Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 55.0 kJ/m² @Temperature -30.0 °C |
26.2 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics Cycolac® S157 ABS (Europe-Africa-Middle East) CYCOLAC S157 is a high flow flame retardant ABS with good processability developed for applications requiring UL94 V0 at reduced wall thickness.This data was supplied by SABIC-IP for the Europe-Afri.. |
|||
Izod Impact, Unnotched (ISO) | 55.0 kJ/m² @Temperature -30.0 °C |
26.2 ft-lb/in² @Temperature -22.0 °F |
ISO 180-1U |
Ineos ABS Triax® KU2-3154 ABS + Polyamide Blend (Conditioned), Injection Molding Grade Triax® KU2-3154 is mineral reinforced, easy-flowing, injection molding grade, and comes in pellets. It has reduced moisture absorption and very low warpage. |
|||
Izod Impact, Unnotched (ISO) | 55.0 kJ/m² @Temperature -30.0 °C |
26.2 ft-lb/in² @Temperature -22.0 °F |
Conditioned; ISO 180-1U |
Lanxess Durethan® AKV 30 H3.0 000000 Nylon 66, 30% Glass Fibers PA 66, 30% glass fibers, injection molding, heat-ageing stabilized |
|||
Izod Impact, Unnotched (ISO) | 55.0 kJ/m² @Temperature 23.0 °C |
26.2 ft-lb/in² @Temperature 73.4 °F |
d.a.m.; ISO 180-1U |
Lanxess Durethan® AM 40 X H2.0 901510 Nylon 66, Glass Fiber/Mineral Reinforced PA 66, 40% glass fibers/mineral, injection molding, heat-aging stabilized, low tendency to warpInformation provided by LANXESS. |
|||
Izod Impact, Unnotched (ISO) | 55.0 kJ/m² @Temperature 23.0 °C |
26.2 ft-lb/in² @Temperature 73.4 °F |
cond.; ISO 180-1U |
Lanxess Durethan® AM 40 X H2.0 901510 Nylon 66, Glass Fiber/Mineral Reinforced PA 66, 40% glass fibers/mineral, injection molding, heat-aging stabilized, low tendency to warpInformation provided by LANXESS. |
|||
Izod Impact, Unnotched (ISO) | 55.0 kJ/m² @Temperature 23.0 °C |
26.2 ft-lb/in² @Temperature 73.4 °F |
ISO 180-1U |
Lanxess Durethan® BKV 115 H2.0 DUS008 000000 Nylon 6, 15% Glass Fiber PA 6, 15% glass fibers, injection molding, impact modified, heat-ageing stabilizedInformation provided by LANXESS. |
|||
Izod Impact, Unnotched (ISO) | 55.0 kJ/m² @Temperature -30.0 °C |
26.2 ft-lb/in² @Temperature -22.0 °F |
cond.; ISO 180-1U |
Lanxess Durethan® BKV 130 GIT DUS008 900116 Nylon 6, Impact Modified PA 6, 30% glass fibers, injection molding, impact modified, GIT/WITInformation provided by LANXESS. |
|||
Izod Impact, Unnotched (ISO) | 55.0 kJ/m² @Temperature 23.0 °C |
26.2 ft-lb/in² @Temperature 73.4 °F |
cond.; ISO 180-1U |
Lanxess Durethan® BKV 25 F30 000000 Nylon 6, Glass Fiber Reinforced, Flame Retardant PA 6, 25% glass fibers, injection molding, flame retardantInformation provided by LANXESS. |
|||
Izod Impact, Unnotched (ISO) | 55.0 kJ/m² @Temperature 23.0 °C |
26.2 ft-lb/in² @Temperature 73.4 °F |
d.a.m.; ISO 180-1U |
Lanxess Durethan® DP 2-2240/15 H2.0 901510 Nylon 66, 15% Glass Fiber PA 66, 15% glass fibers, blow molding, heat-aging stabilized, hydrolysis stabilizedInformation provided by LANXESS. |
|||
Izod Impact, Unnotched (ISO) | 55.0 kJ/m² @Temperature -30.0 °C |
26.2 ft-lb/in² @Temperature -22.0 °F |
cond.; ISO 180-1U |
Lanxess Durethan® DP A 30 S FN30 DUS025 000000 Nylon 66 PA 66, non-reinforced, injection molding, halogen free flame retardant improved flowabilityInformation provided by LANXESS. |
|||
Izod Impact, Unnotched (ISO) | 55.0 kJ/m² @Temperature 23.0 °C |
26.2 ft-lb/in² @Temperature 73.4 °F |
ISO 180-1U |
Lanxess Pocan® BF 4130 XF 000000 PBT, 30% Glass Fiber PBT, 30% glass fibers, injection molding, flame retardant, improved flowabilityInformation provided by LANXESS. |
|||
Izod Impact, Unnotched (ISO) | 55.0 kJ/m² @Temperature 23.0 °C |
26.2 ft-lb/in² @Temperature 73.4 °F |
ISO 180-1U |
Lanxess Pocan® ECO T 3230 000000 PBT + PET, 30% Glass Fiber PBT + PET, 30% glass fibers, injection molding, improved surface finish, contains 30% post-consumer recycled material, increased temperature peak loadInformation provided by LANXESS. |
|||
Izod Impact, Unnotched (ISO) | 55.0 kJ/m² @Temperature 23.0 °C |
26.2 ft-lb/in² @Temperature 73.4 °F |
ISO 180-1U |
Lanxess Pocan® ECO T 3240 000000 PBT + PET, 45% Glass Fiber PBT + PET, 45% glass fibers, injection molding, improved surface finish, contains 25% post-consumer recycled material, increased temperature peak loadInformation provided by LANXESS. |
|||
Izod Impact, Unnotched (ISO) | 55.0 kJ/m² @Temperature 23.0 °C |
26.2 ft-lb/in² @Temperature 73.4 °F |
ISO 180-1U |
Lanxess Pocan® T 7331 POS151 700226 PBT + PET, 30% Glass Fiber PBT + PET, 30% glass fibers, injection molding, improved surface finish, increased temperature peak load, UV stabilizedInformation provided by LANXESS. |
|||
Izod Impact, Unnotched (ISO) | 55.0 kJ/m² @Temperature -30.0 °C |
26.2 ft-lb/in² @Temperature -22.0 °F |
ISO 180-1U |
Lanxess Pocan® T 7391 POS151 900044 PBT + PET, 45% Glass Fiber PBT + PET, 45% glass fibers, injection molding, improved surface finish, increased temperature peak load UV stabilizedInformation provided by LANXESS. |
|||
Izod Impact, Unnotched (ISO) | 55.0 kJ/m² @Temperature 23.0 °C |
26.2 ft-lb/in² @Temperature 73.4 °F |
d.a.m.; ISO 180-1U |
Lanxess Durethan® A 30 S FN31 000000 Nylon 66, Flame Retardant PA 66, non-reinforced, injection molding, halogen-free flame retardant, improved flowabilityInformation provided by LANXESS. |
|||
Izod Impact, Unnotched (ISO) | 55.0 kJ/m² @Temperature -30.0 °C |
26.2 ft-lb/in² @Temperature -22.0 °F |
d.a.m.; ISO 180-1U |
Lanxess Durethan® A 30 S FN31 000000 Nylon 66, Flame Retardant PA 66, non-reinforced, injection molding, halogen-free flame retardant, improved flowabilityInformation provided by LANXESS. |
|||
Izod Impact, Unnotched (ISO) | 55.0 kJ/m² @Temperature 23.0 °C |
26.2 ft-lb/in² @Temperature 73.4 °F |
ISO 180-1U |
Lanxess Durethan® BKV 325 Z H2.0 901510 Nylon 6, 25% Glass Fibers PA 6, 25% glass fibers, blow molding, impact modified, heat-ageing stabilized |
|||
Izod Impact, Unnotched (ISO) | 55.0 kJ/m² @Temperature -30.0 °C |
26.2 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics Valox® VX5005 PBT (Europe-Africa-Middle East) VALOX VX5005 is a 5% glass fibre reinforced, impact modified PBT+PC blend with low warpage characteristics.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Unnotched (ISO) | 55.0 kJ/m² @Temperature 23.0 °C |
26.2 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1U |
Sax Polymers SAXALEN PPH319FX21 Polypropylene Homopolymer SAXALEN PPH319FX21 is a unfilled Polypropylene - Homopolymer intended for injection molding. It has flame retardant properties and suitable to produce thin-walled parts.Information provided by SAX P.. |
|||
Izod Impact, Unnotched (ISO) | 55.0 kJ/m² @Temperature 23.0 °C |
26.2 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics Noryl GTX GTX965 PPE+PA66 NORYL GTX965 is a mineral reinforced PPE/PA blend. It offers excellent surface appearance, processability and dimensional stability at elevated temperatures. The best molding condition for good appe.. |
|||
Izod Impact, Unnotched (ISO) | 55.0 kJ/m² @Temperature -30.0 °C |
26.2 ft-lb/in² @Temperature -22.0 °F |
ISO 180 |
Solvay Specialty Polymers Amodel® A-8940 HS Polyphthalamide (PPA), 40% Glass Fiber Amodel® A-8940 HS is a 40% glass-fiber-reinforced, heat-stabilized polyphthalamide (PPA) with a high heat deflection temperature and very high tensile strength. Excellent creep resistance and low.. |
|||
Izod Impact, Unnotched (ISO) | 55.0 kJ/m² @Temperature 23.0 °C |
26.2 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Thermocomp RF00AES PA 66 (Europe-Africa-Middle East) LNP THERMOCOMP* RF00AES is a compound based on PA66 resin containing Glass Fiber, Mold Release.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Unnotched (ISO) | 55.0 kJ/m² @Temperature 23.0 °C |
26.2 ft-lb/in² @Temperature 73.4 °F |
80x10x4; ISO 180/1U |
Eurostar Staramide RF00AES PA66/6, 50% Glass Filled, Injection Molded Staramide RF00AES is a 50% Glass Fiber Reinforced Polyamide 66/Polyamide 6 Injection Molding Resin (also known as Staramide 66 C 50V S3)Information provided by Eurostar. |
|||
Izod Impact, Unnotched (ISO) | 55.0 kJ/m² @Temperature -30.0 °C |
26.2 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1U |
Eurotec® Tecodur® PB70 GR25 NL100 XA20 PBT, 20% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural Information provided by Eurotec® |
|||
Izod Impact, Unnotched (ISO) | 55.0 kJ/m² @Temperature -30.0 °C |
26.2 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1U |
Eurotec® Tecodur® PB70 GR30 NL XA70 PBT, 30% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural Information provided by Eurotec® |
|||
Izod Impact, Unnotched (ISO) | 55.0 kJ/m² @Temperature -30.0 °C |
26.2 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1U |
Eurotec® Tecomid® NA40 GR20 NL HS PA6.6, 20% glass fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Izod Impact, Unnotched (ISO) | 55.0 kJ/m² @Temperature -30.0 °C |
26.2 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1U |
Eurotec® Tecodur® PB70 GR30 NL100 PBT, 20% glass fiber reinforced, natural Information provided by Eurotec® |
|||
Izod Impact, Unnotched (ISO) | 55.0 kJ/m² @Temperature -30.0 °C |
26.2 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1U |
Eurotec® Tecomid® MB40 GR20 NL PA6, 20% glass fiber reinforced, natural Information provided by Eurotec® |
|||
Izod Impact, Unnotched (ISO) | 55.0 kJ/m² @Temperature 23.0 °C |
26.2 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1U |
Sax Polymers SAXALEN PPC339T20 Polypropylene Copolymer, 20% Talc Filled SAXALEN PPC339T20 is a 20% mineral filled Polypropylene - Copolymer intended for injection molding with good flow properties und higher stiffness. The PP-Copolymer has low warpage behaviors and good.. |