Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 1.31 kN/m | 7.50 pli | after solder float; IPC-TM-650.2.4.8 |
Park Electrochemical Nelco® N4000-7 SI® FR-4 Epoxy Laminate and Prepreg The Nelco® N4000-7 low-CTE epoxy laminate and prepreg system is a cost-effective solution for use in a broad range of multilayer PCB designs requiring low Z-axis expansion, excellent thermal stabil.. |
|||
Peel Strength | 1.31 kN/m | 7.50 pli | after solder float; IPC-TM-650.2.4.8 |
Park Electrochemical Nelco® N4000-13 BC® Buried Capacitance™, High-Speed Multifunctional Epoxy Laminate and Prepreg The Nelco N4000-13 series is an enhanced epoxy resin system engineered to provide both outstanding thermal and high signal speed / low signal loss properties. The Nelco N4000-13 BC® is offered as a.. |
|||
Peel Strength | 1.31 kN/m | 7.50 pli | after solder float; IPC-TM-650.2.4.8 |
Park Electrochemical Nelco® N4000-13 EP™ BC® Buried Capacitance™, High-Speed Multifunctional Epoxy Laminate and Prepreg Nelco N4000-13 EP™ is an enhanced epoxy resin system engineered for today’s leadfree requirements where multiple solder reflow at temperatures approaching 260ºC are required. N4000-13 EP provides.. |
|||
Peel Strength | 1.31 kN/m | 7.50 pli | after solder float; IPC-TM-650.2.4.8 |
Park Electrochemical Nelco® N4000-13 High-Speed Multifunctional Epoxy Laminate and Prepreg The Nelco® N4000-13 series is an enhanced epoxy resin system engineered to provide both outstanding thermal and high signal speed / low signal loss properties. N4000-13 SI® is excellent for applic.. |
|||
Peel Strength | 1.31 kN/m | 7.50 pli | after solder float; IPC-TM-650.2.4.8 |
Park Electrochemical Nelco® N4000-13 SI® High-Speed Multifunctional Epoxy Laminate and Prepreg The Nelco® N4000-13 series is an enhanced epoxy resin system engineered to provide both outstanding thermal and high signal speed / low signal loss properties. N4000-13 SI® is excellent for applic.. |
|||
Peel Strength | 1.31 kN/m | 7.50 pli | after solder float; IPC-TM-650.2.4.8 |
Park Electrochemical Nelco® N4000-7 FR-4 Epoxy Laminate and Prepreg The Nelco® N4000-7 low-CTE epoxy laminate and prepreg system is a cost-effective solution for use in a broad range of multilayer PCB designs requiring low Z-axis expansion, excellent thermal stabil.. |
|||
Peel Strength | 1.31 kN/m | 7.50 pli | after solder float; IPC-TM-650.2.4.8 |
Park Electrochemical Nelco® N4350-13 RF Microwave Performance, Modified Epoxy The Nelco N4350-13 RF and N4380-13 RF series are enhanced epoxy resin systems specifically engineered to provide a unique solution for design applications that demand outstanding thermal properties,.. |
|||
Peel Strength | 1.31 kN/m | 7.50 pli | after solder float; IPC-TM-650.2.4.8 |
Park Electrochemical Nelco® N4380-13 RF Microwave Performance, Modified Epoxy The Nelco N4350-13 RF and N4380-13 RF series are enhanced epoxy resin systems specifically engineered to provide a unique solution for design applications that demand outstanding thermal properties,.. |
|||
Peel Strength | 1.31 kN/m | 7.50 pli | after solder float; IPC-TM-650.2.4.8 |
Park Electrochemical Nelco® N7000-1 Polyimide Laminate and Prepreg The Nelco N7000-1 series of polyimide laminate and prepreg has alow Z-axis expansion and high Tg offering PCB manufacturers consistent board performance and reliability. N7000-1 is a good choice for.. |
|||
Peel Strength | 1.31 kN/m | 7.50 pli | after solder float; IPC-TM-650.2.4.8 |
Park Electrochemical Nelco® N7000-2 HT/N7000-3 Toughened Polyimide Laminate and Prepreg The Nelco N7000-2 HT laminate and N7000-3 prepreg are a series of toughened polyimide materials for use in high-reliability multilayers. This combined resin system provides excellent thermal perform.. |
|||
Peel Strength | 1.31 kN/m | 7.50 pli | 1 oz. Cu, at elevated temperature; IPC-TM-650.2.4.8.2a |
Park Electrochemical Nelco® N8000 Cyanate Ester Epoxy Laminate and Prepreg The Nelco N8000 is a high-Tg cyanate ester laminate and prepreg system that provides superior performance and product integrity and is ideal for board designs with higher layer counts, finer lines a.. |
|||
Peel Strength | 1.31 kN/m | 7.50 pli | 24 hr, Linered side-PVC; ASTM D3330 |
3M 2205 Thin Flexographic Plate Mounting Tape 3M™ Thin Flexographic Mounting Tape 2205 is a double coated film tape constructed of a polyester film carrier with differential adhesives specifically designed for the corrugated printing business .. |
|||
Peel Strength | 1.31 kN/m | 7.50 pli | to Steel; ASTM D3330 |
3M 6910 Cloth Gaffers Tape 3M™ Cloth Gaffers Tape 6910 is coated with a rubber adhesive for use in the entertainment industry as “gaffers” tape where light reflection is a concernInformation provided by 3M |
|||
Peel Strength | 1.31 kN/m | 7.50 pli | (S1 to S2) Bond Strength; Arlon SQA-TMS-011 |
Arlon 48106R008 0.008" (0.203 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 1080 FiberglassSide 2: Uncured Silicone RubberInterleave: Polyethylene This data represents typical values for the production mater.. |
|||
Peel Strength | 1.31 kN/m | 7.50 pli | Bond Strength; Arlon SQA-TMS-011 |
Arlon 51866R015 0.0170" Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PEThis data represents typical values for the production material .. |
|||
Peel Strength | 1.31 kN/m | 7.50 pli | Epoxy, 180° peel, 72°F, (72 hr. dwell); ASTM D3330 |
3M 9485PC Adhesive Transfer Tapes with Adhesive 350 These 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 350 are a modified acrylic adhesive ideal for very high-bond strength to many surfaces. They have excellent chemical resistance and bold strengt.. |
|||
Peel Strength | 1.31 kN/m | 7.50 pli | Epoxy, 180° peel, 72°F, (72 hr. dwell); ASTM D3330 |
3M 9675 Adhesive Transfer Tapes with Adhesive 350 These 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 350 are a modified acrylic adhesive ideal for very high-bond strength to many surfaces. They have excellent chemical resistance and bold strengt.. |
|||
Peel Strength | 1.31 kN/m | 7.50 pli | Bond Strength; Arlon SQA-TMS-011 |
Arlon 55636R025 0.025" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil PESide 2: Uncured Silicone RubberSubstrate: Style 162 FiberglassSide 1: Cured Silicone RubberThis data represents typical values for the production material .. |
|||
Peel Strength | 1.31 kN/m | 7.50 pli | Bond Strength (S1 to S1); ASTM D624 |
Arlon 55869R028 0.0295" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil PELayer 2: Uncured Silicone RubberLayer 1: Cured Silicone RubberSubstrate: Style 162 FiberglassThis data represents typical values for the production materia.. |
|||
Peel Strength | 1.31 kN/m | 7.50 pli | Bond Strength; Arlon SQA -TMS-011 |
Arlon 55638R025 0.025" (0.635 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneSide 2: Uncured Silicone Rubber Substrate: Style 162 Fiberglass Side 1: Cured Silicone Rubber Product Use: Flexible heater SubstrateAppearance: Red silic.. |
|||
Peel Strength | 1.31 kN/m | 7.50 pli | Epoxy, 180° peel, 72°F, (72 hr. dwell); ASTM D3330 |
3M 9445 Adhesive Transfer Tapes with Adhesive 350 These 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 350 are a modified acrylic adhesive ideal for very high-bond strength to many surfaces. They have excellent chemical resistance and bold strengt.. |
|||
Peel Strength | 1.31 kN/m | 7.50 pli | Polycarbonate, 90° peel, 2 mil Al foil backing, 72 hr RT, Faceside; ASTM D3330 |
3M 9475LE High Strength Double Coated Tape with Adhesive 300LSE 3M™ Double Coated Tapes with 3M™ Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints. The acryli.. |
|||
Peel Strength | 1.31 kN/m | 7.50 pli | Polycarbonate, 90° peel, 2 mil Al foil backing, 72 hr RT, Backside; ASTM D3330 |
3M 9475LE High Strength Double Coated Tape with Adhesive 300LSE 3M™ Double Coated Tapes with 3M™ Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints. The acryli.. |
|||
Peel Strength | 1.31 kN/m | 7.50 pli | Polycarbonate, 90° peel, 2 mil Al foil backing, 72 hr RT, Faceside; ASTM D3330 |
3M 9475LEB High Strength Double Coated Tape with Adhesive 300LSE 3M™ Double Coated Tapes with 3M™ Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints. The acryli.. |
|||
Peel Strength | 1.31 kN/m | 7.50 pli | Epoxy, 180° peel, 72°F, (72 hr. dwell); ASTM D3330 |
3M 9485EK Adhesive Transfer Tapes with Adhesive 350 These 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 350 are a modified acrylic adhesive ideal for very high-bond strength to many surfaces. They have excellent chemical resistance and bold strengt.. |
|||
Peel Strength | 1.31 kN/m | 7.50 pli | Polypropylene, 180°, 2 mil al foil, 72 hr RT, Backside; ASTM D3330 |
3M 9626 Adhesive Transfer Tape with Quick Bonding Adhesive 360 3M™ Adhesive Transfer Tapes with 3M™ Quick Bonding Adhesive 360 provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated pai.. |
|||
Peel Strength | 1.31 kN/m | 7.50 pli | Polypropylene, 180°, 2 mil al foil, 15 min RT, Faceside; ASTM D3330 |
3M 9629B Double Coated Tape with Quick Bonding Adhesive 360 3M™ Double Coated Tapes with 3M™ Quick Bonding Adhesive 360 provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints... |
|||
Peel Strength | 1.31 kN/m | 7.50 pli | Polypropylene, 180°, 2 mil al foil, 15 min RT, Backside; ASTM D3330 |
3M 9629FL Double Coated Tape with Quick Bonding Adhesive 360 3M™ Double Coated Tapes with 3M™ Quick Bonding Adhesive 360 provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints... |
|||
Peel Strength | 1.31 kN/m | 7.50 pli | Polypropylene, 180°, 2 mil al foil, 15 min RT, Backside; ASTM D3330 |
3M 9629PC Double Coated Tape with Quick Bonding Adhesive 360 3M™ Double Coated Tapes with 3M™ Quick Bonding Adhesive 360 provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints... |
|||
Peel Strength | 1.31 kN/m | 7.50 pli | To Copper (1 oz./35 micron); After Process Solutions; IPC TM-650 2.4.8 |
Arlon 33N Polyimide Laminate and Prepreg High reliability and high temperature material33N is a flame retardant polyimide laminate and prepreg system where the excellent high performance properties of polyimide need to be combined with fla.. |