Isoflon PA 12 Polyamide 12

Category Polymer , Thermoplastic , Nylon , Nylon 12
Manufacturer Isoflon
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Isoflon PA 12 Polyamide 12.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
General use for mechanical partsGood heat resistanceEasy to useInformation provided by Isoflon.
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
DIN 53479
Water Absorption 0.80 %
0.80 %
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell R 110
110
ASTM D785
Tensile Strength 44.0 MPa
6380 psi
DIN 53455
Elongation at Break 150 %
150 %
DIN 53455
Tensile Modulus 1.55 GPa
225 ksi
DIN 53457
Thermal Properties Metric English Comments
CTE, linear 110 µm/m-°C
61.1 µin/in-°F
DIN 52328
Thermal Conductivity 0.300 W/m-K
2.08 BTU-in/hr-ft²-°F
DIN 52612
Melting Point 185 °C
365 °F
DIN 53736
Maximum Service Temperature, Air 80.0 °C
176 °F
Continuous; DIN 52612
Deflection Temperature at 1.8 MPa (264 psi) 54.0 °C
129 °F
Minimum Service Temperature, Air -50.0 °C
-58.0 °F
Continuous; DIN 52612
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
DIN 53482
Dielectric Constant 3.5

@Frequency 1000 Hz
3.5

@Frequency 1000 Hz
DIN 53483
Dielectric Strength 20.0 - 30.0 kV/mm
508 - 762 kV/in
DIN 53481
Descriptive Properties Value Comments
Color Nat.