Mechanical Properties Metric English Comments
Tensile Modulus 5.80 GPa
841 ksi
Plastcom SLOVAMID 6 GF 10 FRC 2 PA6, 10% glass fibre, flame retardant
FeaturesPA 6 for injection moulding, chemically strengthened with 10 % glass fibre. Application: impacted mouldings and mouldings with high strength applied in automotive, electrical, engineering an..
Tensile Modulus 5.80 GPa
841 ksi
Plastcom SLOVAMID 66 GF 15 T 6 TS PA66, 15% glass fibre, 6% talc
FeaturesChemically reinforced with 15% glass fibre and 6% of talc, suitable for mouldings with high strength and toughness also at low temperatures. Used in the automotive, engineering and electrica..
Tensile Modulus 5.80 GPa
841 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics Cycoloy® CM4219 PC+ABS (Asia Pacific)
Tensile Modulus 5.80 GPa
841 ksi
Plastcom SLOVAMID 6 GF 10 GB 20 PA6, 10% glass fibre, 20% glass beads
FeaturesPA 6 for injection moulding, chemically strengthened with 10% glass fibre and 20% glass beads. Application: impacted mouldings and mouldings with high strength applied in automotive, electri..
Tensile Modulus 5.80 GPa
841 ksi
ISO 527, ASTM D638
Nilit Nilamid B3 H G3 15% Glass Fiber Reinforced PA6
Description: Nilamid B3 H G3 is a general purpose, 15% glass fiber reinforced NYLON 6. These products combine good overall mechanical performance and impact strength with ease of processing. Key cha..
Tensile Modulus 5.80 GPa
841 ksi
ISO 527
Nilit FRIANYL B63 W-GV15 Nylon 6 for injection molding, 15% glass fiber reinforced
Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Tensile Modulus 5.80 GPa
841 ksi
d.a.m.; ISO 527-1, -2; 1 mm/min
Lanxess Durethan® BM 240 000000 Nylon 6, Mineral Reinforced
PA 6, injection molding, 40% mineral, isotopic properties, low warpageInformation provided by LANXESS.
Tensile Modulus 5.80 GPa
841 ksi
ISO 527-1, -2; 1 mm/min
Lanxess Pocan® DP 7102 000000 PBT, 32% Mineral
PBT, 32% mineral, injection molding, LDSInformation provided by LANXESS.
Tensile Modulus 5.80 GPa
841 ksi
ISO 527 Type 1A
Solvay TECHNYLSTARâ„¢ S 218 MT PA6, 40% mineral filled, DRY
Description: TechnylStar Polyamide, 40% mineral filled, heat stabilized, for injection molding. Characterized by a high fluidity of the melt.Available in: Asia Pacific and North AmericaProduct Appli..
Tensile Modulus 5.80 GPa
841 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP PH0320A PA 6 (Asia Pacific)
LNP THERMOCOMP* PH0320A is a compound based on Nylon 6 resin. Added features of this material include: High Specific Gravity.
Tensile Modulus 5.80 GPa
841 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP Thermocomp PX05046 PA 6 (Europe-Africa-Middle East)
LNP* THERMOCOMP* PX05046 is a compound based on PA 6 resin containing Glass Bead, Glass Fiber. Added features include: Heat Stabilized, UV-Stabilized.This data was supplied by SABIC-IP for the Europ..
Tensile Modulus 5.80 GPa
841 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics NORYL IGN5531 PPE+PS
Noryl* IGN5531 is an 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Nor..
Tensile Modulus 5.80 GPa
841 ksi
dry; ISO 527-1/-2
DSM Novamid® 1013G15 1 NA PA6-GF15
15% Glass Reinforced, Injection Molding
Tensile Modulus 5.80 GPa
841 ksi
ISO 527
CP-Polymer-Technik Wellamid® 6000 GS 50 HWCP 50% Glass Sphere Filled Nylon 6, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
Tensile Modulus 5.80 GPa
841 ksi
ISO 527
CP-Polymer-Technik Wellamid® 6000 GS 50 HWUVCP 50% Glass Sphere Filled Nylon 6, UV Stabilized, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
Tensile Modulus 5.80 GPa
841 ksi
ISO 527
CP-Polymer-Technik Wellamid® 6000 MR 409 HWCP Mineral Nylon 6, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
Tensile Modulus 5.80 GPa
841 ksi
ISO 527
CP-Polymer-Technik Wellamid® 6000/52 GV 15 HWUVCP 15% Glass Fiber Nylon 6, Low Temperature Impact Modified, UV Stabilized, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
Tensile Modulus 5.80 GPa
841 ksi
dry; ISO 527-1/-2
EMS-Grivory Grivory® TSGZ-15/4 PA666-GF15
Information provided by EMS Grivory
Tensile Modulus 5.80 GPa
841 ksi
ISO 527-1/-2
DuPont Performance Polymers Crastin® SK602 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)
15% Glass Reinforced Polybutylene Terephthalate Crastin SK602 NC010 is a 15% glass fiber reinforced lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont P..
Tensile Modulus 5.80 GPa

@Temperature 23.0 °C
841 ksi

@Temperature 73.4 °F
EN ISO 527
Ensinger TECASINT 5051 Polyimide, 30% Glass Fiber Filled (PI)
TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel..
Tensile Modulus 5.80 GPa
841 ksi
DAM; ISO 527-1/-2
DuPont Performance Polymers Minlon® 11C140 BK086 Nylon 66  (Unverified Data**)
40% Mineral Reinforced Polyamide 66 Minlon 11C140 BK086 is a 40% mineral reinforced heat stabilized black polyamide 66 resin for injection molding. It has very low warpage.Information provided by Du..
Tensile Modulus 5.80 GPa
841 ksi
DAM; ISO 527-1/-2
DuPont Performance Polymers Minlon® 11C40 BKB086 Nylon 66  (Unverified Data**)
40% Mineral Reinforced Polyamide 66 Minlon 11C40 BKB086 is a 40% mineral reinforced heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers..
Tensile Modulus 5.80 GPa
841 ksi
ISO 527
Eurostar Starglas FF006 HDPE, Glass Fiber Filled
Starglas FF004 is a Glass Fiber Reinforced High Density Polyethylene Resin (also known as Starglas PE HE 30V)Information provided by Eurostar.
Tensile Modulus 5.80 GPa
841 ksi
1 mm/min; ISO 527
Eurostar Staramide BG3H PA6, 15% Glass Filled, Injection Molded
BG3H is a Heat Stabilized, 15% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
Tensile Modulus 5.80 GPa
841 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP PH0320A PA 6