Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 6.70 GPa | 972 ksi | STN EN ISO 527-2 |
Plastcom SLOVAMID® 6 T 30 FRC 4 TS PA6 flame retarded, heat stabilized PA 6 for injection molding, reinforced with 30% mineral filler, flame retarded with nonhalogen flame retardant, heat stabilized. Main features: flammability in accordance with UL 94 3 at 1,6 mm, glo.. |
|||
Tensile Modulus | 6.70 GPa | 972 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP DFL34XXP PC (Europe-Africa-Middle East) LNP* Lubricomp* DFL-4034 HP is a compound based on Polycarbonate resin containing Glass Fiber, PTFE. |
|||
Tensile Modulus | 6.70 GPa @Temperature 150 °C |
972 ksi @Temperature 302 °F |
ISO 527-2 |
Solvay Specialty Polymers Amodel® A-1133 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resistance.. |
|||
Tensile Modulus | 6.70 GPa | 972 ksi | ASTM D638 |
Parker Chomerics PREMIER™ A230-HTHF EMI Shielding Plastic Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer .. |
|||
Tensile Modulus | 6.70 GPa | 972 ksi | Conditioned; ISO 527-1/-2 |
Lanxess Durethan® BKV 140 000000 Copolyamide, 40% Glass Fiber CoPA, injection molding grade, 40% glass fibers, elastomer-modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 40, even in.. |
|||
Tensile Modulus | 6.70 GPa | 972 ksi | Conditioned; ISO 527-1/-2 |
Lanxess Durethan® BKV 140 H2.0 900051 Copolyamide, 40% Glass Fiber CoPA, injection molding grade, 40% glass fibers, elastomer-modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 40, even in.. |
|||
Tensile Modulus | 6.70 GPa | 972 ksi | ISO 527-1/-2 |
Lanxess Durethan® AKV 15 000000 Nylon 66, 15% Glass Fiber PA 66, injection molding grade, 15% glass fibers |
|||
Tensile Modulus | 6.70 GPa | 972 ksi | Conditioned; ISO 527-1/-2 |
Lanxess Durethan® BKV 30 FN00 000000 Nylon 6, 30% Glass Fiber PA6, injection molding grade, 30% glass fibers, UL94 V-0 at 0,75 mm , free of halogen and red phosphorus, glow wire flammability test max. 960°C |
|||
Tensile Modulus | 6.70 GPa | 972 ksi | Conditioned; ISO 527-1/-2 |
Lanxess Durethan® BKV 35 H2.0 EF 901510 Nylon 6, 35% Glass Fiber PA 6, injection molding grade, 35% glass fibers, good heat-ageing resistance, good flowability (easy flow) |
|||
Tensile Modulus | 6.70 GPa | 972 ksi | ISO 527 Type 1A |
Solvay TECHNYL® C 52G1 V20 PA6, DRY Description: Halogen and Red Phosphorous free fire resistant polyamide PA6 Glass reinforced for injection molding of thin walled partsAvailable in: Asia Pacific, Europe, Latin America and North Amer.. |
|||
Tensile Modulus | 6.70 GPa | 972 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Ultem ATX152R PEI+PCE (Asia Pacific) 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Modulus | 6.70 GPa | 972 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Ultem ATX152R PEI+PCE (Europe-Africa-Middle East) 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio.. |
|||
Tensile Modulus | 6.70 GPa @Temperature 150 °C |
972 ksi @Temperature 302 °F |
4; ISO 527-2 |
Solvay Specialty Polymers Amodel® AE-1133 Polyphthalamide (PPA), 33% Glass Fiber Amodel® AE-1133 is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) designed to work in the modern automotive electrical environment. It has a high heat deflection temperature, high .. |
|||
Tensile Modulus | 6.70 GPa | 972 ksi | ISO 527-2 |
Solvay Specialty Polymers Lavanta® 5115 WH 011 Polyester, High Performance (HPP), 15% Glass Fiber Lavanta® 5115 WH011 is a 15% glass fiber reinforced, high-performance polyester (HPP) injection molding grade developed specifically for HB LED packaging applications that utilize surface mount .. |
|||
Tensile Modulus | 6.70 GPa | 972 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp CF004 PS (Europe-Africa-Middle East) LNP* Thermocomp* CF004 is a compound based on Polystyrene resin containing Glass Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Modulus | 6.70 GPa | 972 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP JF004 PES (Europe-Africa-Middle East) LNP* Thermocomp* JF004 is a compound based on Polyethersulfone resin containing Glass Fiber. |
|||
Tensile Modulus | 6.70 GPa | 972 ksi | 1mm/min; ISO 527 |
Teijin Panlite® G-3430H Low Anisotropy, Glass Fiber Reinforced Polycarbonate Resin Reinforced with 30 % of special GF and improved appearance grade, meeting UL 94 V-2.Applications:Mechanical, electric and electronic components that need good appearance and mechanical propertyPreci.. |
|||
Tensile Modulus | 6.70 GPa | 972 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp RFB33 PA6.6 (Europe-Africa-Middle East) LNP*THERMOCOMP* RFB33 is a compound based on PA66 resin containing Glass Bead, Glass Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Modulus | 6.70 GPa | 972 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Ultem ATX152R PEI+PCE 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 6.70 GPa | 972 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® SHF4340 PBT 20% GF Super High Flow PBT |
|||
Tensile Modulus | 6.70 GPa | 972 ksi | ISO 527-1/-2 |
Unitika B2040G33 PA66, 33% Glass Fiber Reinforced, Conditioned Information provided by Unitika Ltd. |
|||
Tensile Modulus | 6.70 GPa | 972 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® BG-15 PA6-GF15 Product description: Grilon BG-15 is a heat stabilized PA 6 injection molding grade with 15% glass fiber reinforcement. Grilon BG-15 has the following important properties: Good surface finishGood b.. |
|||
Tensile Modulus | 6.70 GPa | 972 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® BG-15 S PA6-GF15 Product description: Grilon BG-15 S is a heat stabilized PA6 injection molding grade with 15% glass fibers. Grilon BG-15 S has the following important properties: Excellent surface finishEasy flowin.. |
|||
Tensile Modulus | 6.70 GPa | 972 ksi | 1 mm/min; ISO 527 |
Eurostar Starflam P10003 PA6, Mineral Filled, Flame Retardant, Extrusion Starflam P10003 is a Mineral Filled, Halogen Free, Red Phosphorous Free, Flame Retardant, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Modulus | 6.70 GPa | 972 ksi | cond.; ISO 527 |
Azoty Tarnow™ Tarnamid® T-27 GF10 MX10 Polyamide 6 - Flame Retarded, Reinforced Flame retarded grade, reinforced with 10% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning, good surface quality.T.. |
|||
Tensile Modulus | 6.70 GPa | 972 ksi | ISO 527-1/-2 |
Lanxess Pocan® KU 2-7209 Z 901510 PBT, 15% Glass Fiber PBT, injection molding grade with 15% glass fibers, elastomer modified, UL 94V0 at 0.8 mm (all colors-in house test), UL-listed from 1.5mm thickness. |
|||
Tensile Modulus | 6.70 GPa | 972 ksi | ISO 527-1/-2 |
Lanxess Pocan® B 3225 Z 000000 PBT, 20% Glass Fiber
(discontinued **) PBT, 20% glass fibers, injection molding, impact modified |