Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 19.6 - 29.4 MPa @Temperature 1000 °C, Time 10800 sec |
2840 - 4270 psi @Temperature 1830 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories CT-140S Fireclay Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 19.6 - 29.4 MPa @Temperature 1000 °C, Time 10800 sec |
2840 - 4270 psi @Temperature 1830 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories HACT-165G High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 19.6 - 29.4 MPa @Temperature 110 °C, Time 86400 sec |
2840 - 4270 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories HACT-170 High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 19.6 - 29.4 MPa @Temperature 1000 °C, Time 10800 sec |
2840 - 4270 psi @Temperature 1830 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories HACT-170 High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 24.5 - 29.4 MPa @Temperature 110 °C, Time 86400 sec |
3560 - 4270 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories HACT-180G High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 19.6 - 29.4 MPa @Temperature 110 °C, Time 86400 sec |
2840 - 4270 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories HAPT-80S Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 19.6 - 29.4 MPa @Temperature 1350 °C, Time 10800 sec |
2840 - 4270 psi @Temperature 2460 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories PT-160 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 19.6 - 29.4 MPa @Temperature 1350 °C, Time 10800 sec |
2840 - 4270 psi @Temperature 2460 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories PT-165 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 19.6 - 29.4 MPa @Temperature 1500 °C, Time 10800 sec |
2840 - 4270 psi @Temperature 2730 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories PT-170 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 19.6 - 29.4 MPa @Temperature 1500 °C, Time 10800 sec |
2840 - 4270 psi @Temperature 2730 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories PTA-180 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 19.6 - 29.4 MPa @Temperature 1500 °C, Time 10800 sec |
2840 - 4270 psi @Temperature 2730 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories PTF-175 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 19.6 - 29.4 MPa @Temperature 350 °C, Time 86400 sec |
2840 - 4270 psi @Temperature 662 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories SCX-90IP Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 19.6 - 29.4 MPa @Temperature 1000 °C, Time 10800 sec |
2840 - 4270 psi @Temperature 1830 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories SCX-90IP Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 19.6 - 29.4 MPa @Temperature 1000 °C, Time 10800 sec |
2840 - 4270 psi @Temperature 1830 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories HACT-150S High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 19.6 - 29.4 MPa @Temperature 1350 °C, Time 10800 sec |
2840 - 4270 psi @Temperature 2460 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories HACT-150 High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 19.6 - 29.4 MPa @Temperature 1350 °C, Time 10800 sec |
2840 - 4270 psi @Temperature 2460 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories HACT-155 High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 19.6 - 29.4 MPa @Temperature 110 °C, Time 86400 sec |
2840 - 4270 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories HACT-155 High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 19.6 - 29.4 MPa @Temperature 1350 °C, Time 10800 sec |
2840 - 4270 psi @Temperature 2460 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories HACT-165 High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 19.6 - 29.4 MPa @Temperature 110 °C, Time 86400 sec |
2840 - 4270 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories HACT-165 High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |