Material Notes:
3M™ Double Coated Tapes with 3M™ Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints. The acrylic adhesive also provides excellent adhesion to surfaces contaminated lightly with oil typically used with machine parts.Information provided by 3M
Physical Properties Metric English Comments
Thickness 12.7 microns
0.500 mil
Carrier
50.8 microns
2.00 mil
Faceside Adhesive
50.8 microns
2.00 mil
Backside Adhesive
114 microns
4.50 mil
Total Thickness
157 microns
6.20 mil
Caliper
Mechanical Properties Metric English Comments
Peel Strength 0.49303 kN/m
2.8125 pli
Stainless Steel, 180° peel, 2 mil Al foil backing, 15 min RT, Faceside; ASTM D3330
0.657 kN/m
3.75 pli
Glass, 90° peel, 2 mil Al foil backing, 72 hr RT, Faceside; ASTM D3330
0.657 kN/m
3.75 pli
Polypropylene, 90° peel, 2 mil Al foil backing, 72 hr RT, Faceside; ASTM D3330
0.7669 kN/m
4.375 pli
Stainless Steel, 180° peel, 2 mil Al foil backing, 72 hr RT, Faceside; ASTM D3330
0.7669 kN/m
4.375 pli
Polypropylene, 90° peel, 2 mil Al foil backing, 72 hr RT, Backside; ASTM D3330
0.7669 kN/m
4.375 pli
Stainless Steel, 180°, 2 mil polyester as backing, 72 hr RT, Faceside; ASTM D3330
0.7669 kN/m
4.375 pli
Stainless Steel, 180° peel, 2 mil Al foil backing, 15 min RT, Backside; ASTM D3330
0.82172 kN/m
4.6875 pli
Glass, 90° peel, 2 mil Al foil backing, 72 hr RT, Backside; ASTM D3330
0.877 kN/m
5.00 pli
Stainless Steel, 180°, 2 mil polyester as backing, 72 hr RT, Backside; ASTM D3330
0.93128 kN/m
5.3125 pli
ABS, 90° peel, 2 mil Al foil backing, 72 hr RT, Faceside; ASTM D3330
0.9861 kN/m
5.625 pli
Stainless Steel, 180° peel, 2 mil Al foil backing, 72 hr RT, Backside; ASTM D3330
0.9861 kN/m
5.625 pli
Stainless Steel, 180° peel, 2 mil Al foil backing, 72 hr 70°C, Faceside; ASTM D3330
0.9861 kN/m
5.625 pli
ABS, 90° peel, 2 mil Al foil backing, 72 hr RT, Backside; ASTM D3330
1.1504 kN/m
6.5625 pli
Stainless Steel, 180° peel, 2 mil Al foil backing, 72 hr 70°C, Backside; ASTM D3330
1.31 kN/m
7.50 pli
Polycarbonate, 90° peel, 2 mil Al foil backing, 72 hr RT, Faceside; ASTM D3330
1.31 kN/m
7.50 pli
Polycarbonate, 90° peel, 2 mil Al foil backing, 72 hr RT, Backside; ASTM D3330
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 93.0 °C
199 °F
Long term
149 °C
300 °F
Short term
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Liner #83 Polycoated Kraft