Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP STAT-KON DE0039 PC

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP STAT-KON
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF SABIC Innovative Plastics LNP STAT-KON DE0039 PC.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
LNP* STAT-KON* DE0039 is a compound based on Polycarbonate resin containing 15% Carbon Fiber. Added features of this material include: Flame Retardant. Electrically Conductive.
Physical Properties Metric English Comments
Density 1.29 g/cc
0.0466 lb/in³
ISO 1183
1.30 g/cc
0.0470 lb/in³
ASTM D792
Moisture Absorption 0.100 %
0.100 %
50% RH, 24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.0013 cm/cm
<br>@Time 86400 sec
0.0013 in/in
<br>@Time 24.0 hour
ISO 294
0.0010 - 0.0030 cm/cm
<br>@Time 86400 sec
0.0010 - 0.0030 in/in
<br>@Time 24.0 hour
ASTM D955
Linear Mold Shrinkage, Transverse 0.0038 cm/cm
<br>@Time 86400 sec
0.0038 in/in
<br>@Time 24.0 hour
ISO 294
0.0030 - 0.0050 cm/cm
<br>@Time 86400 sec
0.0030 - 0.0050 in/in
<br>@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 118 MPa
17100 psi
ASTM D638
119 MPa
17300 psi
ISO 527
Tensile Strength, Yield 118 MPa
17100 psi
ASTM D638
119 MPa
17300 psi
ISO 527
Elongation at Break 2.4 %
2.4 %
ASTM D638
2.4 %
2.4 %
ISO 527
Elongation at Yield 2.3 %
2.3 %
ISO 527
2.4 %
2.4 %
ASTM D638
Tensile Modulus 9.26 GPa
1340 ksi
1 mm/min; ISO 527
9.65 GPa
1400 ksi
50 mm/min; ASTM D638
Flexural Strength 144 MPa
20900 psi
ASTM D790
181 MPa
26300 psi
ISO 178
Flexural Modulus 7.58 GPa
1100 ksi
ASTM D790
8.60 GPa
1250 ksi
ISO 178
Izod Impact, Notched 0.640 J/cm
1.20 ft-lb/in
ASTM D256
Izod Impact, Unnotched 5.50 J/cm
10.3 ft-lb/in
ASTM D4812
Izod Impact, Notched (ISO) 6.00 kJ/m²
2.86 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 32.0 kJ/m²
15.2 ft-lb/in²
80*10*4; ISO 180/1U
Dart Drop, Total Energy 18.0 J
13.3 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
Impact Test 4.00 J
2.95 ft-lb
Multiaxial Impact; ISO 6603
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 45.0 µm/m-°C
<br>@Temperature -40.0 - 40.0 °C
25.0 µin/in-°F
<br>@Temperature -40.0 - 104 °F
ASTM E 831
45.0 µm/m-°C
<br>@Temperature -40.0 - 40.0 °C
25.0 µin/in-°F
<br>@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow 37.8 µm/m-°C
<br>@Temperature -40.0 - 40.0 °C
21.0 µin/in-°F
<br>@Temperature -40.0 - 104 °F
ASTM E 831
38.0 µm/m-°C
<br>@Temperature -40.0 - 40.0 °C
21.1 µin/in-°F
<br>@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 150 °C
302 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
150 °C
<br>@Thickness 3.20 mm
302 °F
<br>@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 146 °C
295 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
147 °C
<br>@Thickness 3.20 mm
297 °F
<br>@Thickness 0.126 in
unannealed; ASTM D648
Electrical Properties Metric English Comments
Surface Resistance 100 - 1.00e+6 ohm
100 - 1.00e+6 ohm
ASTM D257