3M 9629B Double Coated Tape with Quick Bonding Adhesive 360

Category Polymer , Adhesive
Manufacturer 3M
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF 3M 9629B Double Coated Tape with Quick Bonding Adhesive 360.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
3M™ Double Coated Tapes with 3M™ Quick Bonding Adhesive 360 provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints.Information provided by 3M
Physical Properties Metric English Comments
Thickness 12.7 microns
0.500 mil
Carrier
44.5 microns
1.75 mil
Faceside Adhesive
44.5 microns
1.75 mil
Backside Adhesive
81.3 microns
3.20 mil
Liner Caliper
102 microns
4.00 mil
Total Thickness
Mechanical Properties Metric English Comments
Peel Strength 0.71216 kN/m
4.0625 pli
LDPE, 180°, 2 mil al foil, 72 hr RT, Faceside; ASTM D3330
0.71216 kN/m
4.0625 pli
LDPE, 180°, 2 mil al foil, 72 hr RT, Backside; ASTM D3330
0.71216 kN/m
4.0625 pli
HDPE, 180°, 2 mil al foil, 72 hr RT, Backside; ASTM D3330
0.82172 kN/m
4.6875 pli
HDPE, 180°, 2 mil al foil, 72 hr RT, Faceside; ASTM D3330
1.10 kN/m
6.25 pli
Polypropylene, 180°, 2 mil al foil, 30 sec RT, Faceside; ASTM D3330
1.10 kN/m
6.25 pli
Polypropylene, 180°, 2 mil al foil, 30 sec RT, Backside; ASTM D3330
1.31 kN/m
7.50 pli
Polypropylene, 180°, 2 mil al foil, 15 min RT, Faceside; ASTM D3330
1.31 kN/m
7.50 pli
Polypropylene, 180°, 2 mil al foil, 15 min RT, Backside; ASTM D3330
1.643 kN/m
9.375 pli
Polypropylene, 180°, 2 mil al foil, 72 hr RT, Faceside; ASTM D3330
1.643 kN/m
9.375 pli
Polypropylene, 180°, 2 mil al foil, 72 hr RT, Backside; ASTM D3330
1.643 kN/m
9.375 pli
ABS, 180°, 2 mil al foil, 72 hr RT, Backside; ASTM D3330
1.75 kN/m
10.0 pli
ABS, 180°, 2 mil al foil, 72 hr RT, Faceside; ASTM D3330
1.75 kN/m
10.0 pli
Polycarbonate, 180°, 2 mil al foil, 72 hr RT, Backside; ASTM D3330
1.75 kN/m
10.0 pli
Stainless Steel 180°, 2 mil al foil, 72 hr RT, Backside; ASTM D3330
1.8626 kN/m
10.625 pli
Polycarbonate, 180°, 2 mil al foil, 72 hr RT, Faceside; ASTM D3330
1.8626 kN/m
10.625 pli
Stainless Steel, 180°, 2 mil al foil, 72 hr RT, Faceside; ASTM D3330
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 93.0 °C
199 °F
Long term
177 °C
351 °F
Short term
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Liner Natural, 60# Glassine
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved