Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 6.00 GPa | 870 ksi | STN EN ISO 527-2 |
Plastcom SLOVAMID 66 GF 30 FRA 3 Polyamide 66, 30% Glass Fiber, Halogen Flame Retardant FeaturesPA 66 for injection moulding, reinforced with 30% glass fiber and halogen flame retardant. Application in electrical industry: breakers, coil forms, covers, terminals. Slightly decreased f.. |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | ASTM D638 |
North Wood Plastics Polypropylene with 60% Wood Fiber, Extrusion Grade Data provided by North Wood Plastics, Inc. |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP FARADEX NX07344 PC+ABS (Asia Pacific) Faradex NX07344 is a compound based on PC+ABS blend resin containing non-brominated and non-chlorinated flame retardant system, Stainless Steel and glass fiber. Added features of this material incl.. |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | ISO 527 |
Nilit FRIANYL B63 H-GV15 Nylon 6 for injection molding, 15% glass fiber reinforced Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | ISO 527 |
Nilit FRIANYL B63 SG-GV 2010 Nylon 6 for injection molding, 20% mineral filled and 10% glass fiber reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | ISO 527 |
Nilit FRIANYL B63 TF-GV 1520 Nylon 6 for injection molding, 15% PTFE lubricated, 20% glass fiber reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | ISO 527-1/-2 |
Mitsubishi Xantar® G4F 22 UR Polycarbonate-20% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | ISO 527-1/-2 |
Mitsubishi Xantar® G4F 25 R Polycarbonate-20% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | ISO 527 |
Grupo Repol Dinalon® B1S25 G15 PA6 15% Glass Fiber Mechanical properties for Dry As Molded samplesInformation provided by Grupo Repol |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP AF004 ABS (Europe-Africa-Middle East) LNP* THERMOCOMP* AF004 is a compound based on Acrylonitrile Butadiene Styren resin containing Glass Fiber. |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP AF004AH ABS LNP THERMOCOMP* AF004AH is a compound based on ABS resin containing 20% Glass Fiber. Added feature of this material is: Healthcare. |
|||
Tensile Modulus | 6.00 - 8.00 GPa | 870 - 1160 ksi | DIN 53457 |
Schwartz Technical Plastics LAMINEX® 2100 Cotton Fabric, Phenolic Resin Impregnated Application: bearing shells and bearing collarsInformation provided by Schwartz Technical Plastics GmbH |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | ASTM D638 |
Styron EMERGEâ„¢ 8702 Polycarbonate EMERGEâ„¢ PC 8702 advanced resin is an ignition-resistant, 20% glass reinforced, polycarbonate resin. This resin contains no bromide, chloride, or phosphate additives. It is a medium flow PC re.. |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | ISO 527 |
Polyram RamOfin PPH301G6NT Polypropylene, 30% Glass Fiber 30% Glass fiber reinforced polypropylene for injection molding applications. Approved and listed by WRAS Potable Water.Information provided by Polyram. |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | cond; ISO 527-1/-2 |
DSM Akulon® K224-G6-FC 99.99.99 PA6-GF30 30% Glass Reinforced, Food Contact Grade |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | cond; ISO 527-1/-2 |
DSM Akulon® K224-LG6 /E PA6-GF30 30% Glass Reinforced, Injection Molding, Improved UV-stability |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | cond; ISO 527-1/-2 |
DSM Novamid® 1017GH33 BK701 PA6-GF33 33% Glass Reinforced, Heat Stabilized, Injection Molding |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | ISO 527-1/-2 |
DSM Stanyl® 46HF4130 Nylon 46-30% Glass Reinforced (European and Asian Grade) (Cond) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6000 GV 30 HW 30% Glass Fiber Nylon 6, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® HT2VZ-15H PA6T/66-GF15 Information provided by EMS Grivory |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® LV-30H FWA black 9225 PA12-GF30 Product description: Grilamid LV-30H FWA black 9225 is a 30 % glass fiber reinforced, heat stabilized polyamide12 injection molding grade with the following special features: Stiffness combined with.. |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® LV-3H PA12-GF30 Product description: Grilamid LV-3H is a 30% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following product profile: very low water absorptionhigh dimensiona.. |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | ISO 527 |
Eurotec® Tecomid® NA40 KK30 NL PA 6.6 30% glass fiber/mineral reinforced, low warpage Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | ISO 527-1/-2 |
DSM Akulon® K-FHG6 (Cond.) 30% Glass Reinforced Nylon 6 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Crastin® SK612SF NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 15% Glass Reinforced Low Viscosity Polybutylene Terephthalate Developed for Super Fast Production Crastin SK612SF is a 15% glass fiber reinforced low viscosity polybutylene terephthalate for injecti.. |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | ISO 527-1/-2 |
DSM Akulon® K220-HGM44 Nylon 6-40% Glass and Mineral Reinforced (European and Asian Grade) (Cond)
(discontinu The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | ISO 527-1/-2 |
DSM Arnite® TV4 230 PBT-15% Glass Reinforced (European and Asian Grade) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
Tensile Modulus | 6.00 GPa | 870 ksi | |
LATI Latilub 67-10STE21 G/20 PA66, 20% Glass Fiber Reinforced, Silicone/PTFE Filled Self-lubricating product based on Polyamide 66 (PA66), impact modified. Silicone / PTFE. Toughened. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North Ameri.. |