Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Park Electrochemical Nelco® N4000-13 BC® Buried Capacitance™, High-Speed Multifunctional Epoxy Laminate and Prepreg

Category Polymer , Thermoset , Epoxy
Manufacturer Park Electrochemical Corp.
Trade Name Nelco®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Park Electrochemical Nelco® N4000-13 BC® Buried Capacitance™, High-Speed Multifunctional Epoxy Laminate and Prepreg.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
The Nelco N4000-13 series is an enhanced epoxy resin system engineered to provide both outstanding thermal and high signal speed / low signal loss properties. The Nelco N4000-13 BC® is offered as a buried capacitance solution, offering a greater degree of design freedom for smaller, more reliable assemblies.Key Features and Benefits:Tg >210°C, outstanding thermal, electrical and signal loss propertiesCAF ResistantBuried Capacitance SolutionProprietary advanced resin technologyHigh-Tg FR-4 processingAvailable in a variety of constructionsApplications/Qualifications:High Density InterconnectsFine-Line MultilayersBackplanesSurface-Mount MultilayersBGA MultilayersMCM-LsCSP AttachmentWireless Communications InfrastructureHigh Speed ServicesHigh Speed Storage NetworksInternet Switching / Routing SystemsInformation provided by Park Electrochemical Corp.
Physical Properties Metric English Comments
Density 1.77 g/cc
0.0639 lb/in³
50% Resin Content; Internal Method
Water Absorption 0.10 %
0.10 %
IPC-TM-650.2.6.2.1
Mechanical Properties Metric English Comments
Peel Strength 1.31 kN/m
7.50 pli
after solder float; IPC-TM-650.2.4.8
1.42 kN/m
8.10 pli
at elevated temperature; IPC-TM-650.2.4.8.2a
1.58 kN/m
9.00 pli
after exposure to process solutions; IPC-TM-650.2.4.8
Thermal Properties Metric English Comments
Specific Heat Capacity 1.21 J/g-°C
0.290 BTU/lb-°F
ASTM E1461
Thermal Conductivity 0.350 W/m-K
2.43 BTU-in/hr-ft²-°F
ASTM E1461
Glass Transition Temp, Tg 200 °C
392 °F
TMA; IPC-TM-650.2.4.24c
210 °C
410 °F
DSC; IPC-TM-650.2.4.25c
240 °C
464 °F
DMA (Tan d Peak); IPC-TM-650.2.4.24.3
Decomposition Temperature 365 °C
689 °F
5% weight loss; TGA; IPC-TM-650.2.4.24.6
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Dielectric Constant 3.2

@Frequency 1.00e+10 Hz
3.2

@Frequency 1.00e+10 Hz
Stripline; IPC-TM-650.2.5.5.5
3.3

@Frequency 1.00e+9 Hz
3.3

@Frequency 1.00e+9 Hz
RF Impedance; IPC-TM-650.2.5.5.9
3.3

@Frequency 2.50e+9 Hz
3.3

@Frequency 2.50e+9 Hz
Split Post Cavity
Dielectric Strength 47.2 kV/mm
1200 kV/in
IPC-TM-650.2.5.6.2
Dissipation Factor 0.0080

@Frequency 2.50e+9 Hz
0.0080

@Frequency 2.50e+9 Hz
Split Post Cavity
0.0090

@Frequency 1.00e+10 Hz
0.0090

@Frequency 1.00e+10 Hz
Stripline; IPC-TM-650.2.5.5.5
Descriptive Properties Value Comments
Methylene Chloride Resistance (% Weight Change) 0.7
IPC-TM-650.2.3.4.3
T260 (minutes) >30
IPC-TM-650.2.4.24.1