Material Notes:
High heat resistance. Easy to use.Processing: 100/90 pbw; Potlife: 15-20 days/20°C (68°F), 7-10 h/120°C (250°F); mix at RT; cures in: 3 h/100°C (212°F) + 3 h/190°C (375°F) postcure.Applications: Castings and laminates for high temperature applications.
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
Water Absorption 0.15 - 0.20 %
0.15 - 0.20 %
(60x10X4 mm bar) after 1 hour at 100°C (212°F)
0.20 - 0.30 %
0.20 - 0.30 %
(60x10X4 mm bar) after 10 days at 20°C (77°F)
Viscosity 1000 - 2500 cP
1000 - 2500 cP
Vapor Pressure <= 0.0000267 bar

@Temperature 50.0 °C
<= 0.0200 torr

@Temperature 122 °F
AboCure
<= 0.00133 bar

@Temperature 180 °C
<= 1.00 torr

@Temperature 356 °F
AboCast
0.00200 bar

@Temperature 100 °C
1.50 torr

@Temperature 212 °F
AboCure
0.0293 bar

@Temperature 165 °C
22.0 torr

@Temperature 329 °F
AboCure
0.0667 bar

@Temperature 180 °C
50.0 torr

@Temperature 356 °F
AboCure
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 75.84 MPa
11000 psi
Modulus of Elasticity 3.102 GPa
449.9 ksi
Flexural Yield Strength 131 MPa
19000 psi
Compressive Yield Strength 137.9 MPa
20000 psi
Thermal Properties Metric English Comments
CTE, linear 55.0 - 65.0 µm/m-°C

@Temperature 20.0 °C
30.6 - 36.1 µin/in-°F

@Temperature 68.0 °F
Maximum Service Temperature, Air 150 °C
302 °F
Deflection temperature; load unknown.
Electrical Properties Metric English Comments
Electrical Resistivity >= 1.50e+16 ohm-cm
>= 1.50e+16 ohm-cm
Dielectric Constant 3.3 - 3.5

@Frequency 1e+6 Hz
3.3 - 3.5

@Frequency 1e+6 Hz
3.4 - 3.6

@Frequency 1000 Hz
3.4 - 3.6

@Frequency 1000 Hz
3.6 - 3.8

@Frequency 50 Hz
3.6 - 3.8

@Frequency 50 Hz
Dielectric Strength 13.8 - 17.7 kV/mm

@Thickness 3.17 mm
350 - 450 kV/in

@Thickness 0.125 in
Short time value
Dissipation Factor 0.0020 - 0.0040

@Frequency 50 Hz
0.0020 - 0.0040

@Frequency 50 Hz
0.0030 - 0.0050

@Frequency 1000 Hz
0.0030 - 0.0050

@Frequency 1000 Hz
0.010 - 0.015

@Frequency 1e+6 Hz
0.010 - 0.015

@Frequency 1e+6 Hz
Processing Properties Metric English Comments
Processing Temperature 25.0 °C
77.0 °F
Pot Life 420 - 600 min

@Temperature 120 °C
420 - 600 min

@Temperature 248 °F
21600 - 28800 min

@Temperature 20.0 °C
21600 - 28800 min

@Temperature 68.0 °F
Copyright © lookpolymers.com All Rights Reserved