Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 85.0 MPa | 12300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® CX5640 PC+ABS Cycoloy* CX5640 is a all purpose PC+ABS blend specially developed for applications requiring weld line strength. High heat resistance combined with good flow, excellent impact and low temperature du.. |
|||
Flexural Yield Strength | 85.0 MPa | 12300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycoloy® HCX1640 PC+ABS (Europe-Africa-Middle East) CYCOLOY™ HCX1640 a PC+ABS blend specially developed for medical devices and pharmaceutical applications requiring improved mechanical performance . It combines good flow with excellent impact and l.. |
|||
Flexural Yield Strength | 85.0 MPa | 12300 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Cycoloy® LG8002 PC+ABS (Asia Pacific) Automotive. Low gloss, high impact and ductility at 73F and -22F. UV-stable colors.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Yield Strength | 85.0 MPa | 12300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics GELOY FXW749SK ASA Sparkle VisualFx ASA Resin - Weatherable |
|||
Flexural Yield Strength | 85.0 MPa | 12300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EXL1132 PC Copolymer Lexan* EXL1132 polycarbonate (PC) siloxane copolymer resin is a high flow, UV stabilized injection molding grade. This resin offers good low temperature (-20 C) ductility in combination with high fl.. |
|||
Flexural Yield Strength | 85.0 MPa | 12300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EXL1330 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1330 polycarbonate (PC) siloxane copolymer resin is a UV stabilized opaque injection molding (IM) and sheet extrusion grade. This resin offers extreme low temperature (-60 C) ductility in .. |
|||
Flexural Yield Strength | 85.0 MPa | 12300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EXL1414 PC Copolymer Lexan* EXL1414 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade. This resin offers extreme low temperature (-40 C) ductility in combination with excel.. |
|||
Flexural Yield Strength | 85.0 MPa | 12300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EXL1414 PC Copolymer (Asia Pacific) Lexan* EXL1414 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade. This resin offers extreme low temperature (-40 C) ductility in combination with excel.. |
|||
Flexural Yield Strength | 85.0 MPa | 12300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EXL1434 PC Copolymer Lexan* EXL1434 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade and is UV stabilized. This resin offers extreme low temperature (-40 C), exhibits exce.. |
|||
Flexural Yield Strength | 85.0 MPa | 12300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EXL1434 PC Copolymer (Asia Pacific) Lexan* EXL1434 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade and is UV stabilized. This resin offers extreme low temperature (-40 C), exhibits exce.. |
|||
Flexural Yield Strength | 85.0 MPa | 12300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® FXE1414 PC Copolymer Lexan* FXE1414 polycarbonate (PC) siloxane copolymer resin is a special effects fluorescent, medium flow opaque injection molding (IM) grade. This resin offers extreme low temperature (-40 C) ductil.. |
|||
Flexural Yield Strength | 85.0 MPa | 12300 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® FXM1414T PC Copolymer (Europe-Africa-Middle East) PC-siloxane copolymer in special metallic colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.This data was supplied by .. |
|||
Flexural Yield Strength | 85.0 MPa | 12300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® IM1063 PC (Europe-Africa-Middle East) Lexan* IM1063 is a impact modified polycarbonate gradeThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Yield Strength | 85.0 MPa | 12300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® ML3729 PC Excellent flow, UV stabilized, grade which contains a release agent to ensure easy processing. |
|||
Flexural Yield Strength | 85.0 MPa | 12300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® FXD1414T PC Copolymer PC-siloxane copolymer in special light diffusion colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance. |
|||
Flexural Yield Strength | 85.0 MPa | 12300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® HP1HF PC (Asia Pacific) Very high flow, biocompatible polycarbonate for healthcare applications. EtO sterilizable. |
|||
Flexural Yield Strength | 85.0 MPa | 12300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® ML3982 PC (Europe-Africa-Middle East) LEXAN ML3982 is an UV stabilized grade, with an excellent flow. It contains a release agent to ensure easy processing. |
|||
Flexural Yield Strength | 85.0 MPa | 12300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP DX98306H PC (Asia Pacific) LNP* Lubricomp* DX98306H is a compound based on Polycarbonate resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated, Low Extractible. |
|||
Flexural Yield Strength | 85.0 MPa | 12300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Xenoy® CL100 PBT+PC Xenoy CL100 is an unfilled, impact modified, UV-stabilized PC/PBT blend with excellent solvent resistance and good low-temperature ductility. It has a proven track record in unpainted exterior autom.. |
|||
Flexural Yield Strength | 84.8 MPa | 12300 psi | ASTM D790 |
Star Plastics ABSGF20 Molding Grade ABS With 20% Glass Information provided by Star Plastics, Inc. |
|||
Flexural Yield Strength | 85.0 MPa | 12300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics XYLEX X8419 PC+POLYESTER (Asia Pacific) Low-medium flow, suitable for blow molding, injection molding, extrusion. |
|||
Flexural Yield Strength | 85.0 MPa | 12300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL PX1007 PPE+PS Noryl* PX1007 is an unfilled non-chlorinated, non-brominated flame retardant PPE/HIPS grade. |
|||
Flexural Yield Strength | 85.0 MPa | 12300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL FXN4020H PPE+HIPS (Europe-Africa-Middle East) high gloss Noryl |
|||
Flexural Yield Strength | 85.0 MPa | 12300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Noryl GTX GTX918WR PPE+PS+PA (Asia Pacific) High flow PPE+PS+PA for under-the-hood and electrical applications. With mold releaseThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Yield Strength | 85.0 MPa | 12300 psi | ISO 178 |
Wellman Wellamid® XT1486-N Impact Modified Nylon 66, Lubricated & Heat Stabilized Typical Applications: Automotive fasteners, living hinge, head lamp adjustment devices, ink pen components, wire separators, hardware components, window installation clips, safety equipment.Data pro.. |
|||
Flexural Yield Strength | >= 85.0 MPa | >= 12300 psi | ASTM D790 |
Cresset Powers Cress-Alon™ A2700 2.7 r.v. Compounding Grade Nylon 6, Dry As Molded Neat resin, for compounding.Information provided by Cresset Powers Ltd. |
|||
Flexural Yield Strength | 85.0 MPa | 12300 psi | ASTM D790 |
Ascend Performance Materials VYDYNE® 45 Nylon, Impact Modified, Weather Stable Typical property data. VYDYNE is a registered trademark of Solutia Inc. |
|||
Flexural Yield Strength | 85.0 MPa | 12300 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Noryl FXN119LG PPE+HIPS Noryl FXN119LG is a low gloss PPE/HIPS grade. It provides a balance of mechanical properties and heat performance with intrinsic low gloss appreance. FXN119LG is available in mutliple colors.This da.. |
|||
Flexural Yield Strength | 85.0 MPa | 12300 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Noryl FXN119LG PPE+HIPS (Europe-Africa-Middle East) Noryl FXN119LG is a low gloss PPE/HIPS grade. It provides a balance of mechanical properties and heat performance with intrinsic low gloss appreance. FXN119LG is available in mutliple colors.This da.. |
|||
Flexural Yield Strength | 85.0 MPa | 12300 psi | ASTM D790 |
Eastman 9921W PET Injection Molded