Category | Polymer , Thermoplastic , Polyetherimide (PEI) |
Manufacturer | SABIC Innovative Plastics (GE Plastics) |
Trade Name | ULTEM |
Port | Shanghai port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Download PDF | SABIC Innovative Plastics ULTEM HU2410 PEI.pdf ![]() |
Price | EMAIL US sales@lookpolymers.com |
Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.61 g/cc | 1.61 g/cc | ASTM D792 |
Density | 1.56 g/cc | 0.0564 lb/in³ | ISO 1183 |
Water Absorption | 0.13 % @Time 86400 sec |
0.13 % @Time 24.0 hour |
ASTM D570 |
Moisture Absorption | 0.400 % | 0.400 % | 23°C / 50% RH; ISO 62 |
Moisture Absorption at Equilibrium | 0.90 % | 0.90 % | ASTM D570 |
Water Absorption at Saturation | 0.80 % | 0.80 % | ISO 62 |
Linear Mold Shrinkage, Flow | 0.0010 - 0.0030 cm/cm @Thickness 3.20 mm |
0.0010 - 0.0030 in/in @Thickness 0.126 in |
SABIC Method |
Melt Flow | 5.2 g/10 min @Load 6.60 kg, Temperature 337 °C |
5.2 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
Melt Index of Compound | 11 g/10 min @Load 5.00 kg, Temperature 220 °C |
11 g/10 min @Load 11.0 lb, Temperature 428 °F |
MVR [cm^3/10 min]; ISO 1133 |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 179 MPa | 26000 psi | Type I, 5 mm/min; ASTM D638 |
180 MPa | 26100 psi | 5 mm/min; ISO 527 | |
Tensile Strength, Yield | 180 MPa | 26100 psi | 5 mm/min; ISO 527 |
186 MPa | 27000 psi | Type I, 5 mm/min; ASTM D638 | |
Elongation at Break | 2.0 % | 2.0 % | 5 mm/min; ISO 527 |
2.5 % | 2.5 % | Type I, 5 mm/min; ASTM D638 | |
Elongation at Yield | 2.0 % | 2.0 % | 5 mm/min; ISO 527 |
2.5 % | 2.5 % | Type I, 5 mm/min; ASTM D638 | |
Tensile Modulus | 11.5 GPa | 1670 ksi | 1 mm/min; ISO 527 |
11.72 GPa | 1700 ksi | 5 mm/min; ASTM D638 | |
Flexural Yield Strength | 240 MPa | 34800 psi | 2 mm/min; ISO 178 |
254 MPa | 36800 psi | 1.3 mm/min, 50 mm span; ASTM D790 | |
Flexural Modulus | 10.0 GPa | 1450 ksi | 2 mm/min; ISO 178 |
11.43 GPa | 1658 ksi | 1.3 mm/min, 50 mm span; ASTM D790 | |
Izod Impact, Notched | 1.12 J/cm | 2.10 ft-lb/in | ASTM D256 |
1.14 J/cm @Temperature -30.0 °C |
2.14 ft-lb/in @Temperature -22.0 °F |
ASTM D256 | |
Izod Impact, Unnotched | 4.27 J/cm | 8.00 ft-lb/in | ASTM D4812 |
Izod Impact, Notched (ISO) | 10.0 kJ/m² | 4.76 ft-lb/in² | 80*10*4; ISO 180/1A |
10.0 kJ/m² @Temperature -30.0 °C |
4.76 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A | |
Charpy Impact, Notched | 1.00 J/cm² | 4.76 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
Dart Drop, Total Energy | 18.0 J @Temperature 23.0 °C |
13.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 14.4 µm/m-°C @Temperature -20.0 - 150 °C |
8.00 µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E 831 |
15.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
8.33 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 | |
CTE, linear, Transverse to Flow | 45.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
25.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
45.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
25.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 | |
Deflection Temperature at 1.8 MPa (264 psi) | 197 °C | 387 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
212 °C @Thickness 6.40 mm |
414 °F @Thickness 0.252 in |
unannealed; ASTM D648 | |
Vicat Softening Point | 214 °C | 417 °F | Rate B/50; ISO 306 |
215 °C | 419 °F | Rate B/120; ISO 306 | |
234 °C | 453 °F | Rate B/50; ASTM D1525 | |
Glass Transition Temp, Tg | 217 °C | 423 °F | |
Oxygen Index | 54 % | 54 % | ASTM D2863 |
Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.50e+16 ohm-cm | 1.50e+16 ohm-cm | ASTM D257 |
Dielectric Constant | 3.7 @Frequency 1000 Hz |
3.7 @Frequency 1000 Hz |
ASTM D150 |
Dielectric Strength | 24.0 kV/mm @Thickness 1.60 mm |
610 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
Dissipation Factor | 0.0020 @Frequency 1000 Hz |
0.0020 @Frequency 1000 Hz |
ASTM D150 |