Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 131 MPa | 19000 psi | ASTM D790 |
Chevron Phillips Ryton® R10 5004A PPS Polyphenylene Sulfide
(discontinued **) Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol.. |
|||
Flexural Yield Strength | 131 MPa | 19000 psi | ASTM D790 |
Covestro Petlon® PC/PET 36A 620UV Yellow Semi-Crystalline PET, 10% Glass Fiber
(discontinued **) Characteristics: Good Thermal and Dimensional Stability, Good Chemical ResistanceApplications: Automotive Panels, Electronic Housings, Pump HousingsProcessing: Injection Molding (Melt Temperature: 5.. |
|||
Flexural Yield Strength | 131 MPa | 19000 psi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON Noryl_HMC1508 PPE+HIPS (Europe-Africa-Middle East) LNP* Stat-kon* Noryl_HMC1508 compound is a static dissipative NORYL resin. |
|||
Flexural Yield Strength | 131 MPa | 19000 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Xenoy® 1760E PBT+PC 11% Glass Reinforced alloy. Impact/chemical resistant. Excellent physical property retention in automotive exteriors. High flow version of Xenoy 1760 resin. |
|||
Flexural Yield Strength | 131 MPa | 19000 psi | ASTM D790 |
Techmer ES HiFill® POM CO GF10 CC 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforced, 10% Filler by WeightFeatures: Copolymer and Chemically CoupledInformation provided by TP Composites, Inc. |
|||
Flexural Yield Strength | 131 MPa | 19000 psi | ASTM D790 |
Sumitomo Bakelite North America 3-2-530 Short-Glass Reinforced Diallyl Phthalate Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Information provided by Sumitomo Bak North A.. |
|||
Flexural Yield Strength | 131 MPa | 19000 psi | ASTM D790 |
Sumitomo Bakelite North America RX® 3-2-520F-P Short-Glass Reinforced Diallyl Phthalate Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type SI.. |
|||
Flexural Yield Strength | 131 MPa | 19000 psi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL GFN2 PPE+HIPS (Asia Pacific) PPE+PS blend. 20% Glass reinforced. FDA compliance (restrictions apply). Low water absorption. Hydrolytic stability. Dimensional stability. Suitable for fluid engineering applications including pump.. |
|||
Flexural Yield Strength | 131 MPa | 19000 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL LTA1350 PPE+PS Noryl* LTA1350 is an unfilled, injection moldable grade. Designed for improved long term heat aging, this resin also uses non-chlorinated, non-brominated FR additives to achieve a V0 UL94 rating. No.. |
|||
Flexural Yield Strength | 131 MPa | 19000 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL LTA1350 PPE+PS (Asia Pacific) Noryl* LTA1350 is an unfilled, injection moldable grade. Designed for improved long term heat aging, this resin also uses non-chlorinated, non-brominated FR additives to achieve a V0 UL94 rating. No.. |
|||
Flexural Yield Strength | 131 MPa | 19000 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL LTA5020 PPE+PS Noryl* LTA5020 is an unfilled, injection moldable grade. Designed for improved long term heat aging, this resin also uses non-chlorinated, non-brominated FR additives to achieve a V0 UL94 rating. No.. |
|||
Flexural Yield Strength | 131 MPa | 19000 psi | ASTM D790 |
Sumitomo Bakelite North America 2-530 Short-Glass Reinforced Diallyl Phthalate Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Information provided by Sumitomo Bak North Am.. |
|||
Flexural Yield Strength | 131 MPa | 19000 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL GFN1410V PPE+PS (Europe-Africa-Middle East) Noryl* GFN1410V resin is a blend of polyphenylene ether (PPE) and polystyrene (PS) resin that contains 10 % glass reinforcement. The resin is suitable for injection molding. Noryl GFN1410V resin has.. |
|||
Flexural Yield Strength | 131 MPa | 19000 psi | ASTM D790 |
Clariant Renol 66B40 Nylon 66, 40% Glass Bead Filled Data provided by Clariant Masterbatches |
|||
Flexural Yield Strength | 131 MPa | 19000 psi | |
Abatron AboCast/AboCure 8109-6 High heat resistance. Easy to use.Processing: 100/90 pbw; Potlife: 15-20 days/20°C (68°F), 7-10 h/120°C (250°F); mix at RT; cures in: 3 h/100°C (212°F) + 3 h/190°C (375°F) postcure.Applicat.. |
|||
Flexural Yield Strength | 131 MPa | 19000 psi | ASTM D790 |
Chem Polymer Formax 630 G Acetal, 30% Glass Fiber Reinforced A copolymer acetal reinforced with 30% glass fiber for use in applications requiring great strength and rigidity.Data provided by the manufacturer, Chem Polymer. |
|||
Flexural Yield Strength | 131 - 275 MPa | 19000 - 39900 psi | Average value: 160 MPa Grade Count:12 |
Overview of materials for Polyphthalamide (PPA), 10% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% are .. |
|||
Flexural Yield Strength | 131 MPa | 19000 psi | ASTM D790 |
PlastxWorld CEVIAN® B2703 15% GF PBT/ABS Alloy Glass fiber reinforced PBT/ABS alloy.Information provided by PlastxWorld Inc. |
|||
Flexural Yield Strength | 131 MPa | 19000 psi | ASTM D790 |
Custom Resins Norpex® GF3 PPE (Polyphenylene Ether), 30% Glass Filled
(discontinued **) Properties for dry as molded samples.Data provided by the manufacturer |
|||
Flexural Yield Strength | 131 MPa | 19000 psi | ASTM D790 |
Devcon Zip Patch™ Epoxy Emergency Repair ProductsComments: High-technology, adhesive-impregnated, putty patching system that cures at room temperature. Hardens to a tough, durable, waterproof finish in minutes. Easy-to-u.. |
|||
Flexural Yield Strength | 131 - 348 MPa | 19000 - 50500 psi | Average value: 246 MPa Grade Count:24 |
Overview of materials for Polyphthalamide (PPA), Glass/PTFE This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide + Glass/PTFE". Each property range of values reported is minimum and maximum values of a.. |