Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 11.0 J | 8.11 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP FARADEX AS002 ABS LNP* Faradex* AS002 is a compound based on Acrylonitrile Butadiene Styrene resin containing 10% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding... |
|||
Dart Drop, Total Energy | 11.0 J | 8.11 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP FARADEX AS002 ABS (Asia Pacific) LNP* Faradex* AS002 is a compound based on Acrylonitrile Butadiene Styrene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Dart Drop, Total Energy | 11.0 J | 8.11 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP FARADEX AS002 ABS (Europe-Africa-Middle East) LNP* Faradex* AS002 is a compound based on Acrylonitrile Butadiene Styrene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Dart Drop, Total Energy | 11.0 J | 8.11 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP KONDUIT PTF2BXXX PA 6 LNP KONDUIT* PTF2BXXX is a compound based on Nylon 6 resin containing 10% Glass Fiber, 55% Proprietary Thermal Filler. Added features of this material include: Thermally Conductive. |
|||
Dart Drop, Total Energy | 11.0 J | 8.11 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP KONDUIT PTF2BXXX PA 6 (Asia Pacific) LNP KONDUIT* PTF2BXXX is a compound based on Nylon 6 resin containing Glass Fiber, Proprietary Thermal Filler. Added features of this material include: Thermally Conductive. |
|||
Dart Drop, Total Energy | 11.0 J | 8.11 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP DFL32 PC LNP LUBRICOMP* DFL32 is a compound based on Polycarbonate resin containing 10% Glass Fiber and 15% PTFE. Added features of this material include: Internally Lubricated. |
|||
Dart Drop, Total Energy | 11.0 - 35.0 J | 8.11 - 25.8 ft-lb | Average value: 18.1 J Grade Count:19 |
Overview of materials for Polycarbonate/ABS Alloy, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Glass Fiber Filled". Each property range of values reported is minimum and maxi.. |
|||
Dart Drop, Total Energy | 11.0 J @Temperature 23.0 °C |
8.11 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP ECL36XXQ PEI LNP* Lubricomp* ECL36XXQ is a compound based on Polyetherimide containing 30% Carbon Fiber, 15% PTFE. Added features of this material include: Internally Lubricated. |
|||
Dart Drop, Total Energy | 11.0 J @Temperature 23.0 °C |
8.11 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP OFL36 PPS - Linear LNP* LUBRICOMP* OFL36 is a compound based on PPS - Linear resin containing 30% Glass Fiber, 15% PTFE. Added features of this grade include: Wear Resistant. |
|||
Dart Drop, Total Energy | 11.0 J | 8.11 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRILOY DF2041 PC LNP LUBRILOY* DF2041 is a compound based on Polycarbonate resin containing 20% Glass Fiber, Proprietary Lubricant. Added features include: Flame Retardant. |
|||
Dart Drop, Total Energy | 11.0 J @Temperature 23.0 °C |
8.11 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP LUBRILOY RF203AXH PA 66 LNP* LUBRILOY* RF203AXH is a compound based on Nylon 66 resin containing 15% Glass Fiber, Proprietary Lubricant. Added features of this material include: Wear Resistant, Healthcare. |
|||
Dart Drop, Total Energy | 11.0 J | 8.11 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP STAT-KON DD0009XP PC (Asia Pacific) LNP* Stat-kon* DD0009XP is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include:Electrically Conductive, Flame Retardant. Also known as Stat-Kon*.. |
|||
Dart Drop, Total Energy | 11.0 J | 8.11 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP STAT-KON DX01303C PC LNP STAT-KON* DX01303C is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive. |
|||
Dart Drop, Total Energy | 11.0 J | 8.11 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP STAT-KON DX04489C PC LNP STAT-KON* DX04489C is a high modulus compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Clean Compounding System, Electrically Con.. |
|||
Dart Drop, Total Energy | 11.0 J @Temperature 23.0 °C |
8.11 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP STAT-KON EEF42 PEI LNP STAT-KON* EEF42 is a compound based on Polyetherimide resin containing 10% Carbon Fiber, 20% Glass Fiber. Added features of this material include: Electrically Conductive. |
|||
Dart Drop, Total Energy | 11.0 J | 8.11 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP STAT-KON Lexan_LCF1506 PC LNP* Stat-kon* Lexan_LC1500N compound is a 15% carbon fiber, 6% PTFE reinforced polycarbonate. |
|||
Dart Drop, Total Energy | 11.0 J | 8.11 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP STAT-KON Lexan_LCF1506 PC (Europe-Africa-Middle East) LNP* Stat-kon* Lexan_LCF1506 is a 15% carbon fiber, 6% PTFE reinforced polycarbonate. |
|||
Dart Drop, Total Energy | 11.0 J | 8.11 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP STAT-KON ZE0039 MODIFIED POLYPHENYLENE (Asia Pacific) LNP* Stat-kon* ZE0039 is a compound based on MODIFIED POYPHENYLENE resin containing Carbon Fiber. |
|||
Dart Drop, Total Energy | 11.0 J | 8.11 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP STAT-KON ZE0039 PPO LNP* STAT-KON* ZE0039 is a compound based on PPO resin containing 15% Carbon Fiber. Added features of this grade includes: Flame Retardant, Electrically Conductive. |
|||
Dart Drop, Total Energy | 11.0 J | 8.11 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP DC006H PC LNP* THERMOCOMP* DC006H is a compound based on Polycarbonate resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive, Healthcare. |
|||
Dart Drop, Total Energy | 11.0 J | 8.11 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP DC006H PC (Asia Pacific) LNP* Thermocomp* DC006H is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Dart Drop, Total Energy | 11.0 J @Temperature 23.0 °C |
8.11 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP EC005 PEI LNP THERMOCOMP* EC005 is a compound based on Polyetherimide resin containing 25% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Dart Drop, Total Energy | 11.0 J @Temperature 23.0 °C |
8.11 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP EX93452 PEI LNP THERMOCOMP* EX93452 is a compound based on Polyetherimide resin containing Proprietary Fillers. Added features of this material include: Electrically Conductive. |
|||
Dart Drop, Total Energy | 11.0 J | 8.11 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP RF004H PA 66 LNP* THERMOCOMP* RF004H is a compound based on Nylon 66 containing 20% Glass Fiber. Added feature of this grade is: Healthcare. |
|||
Dart Drop, Total Energy | 11.0 J @Temperature 23.0 °C |
8.11 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP RF009S PA 66 LNP* THERMOCOMP* RF009S is a compound based on Nylon 66 resin containing 45% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Dart Drop, Total Energy | 11.0 J | 8.11 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP WF006 PBT LNP THERMOCOMP* WF006 is a compound based on PBT resin containing 30% Glass Fiber. |
|||
Dart Drop, Total Energy | 11.0 J @Temperature 23.0 °C |
8.11 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP YH0235AC PE LNP* Thermocomp* YH0235AC is a compound based on Polyester Elastomer containing a metal filler. |
|||
Dart Drop, Total Energy | 11.0 J @Temperature -30.0 °C |
8.11 ft-lb @Temperature -22.0 °F |
Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics NORYL N225X PPE+PS PPE+PS blend. Unfilled. Halogen-Free FR performance. UL94 V0/5VA. UL746C F1. Dielectric Strength. Suitable for E/E market indoor/outdoor applications. |
|||
Dart Drop, Total Energy | 11.0 J @Temperature 23.0 °C |
8.11 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP VERTON RV0079 PA 66 LNP VERTON* RV0079 is a compound based on Nylon 66 resin containing 35% Long Glasss Fiber. Added features of this material include: Flame Retardant, Structural. |
|||
Dart Drop, Total Energy | 11.0 - 38.3697 J @Temperature -30.0 - -29.0 °C |
8.11 - 28.3000 ft-lb @Temperature -22.0 - -20.2 °F |
Average value: 25.5 J Grade Count:12 |
Overview of materials for Polypropylene Copolymer This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Copolymer". Each property range of values reported is minimum and maximum values of approp.. |