Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Techmer ES HiFill® POM CO GF10 CC 10% Glass Filled

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Copolymer, 10% Glass Fiber Reinforced
Manufacturer Techmer ES
Trade Name HiFill®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES HiFill® POM CO GF10 CC 10% Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforced, 10% Filler by WeightFeatures: Copolymer and Chemically CoupledInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.47 g/cc
0.0531 lb/in³
ASTM D792
Water Absorption 0.20 %

@Time 86400 sec
0.20 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0090 cm/cm

@Thickness 3.17 mm
0.0090 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 82
82
ASTM D785
Tensile Strength, Yield 89.6 MPa
13000 psi
ASTM D638
Elongation at Break 2.0 %
2.0 %
ASTM D638
Flexural Yield Strength 131 MPa
19000 psi
ASTM D790
Flexural Modulus 3.79 GPa
550 ksi
ASTM D790
Izod Impact, Notched 0.801 J/cm

@Thickness 3.17 mm
1.50 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 46.8 µm/m-°C
26.0 µin/in-°F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 152 °C
305 °F
Unannealed; ASTM D648
Flammability, UL94 HB
HB