Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | >= 24.5 MPa @Temperature 110 °C |
>= 3560 psi @Temperature 230 °F |
Cold Crushing |
Sharadaa Ceramics PHOSTCAST 80 XL Phosphate Bonded Castables Description: We hold expertise in manufacturing a range of Phosphate Bonded Castables, that find wide application in boilers, power plant, refineries, foundries, rolling mills, forging furnaces and .. |
|||
Compressive Strength | 24.5 MPa @Time 86400 sec |
3560 psi @Time 24.0 hour |
Cold Crushing |
Sharadaa Ceramics REFCAST 80 High Alumina Castables Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr.. |
|||
Compressive Strength | 24.5 MPa @Temperature 110 °C |
3560 psi @Temperature 230 °F |
Cold Crushing |
Sharadaa Ceramics REFCAST Dense Castables Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |
|||
Compressive Strength | 24.5 MPa @Time 86400 sec |
3560 psi @Time 24.0 hour |
Cold Crushing |
Sharadaa Ceramics REFCAST HA High Alumina Castables Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr.. |
|||
Compressive Strength | 24.5 MPa @Time 86400 sec |
3560 psi @Time 24.0 hour |
Cold Crushing |
Sharadaa Ceramics REFCAST K SUPER High Alumina Castables Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr.. |
|||
Compressive Strength | 24.5 MPa @Time 86400 sec |
3560 psi @Time 24.0 hour |
Cold Crushing |
Sharadaa Ceramics REFCAST LC60ABR Low Cement Castables Description: We bring to our clients a range of Low Cement Castables, that are available in varied alumina content and service range. Designed for abrasion resistance application, these are widely u.. |
|||
Compressive Strength | 24.5 MPa @Time 86400 sec |
3560 psi @Time 24.0 hour |
Cold Crushing |
Sharadaa Ceramics REFCAST LC70 Low Cement Castables Description: We bring to our clients a range of Low Cement Castables, that are available in varied alumina content and service range. Designed for abrasion resistance application, these are widely u.. |
|||
Compressive Strength | 24.5 MPa @Time 86400 sec |
3560 psi @Time 24.0 hour |
Cold Crushing |
Sharadaa Ceramics REFCAST LC80 Low Cement Castables Description: We bring to our clients a range of Low Cement Castables, that are available in varied alumina content and service range. Designed for abrasion resistance application, these are widely u.. |
|||
Compressive Strength | 24.5 MPa @Time 86400 sec |
3560 psi @Time 24.0 hour |
Cold Crushing |
Sharadaa Ceramics REFCAST LC90 Low Cement Castables Description: We bring to our clients a range of Low Cement Castables, that are available in varied alumina content and service range. Designed for abrasion resistance application, these are widely u.. |
|||
Compressive Strength | 24.5 MPa @Temperature 110 °C |
3560 psi @Temperature 230 °F |
Cold Crushing |
Sharadaa Ceramics REFCAST LT Dense Castables Description: We offer a range of Dense Castables that are conventional castable and extensively used in boiler work, general furnace and burner blocks. Made as per international standards, our range.. |
|||
Compressive Strength | 24.5 MPa @Temperature 1100 °C |
3560 psi @Temperature 2010 °F |
Cold Crushing |
Sharadaa Ceramics REFCAST NORMAL Dense Castables Description: We offer a range of Dense Castables that are conventional castable and extensively used in boiler work, general furnace and burner blocks. Made as per international standards, our range.. |
|||
Compressive Strength | 24.5 MPa @Temperature 1100 °C |
3560 psi @Temperature 2010 °F |
Cold Crushing |
Sharadaa Ceramics REFCAST SPECIAL Dense Castables Description: We offer a range of Dense Castables that are conventional castable and extensively used in boiler work, general furnace and burner blocks. Made as per international standards, our range.. |
|||
Compressive Strength | >= 24.5 MPa @Temperature 800 °C, Time 10800 sec |
>= 3560 psi @Temperature 1470 °F, Time 3.00 hour |
Cold Crushing, Specification, After firing @ 800°C |
Sharadaa Ceramics REFPLAST 60 60% Alumina Plastic Nature of bond: Chemical-CeramicInstallation: Pneumatic rammingInformation provided by Sharadaa Ceramics Pvt. Ltd. |
|||
Compressive Strength | 24.5 MPa @Temperature 1400 °C |
3560 psi @Temperature 2550 °F |
Cold Crushing |
Sharadaa Ceramics Sharada AIO-SiC-C Gel Bonded Castables Mullite Bonded Free Flowing Cement Free Versatile Castable SystemProduct Characteristics: High Mullitisation, Free from Low Temperature eutectics, Non wetting to molten metals Ferrous/Non Ferrous, E.. |
|||
Compressive Strength | 24.5 MPa @Time 86400 sec |
3560 psi @Time 24.0 hour |
Cold Crushing |
Sharadaa Ceramics ZAP 004 Smart Cast Application Special Properties: Thermal Shock, Abrasion, Alkali ResistanceIndustry: SteelApplication: Lances, Launders, Riser TubesInformation provided by Sharadaa Ceramics Pvt. Ltd. |
|||
Compressive Strength | 24.5 MPa @Temperature 1100 °C |
3560 psi @Temperature 2010 °F |
Cold Crushing |
Sharadaa Ceramics REFCAST C High Alumina Castables Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr.. |
|||
Compressive Strength | 24.5 MPa @Temperature 110 °C, Time 86400 sec |
3560 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories APC-100G Acid-proof Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 24.5 MPa @Temperature 500 °C, Time 10800 sec |
3560 psi @Temperature 932 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories APC-120G Acid-proof Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 24.5 MPa @Temperature 500 °C, Time 10800 sec |
3560 psi @Temperature 932 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories APC-80 Acid-proof Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 24.5 MPa @Temperature 1000 °C, Time 10800 sec |
3560 psi @Temperature 1830 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories BCT-145 Acid-proof Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 24.5 - 34.3 MPa @Temperature 1350 °C, Time 10800 sec |
3560 - 4980 psi @Temperature 2460 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories CT-140S Fireclay Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 24.5 - 34.3 MPa @Temperature 1350 °C, Time 10800 sec |
3560 - 4980 psi @Temperature 2460 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories HACT-170 High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 24.5 - 29.4 MPa @Temperature 110 °C, Time 86400 sec |
3560 - 4270 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories HACT-180G High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 24.5 - 34.3 MPa @Temperature 1500 °C, Time 10800 sec |
3560 - 4980 psi @Temperature 2730 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories PT-160 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 24.5 - 34.3 MPa @Temperature 1500 °C, Time 10800 sec |
3560 - 4980 psi @Temperature 2730 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories PT-165 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 24.5 - 34.3 MPa @Temperature 1350 °C, Time 10800 sec |
3560 - 4980 psi @Temperature 2460 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories PTA-180 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 24.5 - 34.3 MPa @Temperature 1350 °C, Time 10800 sec |
3560 - 4980 psi @Temperature 2460 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories PTF-175 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 24.5 MPa @Temperature 110 °C, Time 86400 sec |
3560 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories FM Blast Furnace Runner Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 24.5 - 44.1 MPa @Temperature 1500 °C, Time 10800 sec |
3560 - 6400 psi @Temperature 2730 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories TPA-175 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 24.5 MPa @Temperature 1500 °C, Time 10800 sec |
3560 psi @Temperature 2730 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories TD-R75 Monolithic Refractories for Ladle and Tundish Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |