Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 18.0 J @Temperature 23.0 °C |
13.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycoloy® RCY6013 PC+ABS (Asia Pacific) Cycoloy* RCY6013 resin is an injection moldable high flow PC/ABS blend with non-brominated and non-chlorinated flame retardant. It contains 30% post consumer recycle content with a UL-94 V0 @ 1.5 mm.. |
|||
Dart Drop, Total Energy | 18.0 J @Temperature 23.0 °C |
13.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics NORYL SE1GFN2 PPE+PS (Asia Pacific) PPE+PS blend. 20% Glass reinforced. Non-brominated, non-chlorinated FR system. UL94 V1 listing. Dielectric strength. Dimensional stability. Suitable for E/E applications. |
|||
Dart Drop, Total Energy | 18.0 J @Temperature 23.0 °C |
13.3 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak, 6.6 m/s; ASTM D3763 |
SABIC Innovative Plastics SABIC PPCOMPOUND 55T1030 PP SABIC® PPcompound 55T1030 is a general purpose, talc filled, heat stabilized copolymer polypropylene compound. This compound exhibits very high impact, and is suitable for multiple processing met.. |
|||
Dart Drop, Total Energy | 18.0 J @Temperature 23.0 °C |
13.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics ULTEM 2410EPR PEI 40% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release for enhanced electroplatability. ECO Conforming, UL94 V0 listing. |
|||
Dart Drop, Total Energy | 18.0 J @Temperature 23.0 °C |
13.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics ULTEM 2410EPR PEI (Asia Pacific) 40% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release for enhanced electroplatability. ECO Conforming, UL94 V0 listing. |
|||
Dart Drop, Total Energy | 18.0 J @Temperature 23.0 °C |
13.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP STAT-KON CD000I PS LNP* Stat-kon* CD000I is a compound based on Polystyrene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact. |
|||
Dart Drop, Total Energy | 18.0 J | 13.3 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP STAT-KON DE0039 PC LNP* STAT-KON* DE0039 is a compound based on Polycarbonate resin containing 15% Carbon Fiber. Added features of this material include: Flame Retardant. Electrically Conductive. |
|||
Dart Drop, Total Energy | 18.0 J @Temperature 23.0 °C |
13.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP DF002 PC LNP THERMOCOMP* DF002 is a compound based on Polycarbonate resin containing 10% Glass Fiber. |
|||
Dart Drop, Total Energy | 18.0 J @Temperature 23.0 °C |
13.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP DF002H PC LNP THERMOCOMP* DF002H is a compound based on Polycarbonate resin containing 10% Glass Fiber. Added feature includes: Healthcare. |
|||
Dart Drop, Total Energy | 18.0 J | 13.3 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP PF00A PA 6 LNP THERMOCOMP* PF00A is a compound based on Nylon 6 resin containing 50% Glass Fiber. |
|||
Dart Drop, Total Energy | 18.0 J | 13.3 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP PF00ASXS PA 6 (Asia Pacific) LNP THERMOCOMP* PF00ASXS is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Dart Drop, Total Energy | 18.0 J @Temperature 23.0 °C |
13.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP RF008 PA 66 LNP* THERMOCOMP* RF-1008 is a compound based on Nylon 66 resin containing Glass Fiber. |
|||
Dart Drop, Total Energy | 18.0 J @Temperature 23.0 °C |
13.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics NORYL GFN1740V PPE+PS (Asia Pacific) Noryl* GFN1740V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 40 % Glass Reinforced, injection moldable grade with improved hydrolytic stability and with a Tensile Modulus > 11000 MPa; thi.. |
|||
Dart Drop, Total Energy | 18.0 J @Temperature 23.0 °C |
13.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics NORYL GFN1740V PPE+PS (Europe-Africa-Middle East) Noryl* GFN1740V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 40 % Glass Reinforced, injection moldable grade with improved hydrolytic stability and with a Tensile Modulus > 11000 MPa; thi.. |
|||
Dart Drop, Total Energy | 18.0 J @Temperature 23.0 °C |
13.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics NORYL NH6020 PPE+HIPS (Asia Pacific) Noryl NH6020 resin is an unfilled, injection moldable modified polyphenylene ether resin. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 0.8 .. |
|||
Dart Drop, Total Energy | 18.0 J @Temperature 23.0 °C |
13.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics NORYL NH6020 PPE+HIPS (Europe-Africa-Middle East) Noryl* NH6020 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 0.8 mm an.. |
|||
Dart Drop, Total Energy | 18.0 J @Temperature 23.0 °C |
13.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics ULTEM HU2410 PEI 40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP.. |
|||
Dart Drop, Total Energy | 18.0 J @Temperature 23.0 °C |
13.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics ULTEM HU2410 PEI (Asia Pacific) 40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP.. |
|||
Dart Drop, Total Energy | 18.0 J | 13.3 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP HF008 PA11 LNP THERMOCOMP* HF008 is a compound based on Nylon 11 resin containing 40% Glass Fiber. |
|||
Dart Drop, Total Energy | 18.0 J | 13.3 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP NF004 PC+ABS LNP* THERMOCOMP* NF004 is a compound based on PC+ABS resin containing 20% Glass Fiber. |
|||
Dart Drop, Total Energy | 18.0 J | 13.3 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP NF004 PC+ABS (Asia Pacific) LNP* Thermocomp* NF004 is a compound based on PC+ABS Blend resin containing Glass Fiber. |
|||
Dart Drop, Total Energy | 18.0 J @Temperature 23.0 °C |
13.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP RF008XXH PA 66 LNP* THERMOCOMP* RF008XXH is a compound based on Nylon 66 resin containing 40% Glass Fiber. Added feature of this material includes: Healthcare. |
|||
Dart Drop, Total Energy | 18.0 J | 13.3 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP VERTON RX06424 PA 66 (Asia Pacific) LNP VERTON* RX06424 is a compound based on Nylon 66 resin containing Long Glass. Added features of this material include: Easy Molding. |
|||
Dart Drop, Total Energy | 18.0 J | 13.3 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP DFL329 PC LNP LUBRICOMP* DFL329 is a compound based on Polycarbonate resin containing 10% Glass Fiber, 15% PTFE. Added features of this material include: Flame Retardant, Internally Lubricated. |
|||
Dart Drop, Total Energy | 18.0 J | 13.3 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP VERTON RV00CES PA 66 LNP VERTON* RV00CES is a compound based on Nylon 66 resin containing 60% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, Structural. |
|||
Dart Drop, Total Energy | 18.0 J | 13.3 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP VERTON RV00CESS PA 66 LNP VERTON* RV00CESS is a compound based on Nylon 66 resin containing 60% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, Structural. |
|||
Dart Drop, Total Energy | 18.0 J | 13.3 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP VERTON RV00CESS PA 66 (Asia Pacific) LNP VERTON* RV00CESS is a compound based on Nylon 66 resin containing Long Glass. Added features of this material include: Easy Molding. |
|||
Dart Drop, Total Energy | 18.0 J | 13.3 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP VERTON RX06424 PA 66 LNP VERTON* RX06424 is a compound based on Nylon 66 resin containing 60% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, UV Stabilized, Structural |
|||
Dart Drop, Total Energy | 18.0 J | 13.3 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP 2X04505 ETFE LNP* THERMOCOMP* 2X04505 is a compound based on ETFE resin containing Proprietary Filler(s). |
|||
Dart Drop, Total Energy | 18.0 J @Temperature 23.0 °C |
13.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics NORYL FE1740PW PPE+PS (Europe-Africa-Middle East) Noryl* FE1740PW Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 40 % Glass Reinforced, injection moldable grade with improved hydrolytic stability and with a Tensile Modulus > 11000 MPa; thi.. |