbonate resin. This resin contains no bromide, chloride, or phosphate additives. It is a medium flow PC re.. |
|||
Tensile Strength, Ultimate | 100 MPa | 14500 psi | |
Covestro Makrolon® 9425 Polycarbonate High viscosity, flame retardant extrusion and injection molding grade with 20% standard glass fibers and easy mold release agent.Information provided by Bayer.As of 1 September 2015, Bayer MaterialS.. |
|||
Tensile Strength, Ultimate | 100 MPa @Temperature 120 °C |
14500 psi @Temperature 248 °F |
ISO 527-1/-2 |
DSM Stanyl® OCD2100 BK27021 PA46-GF40 40% Glass Reinforced, Heat Stabilized |
|||
Tensile Strength, Ultimate | 100 MPa | 14500 psi | |
China Tungsten STG30-10 PM Structural Parts Information provided by China Tungsten |
|||
Tensile Strength, Ultimate | 100 MPa | 14500 psi | ASTM D638 |
Adell BJ-34 Nylon 6, 20% Glass Reinforced; High Impact Data provided by Adell Plastics, Inc. |
|||
Tensile Strength, Ultimate | 100 MPa | 14500 psi | ASTM D638 |
Adell BR-13 Nylon 6, 15% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Tensile Strength, Ultimate | 100 MPa | 14500 psi | ASTM D638 |
Adell BR-33 Nylon 6, 15% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Tensile Strength, Ultimate | 100 MPa | 14500 psi | ISO 527-1/-2 |
DSM Arnite® TZ6 280 PBT-(GF+GB)40 20% Glass Reinforced, 20% Glass Beads Reinforced |
|||
Tensile Strength, Ultimate | 100 MPa | 14500 psi | ASTM data at 5 mm/min. |
BASF Capron® HPN 9333G HS Impact Modified, 33% Glass-Filled Nylon 6 (Conditioned)
(discontinued **) Capron HPN 9333G HS is a heat stabilized, 33% glass reinforced, impact modified polyamide 6 injection molding compound combining exceptional strength, stiffness and high temperature performance with.. |
|||
Tensile Strength, Ultimate | 100 MPa @Temperature 900 °C |
14500 psi @Temperature 1650 °F |
|
Resistalloy International Resistalloy 6015 Nickel Chromium Electrical Resistance Alloy Used mainly for electrical elements in both industrial and domestic applications. Industrial applications vary from small laboratory kilns to heavy-duty heat-treatment furnaces under all types of at.. |
|||
Tensile Strength, Ultimate | 100 MPa | 14500 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Lubri-Tech™ MP-20CF/15T Modified Polyphenylene Oxide (mPPO), Carbon Fiber Reinforced, PTFE Lubricated
  Description/Features:Carbon Fiber ReinforcedPTFE LubricatedUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Ultimate | 100 MPa | 14500 psi | ASTM D638 |
Adell ER-39 Polypropylene Homopolymer; 43% Glass Reinforced, High Stiffness Data provided by Adell Plastics, Inc. |
|||
Tensile Strength, Ultimate | 100 - 107.5 MPa @Temperature 130 - 180 °C |
14500 - 15590 psi @Temperature 266 - 356 °F |
Average value: 100 MPa Grade Count:4 |
Overview of materials for Polyphthalamide (PPA), 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are.. |
|||
Tensile Strength, Ultimate | 100 - 300 MPa | 14500 - 43500 psi | Average value: 208 MPa Grade Count:29 |
Overview of materials for Polyphthalamide (PPA), Carbon Fiber + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Carbon Fiber + PTFE Filled". Each property range of values reported is minimum and maxi.. |
|||
Tensile Strength, Ultimate | 100 MPa @Temperature 900 °C |
14500 psi @Temperature 1650 °F |
|
Resistalloy International Resistalloy 8020 Nickel Chromium Electrical Resistance Alloy Used mainly for electrical elements in both industrial and domestic applications. Industrial applications vary from small laboratory kilns to heavy-duty heat-treatment furnaces under all types of at.. |
|||
Tensile Strength, Ultimate | 100 MPa | 14500 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® AM-30GM/15TF Polyphthalamide (PPA), Glass Filled, PTFE Lubricated
(discontinued **) Description/Features:Glass Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Ultimate | 100 MPa | 14500 psi | 5mm/min; ISO 527 |
BASF Ultramid® N-265 NF3001 40% Mineral Filled PA66 (Dry) Ultramid N-265 NF3001 is a general purpose, 40% mineral reinforced PA6/6 that provides excellent flatness and dimensional stability in injection molding. |