Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M 9675 Adhesive Transfer Tapes with Adhesive 350

Category Polymer , Adhesive
Manufacturer 3M
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 9675 Adhesive Transfer Tapes with Adhesive 350.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
These 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 350 are a modified acrylic adhesive ideal for very high-bond strength to many surfaces. They have excellent chemical resistance and bold strength even at elevated temperatures. These tapes are offered with a fiber reinforced adhesive which is important for roll stability in narrow widths. Tapes using adhesive 350 are designed for temperature exposure to 450°F (232°C) for short periods of time and up to 300°F (149°C) over long time frames. This adhesive is a good choice for applications which require adhesion to Low Surface Energy plastics, powder coatings and oily metals.Information provided by 3M
Physical Properties Metric English Comments
Thickness 127 microns
5.00 mil
Mechanical Properties Metric English Comments
Peel Strength 0.38347 kN/m
2.1875 pli
H.D. Polyethylene, 180° peel, 72°F, (72 hr. dwell); ASTM D3330
0.438 kN/m
2.50 pli
L.D. Polyethylene, 180° peel, 72°F, (72 hr. dwell); ASTM D3330
0.877 kN/m
5.00 pli
Polypropylene, 180° peel, 72°F, (72 hr. dwell); ASTM D3330
0.93128 kN/m
5.3125 pli
ABS, 180° peel, 72°F, (72 hr. dwell); ASTM D3330
0.9861 kN/m
5.625 pli
Rigid PVC, 180° peel, 72°F, (72 hr. dwell); ASTM D3330
1.05 kN/m
6.00 pli
Aluminum, 180° peel, 72°F, (72 hr. dwell); ASTM D3330
1.31 kN/m
7.50 pli
Epoxy, 180° peel, 72°F, (72 hr. dwell); ASTM D3330
1.3695 kN/m
7.8125 pli
Acrylic, 180° peel, 72°F, (72 hr. dwell); ASTM D3330
1.5887 kN/m
9.0625 pli
Painted Metal, 180° peel, 72°F, (72 hr. dwell); ASTM D3330
1.5887 kN/m
9.0625 pli
Glass, 180° peel, 72°F, (72 hr. dwell); ASTM D3330
1.5887 kN/m
9.0625 pli
Polycarbonate, 180° peel, 72°F, (72 hr. dwell); ASTM D3330
1.643 kN/m
9.375 pli
Stainless Steel, 180° peel, 72°F, (72 hr. dwell); ASTM D3330
Thermal Properties Metric English Comments
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Liner 83# Polycoated Kraft lay flat - 6.2 mils thick